EFFECTS OF GRAIN REFINEMENT ON CREEP PROPERTIES OF K417G SUPERALLOY

  • Beining DU ,
  • Jinxia YANG ,
  • Chuanyong CUI ,
  • Xiaofeng SUN
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2014-07-02

  Revised date: 2014-05-07

  Online published: 2014-11-25

Supported by

Supported by National Natural Science Foundation of China (Nos.51171179, 51128101, 51271171 and 11332010), National Basic Research Program of China (No.2010CB631206) and Program of One Hundred of Talented People of Chinese Academy of Sciences

Abstract

Grain size is one of the most important parameters which affect the mechanical properties of cast polycrystalline superalloys. To study the effect of grain refinement on the creep behaviors of K417G superalloy, the creep behaviors of K417G superalloy with four grain sizes were investigated at 760 ℃/645 MPa, 900 ℃/315 MPa and 950 ℃/235 MPa. The longitudinal section of the fracture surface, crack propagation path, dislocation structure and plastic deformation distribution in the vicinity of the cracks were investigated by using SEM, TEM and EBSD techniques, thus the deformation mechanism and effect of grain refinement on the creep properties of K417G superalloy were determined under different creep conditions. The results showed that the effects of grain refinement on the creep property of the alloy varied with the temperatures and stress. At 760 ℃/645 MPa, grain refinement improved the creep life and reduced the steady-state deformation rate of the alloy. The creep deformation was dominated by intragranular deformation. At 900 ℃/315 MPa, as grain size decreased, the creep life increased firstly and then decreased, while the steady-state deformation rate decreased firstly and then increased. The creep deformation showed a competitive effect of intragranular deformation and grain boundary sliding. At 950 ℃/235 MPa, the creep life decreased and the steady-state deformation rate increased with the decrease of the grain size. Grain boundary sliding was the main deformation mode. At the same time, grain refinement could cause a refinement of the dendrite and carbide of the alloy, which would also affect the creep behavior of the alloy to a small extent. The TEM observation showed that at 760 ℃/645 MPa, the dislocations interacted with g' particles through shearing mechanism and no dislocation network was found in the matrix. While at 900 ℃/315 MPa and 950 ℃/235 MPa, the dislocations crossed the g' particles through Orowan bypass mechanism, dislocation network formed in the matrix, and M23C6 precipitated in the interior of the grains, which had a orientation relationship between the M23C6 precipitates and matrix .

Cite this article

Beining DU , Jinxia YANG , Chuanyong CUI , Xiaofeng SUN . EFFECTS OF GRAIN REFINEMENT ON CREEP PROPERTIES OF K417G SUPERALLOY[J]. Acta Metall Sin, 2014 , 50(11) : 1384 -1392 . DOI: 10.11900/0412.1961.2014.00245

References

[1] Yang Y H, Xie Y J, Wang M S, Ye W. Mater Des, 2013; 51: 141
[2] Xu Y, Guo S R. Acta Metall Sin, 1999; 35: 1249
[2] (徐 岩, 郭守仁. 金属学报, 1999; 35: 1249)
[3] Zheng L. J Aeronaut Mater, 2006; 26(3): 7
[3] (郑 亮. 航空材料学报, 2006; 26(3): 7)
[4] Andersson J. Int J Fatigue, 2005; 27: 847
[5] Ho H, Risbet M, Feaugas X, Moulin G. Scr Mater, 2011; 65: 998
[6] Kobayashi K, Yamaguchi K, Hayakawa M, Kimura M. Mater Lett, 2005; 59: 383
[7] Torster F, Baumeister G, Albrecht J, Lütjering G, Helm D, Daeubler M A. Mater Sci Eng, 1997; A234: 189
[8] Wei C N, Bor H Y, Ma C Y, Lee T S. Macromol Chem Phys, 2003; 80: 89
[9] Xiong Y H, Liu W, Yang A M, Zhang R, Liu L. Acta Metall Sin, 1999; 35: 689
[9] (熊玉华, 柳 伟, 杨爱民, 张 蓉, 刘 林. 金属学报, 1999; 35: 689)
[10] Yang A M. PhD Dissertation, Northwestern Polytechnical University, Xi'an, 2002
[10] (杨爱民. 西北工业大学博士学位论文, 西安, 2002)
[11] Soula A, Renollet Y, Boivin D, Pouchou J L, Locq D, Caron P. Mater Sci Eng, 2009; A510: 301
[12] Yuan Y, Gu Y F, Cui C Y, Osada T, Tetsui T, Yokokawa T. Mater Sci Eng, 2011; A528: 5106
[13] Thibault K, Locq D, Caron P, Boivin D, Renollet Y, Bréchet Y. Mater Sci Eng, 2013; A588: 14
[14] Shingledecker J P, Evans N D, Pharr G M. Mater Sci Eng, 2013; A578: 277
[15] Morrison D J, Moosbrugger J C. Int J Fatigue, 1997; 19: 51
[16] Qiao Y, Chakravarthula S S. Int J Fatigue, 2005; 27: 1251
[17] Larson J M, Floreen S. Metall Trans, 1977; 8A: 51
[18] Quested P N, Osgerby S. Mater?Sci?Technol, 1986; 2: 461
[19] Kuhn F, Zeismann F, Brueckner-Foit A. Int J Fatigue, 2014; 65: 86
[20] Miao J, Pollock T M, Wayne Jones J. Acta Mater, 2009; 57: 5964
[21] Miao J, Pollock T M, Wayne Jones J. Acta Mater, 2012; 60: 2840
[22] Brewer L N, Field D P, Merriman C C. Electron Backscatter Diffraction in Materials Science. New York: Springer, 2009: 18
[23] Wang D, Zhang J, Lou L H. Mater Charact, 2009; 60: 1517
[24] Liu L R, Jin T, Zhao N R, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2003; A361: 191
[25] Guo Y, Wang B H, Hou S F. Acta Metall Sin (Eng Lett), 2013; 26: 307
[26] Zhang J X, Murakumo T, Harada H, Koizumi Y. Scr Mater, 2003; 48: 287
[27] Nategh S, Sajjadi S A. Mater Sci Eng, 2003; A339: 103
[28] Zhu Y, Li Z, Huang M. Comput Mater Sci, 2013; 70: 178
[29] Tian S G, Zhou H H, Zhang J H,Yang H C, Xu Y B, Hu Z Q. Mater Sci Eng, 2000; A279: 160
[30] Hantcherli M, Pettinari-Sturmel F, Viguier B, Douin J, Coujou A. Scr Mater, 2012; 66: 143
Outlines

/

〈 〉