EFFECT OF HIGH TEMPERATURE PRE-AGEING AND LOW-TEMPERATURE RE-AGEING ON MECHANICAL PROPERTIES AND INTERGRANULAR CORROSION SUSCEPTIBILITY OF Al-Mg-Si-Cu ALLOYS

  • Hai LI ,
  • Qingzhong MAO ,
  • Zhixiu WANG ,
  • Fenfen MIAO ,
  • Bijun FANG ,
  • Renguo SONG ,
  • Ziqiao ZHENG
Expand
  • 1 School of Materials Science and Engineering, Changzhou University, Changzhou 213164
    2 School of Materials Science and Engineering, Central South University, Changsha 410083
    3 Jiangsu Key Laboratory of Materials Surface Technology, Changzhou University, Changzhou 213164

Received date: 2014-08-16

  Revised date: 2014-03-24

  Online published: 2014-11-25

Supported by

National Natural Science Foundation of China (No.51301027), National Basic Research Program of China (No.2005CB623705) and Natural Science Foundation of the Jiangsu Higher Education Institutions of China (No.14KJB430002)

Abstract

It is well known that in peak-aged conditions age-hardenable aluminum alloys usually have high strength but low corrosion resistance. Low corrosion resistance of peak-aged Al alloys limits their applications in some corrosive conditions. In order to enhance the corrosion resistance, over-ageing treatments are often carried out but at the expense of strength. Therefore, it is of great industrial value to improve both strength and corrosion resistance of Al alloys simultaneously. In the present work, a novel two-step ageing treatment consisted of high-temperature pre-ageing and low-temperature re-ageing was proposed to improve both the tensile properties and intergranular corrosion (IGC) resistance of Al-Mg-Si-Cu alloys simultaneously. Furthermore, the effects of pre-ageing time at 180 ℃ and re-ageing time at 160 ℃ on the mechanical property and IGC susceptibility of the 6061 Al alloy were investigated by tensile testing and immersion corrosion testing. It was shown that after the optimized two-step ageing treatment of 180 ℃, 2 h+160 ℃, 120 h, the 6061 Al alloy had slightly higher strength than that of the conventional peak-aged samples and no susceptibility to intergranular corrosion. TEM observation revealed that the microstructures of the two-step treated 6061 Al alloy were consisted of high density of b″ phase along with small amount of Q' phase in the matrix and discontinuously distributed, spherical grain boundary precipitates, which led to high strength and IGC resistance of the 6061 Al alloy, respectively. The formation of the characteristic microstructures were attributed to the different decreased level of atomic diffusion rate between the matrix and grain boundary when decreasing from relatively high pre-ageing temperature to low re-ageing temperature, which resulted in the relatively slow growth of the matrix pre-precipitates and rapid coarsening of the grain boundary pre-precipitates, simultaneously.

Cite this article

Hai LI , Qingzhong MAO , Zhixiu WANG , Fenfen MIAO , Bijun FANG , Renguo SONG , Ziqiao ZHENG . EFFECT OF HIGH TEMPERATURE PRE-AGEING AND LOW-TEMPERATURE RE-AGEING ON MECHANICAL PROPERTIES AND INTERGRANULAR CORROSION SUSCEPTIBILITY OF Al-Mg-Si-Cu ALLOYS[J]. Acta Metall Sin, 2014 , 50(11) : 1357 -1366 . DOI: 10.11900/0412.1961.2014.00132

References

[1] Williams J C, Starke E A. Acta Mater, 2003; 51: 5775
[2] Pogatscher S, Antrekowitscha H, Leitner H, Ebner T, Uggowitzer P J. Acta Mater, 2011; 59: 3352
[3] Zhang X M. Acta Metall Sin, DOI: 10.11900/0412.1961.2013.00835
[3] (张新明. 金属学报, DOI: 10.11900/0412.1961.2013.00835)
[4] Yang W C, Wang M P, Sheng X F, Zhang Q, Wang Z A. Acta Metall Sin, 2010; 46: 1481
[4] (杨文超, 汪明朴, 盛晓菲, 张 茜, 王正安. 金属学报, 2010; 46: 1481)
[5] El-Menshawy K, El-Sayed A W A, El-Bedawy M E, Ahmed H A, El-Raghy S M. Corros Sci, 2012; 54: 167
[6] Svenningsen G, Lein J E, Bj?rgum A, Nordlien J H, Yu Y, Nisanciouglu K. Corros Sci, 2006; 48: 226
[7] Svenningsen G, Larsen M H, Nordlien J H, Nisanciouglu K. Corros Sci, 2006; 48: 258
[8] Svenningsen G, Larsen M H, Nordlien J H, Nisanciouglu K. Corros Sci, 2006; 48: 3969
[9] Svenningsen G, Larsen M H, Walmsley J C, Nordlien J H, Nisancioglu K. Corros Sci, 2006; 48: 1528
[10] He L Z, Chen Y B, Cui J Z, Sun X F, Guan H R, Hu Z Q. Corros Sci Protect Technol, 2004; 16: 129
[10] (何立子, 陈彦博, 崔建忠, 孙晓峰, 管恒荣, 胡壮麒. 腐蚀科学与防护技术, 2004; 16: 129)
[11] Wang Z X, Li H, Gu J H, Song R G, Zheng Z Q. Chin J Nonferrous Met, 2012; 22: 3348
[11] (王芝秀, 李 海, 顾建华, 宋仁国, 郑子樵. 中国有色金属学报, 2012; 22: 3348)
[12] Liang W J, Rometsch P A, Cao L F, Birbilis N. Corros Sci, 2013; 76: 119
[13] Dif R, Bes B, Ehrstro J C, Sigli J C, Warner J T, Lassince P, Ribes H. Mater Sci Forum, 2000; 331-337: 1613
[14] Pan D Z, Wang Z X, Li H, Zheng Z Q. Chin J Nonferrous Met, 2010; 20: 435
[14] (潘道召, 王芝秀, 李 海, 郑子樵. 中国有色金属学报, 2010; 20: 435)
[15] Lin L, Zheng Z Q, Li J F. Rare Met Mater Eng, 2012; 41: 1004
[15] (林 莉, 郑子樵, 李劲风. 稀有金属材料与工程, 2012; 41: 1004)
[16] Li H, Pan D Z, Wang Z X, Zheng Z Q. Acta Metall Sin, 2010; 46: 494
[16] (李 海, 潘道召, 王芝秀, 郑子樵. 金属学报, 2010; 46: 494)
[17] Sheng X F, Yang W C, Xia C D, Gong J, Wang M P, Li Z, Zhang Q. Chin J Nonferrous Met, 2012; 22: 1276
[17] (盛晓菲, 杨文超, 夏承东, 龚 静, 汪明朴, 李 周, 张 茜. 中国有色金属学报, 2012; 22: 1276
[18] Wang S Q, Lu Z, Dai S L, Yang S J, Jiang H F. J Aeronaut Mater, 2003; (S1): 79
[18] (王胜强, 陆 政, 戴圣龙, 杨守杰, 姜海峰. 航空材料学报, 2003; (增刊): 79)
[19] Buha J, Lumley R N, Crosky A G, Hono K. Acta Mater, 2007; 55: 3015
[20] Ninive P H, Strandlie A, Gulbrandsen-Dahl S, Lefebvre W, Marioara C D, Andersen S J, Friis J, Holmestad R, L?vvik O M. Acta Mater, 2014; 69: 126
[21] Wang B, Wang X J, Song H, Yan J J, Qiu T, Liu W Q, Li H. Acta Metall Sin, 2014; 50: 685
[21] (汪 波, 王晓姣, 宋 辉, 严菊杰, 邱 涛, 刘文庆, 李 慧. 金属学报, 2014; 50: 685)
[22] Chakrabarti D J, Laughlin D E. Prog Mater Sci, 2004; 49: 389
[23] Gaber A, Gaffar M A, Mostafa M S, Abo Zeid E F. J Alloys Compd, 2007; 429: 167
[24] Weatherly G C, Perovic A, Mukhopakhyay N K, Lloyd D J, Perovic D D. Metall Mater Trans, 2001; 32A: 213
[25] Miao W F, Laughlin D E. Scr Mater, 1999; 40: 873
[26] Wang Z X, Li H, Miao F F, Sun W J, Fang B J, Song R G, Zheng Z Q. Mater Sci Eng, 2014; A590: 267
[27] Li C X. Master Thesis, Central South University, Changsha, 2010
[27] (李朝兴. 中南大学硕士学位论文, 长沙, 2010)
Outlines

/

〈 〉