PRECIPITATION CHARACTERIZATION OF NiAl AND Cu-RICH PHASES IN DUAL-PHASE REGION OF PRECIPITATION STRENGTHENING STEEL

  • Xiaojiao WANG ,
  • Qin SHEN ,
  • Jujie YAN ,
  • Tao QIU ,
  • Bo WANG ,
  • Hui LI ,
  • Wenqing LIU
Expand
  • Laboratory for Microstructures, Shanghai University, Shanghai 200444

Received date: 2014-08-20

  Revised date: 2014-03-19

  Online published: 2014-11-25

Supported by

Joint Funds of the National Natural Science Foundation of China (No.U1460103)

Abstract

Precipitation strengthening plays an important role on improving the mechanical properties of steels, NiAl and Cu-rich phases are two kinds of common precipitates. This work aims to reveal the precipitation characteristics of these two phases in martensite and retained austenite in precipitation strengthening steel by atom probe tomography (APT). The hot rolled samples were aged at 500 ℃ for 1 h after solution treatment at 900 ℃ for 2 h, followed by microstructure analysis. The results show that NiAl and Cu-rich phases form in martensite phase as well as at martensite/austenite phase boundaries, while no precipitate develops in retained austenite. Precipitation was not observed near the phase boundaries in martensite. Equivalent radius, spacing and concentration of the strengthening phases at phase boundary are larger than that inside martensite. In addition, NiAl phase tend to separate from Cu-rich phase, and the separated tendency becomes stronger at phase boundaries than in martensite. Besides, the growth of NiAl and Cu-rich phases at phase boundary differs from that within martensite, which should be induced by the defect density difference between them.

Cite this article

Xiaojiao WANG , Qin SHEN , Jujie YAN , Tao QIU , Bo WANG , Hui LI , Wenqing LIU . PRECIPITATION CHARACTERIZATION OF NiAl AND Cu-RICH PHASES IN DUAL-PHASE REGION OF PRECIPITATION STRENGTHENING STEEL[J]. Acta Metall Sin, 2014 , 50(11) : 1305 -1310 . DOI: 10.11900/0412.1961.2014.00118

References

[1] Monzen R, Iguchi M, Jenkins M L. Philos Mag Lett, 2000; 80: 137
[2] Lee T H, Kim Y O, Kim S J. Philos Mag, 2007; 87: 209
[3] Othen P J, Jenkins M L, Smith G D W, Phythian W J. Philos Mag Lett, 1991; 64: 383
[4] Othen P J, Jenkins M L, Smith G D W. Philos Mag, 1994; 70A: 1
[5] Xu G, Chu D F, Cai L L, Zhou B X, Wang W, Peng J C. Acta Metall Sin, 2011; 47: 905
[5] (徐 刚, 楚大锋, 蔡琳玲, 周邦新, 王 伟, 彭剑超. 金属学报, 2011; 47: 905)
[6] Isheim D, Kolli R P, Fine M E, Seidman D N. Scr Mater, 2006; 55: 35
[7] Miller M K, Russell K F. J Nucl Mater, 2007; 371: 145
[8] Sen I, Amankwah E, Kumar N S, Fleury E, Oh-ishi K, Hono K, Ramamurty U. Mater Sci Eng, 2011; A528: 4491
[9] Chi C Y, Dong J X, Liu W Q, Xie X S. Acta Metall Sin, 2010; 46: 1141
[9] (迟成宇, 董建新, 刘文庆, 谢锡善. 金属学报, 2010; 46: 1141)
[10] Isheim D, Vaynman S, Fine M E, Seidman D N. Scr Mater, 2008; 59: 1235
[11] Burnett H C, Duff R H, Vacher H C. J Res Natl Bur Stand, 1962; 66C: 113
[12] Irvine K J. J Iron Steel Inst, 1962; 200: 820
[13] Guo Z, Sha W, Vaumousse D. Acta Mater, 2003; 51: 101
[14] Ping D H, Ohnuma M, Hirakawa Y, Kadoya Y, Hono K. Mater Sci Eng, 2005; A394: 285
[15] Zhang Z W, Liu C T, Miller M K, Wang X L, Wen Y, Takeshi F, Akihiko H, Chen M W, Chen G, Bryan A C. Sci Rep, 2013; 3: 1
[16] Vaynman S, Isheim D, Kolli R P, Bhat S P, Seidman D N, Fine M E. Metall Mater Trans, 2008; 39A: 363
[17] Xiang H L, Fan J C, Liu D, Guo P P. Acta Metall Sin, 2012; 48: 1081
[17] (向红亮, 范金春, 刘 东, 郭培培. 金属学报, 2012; 48: 1081)
[18] Miller M K. Atom Probe Tomography: Analysis at the Atomic Level. New York: Kluwer Academic/Plenum Publishers, 2000: 11, 160
[19] Dmitrieva O, Ponge D, Inden G, Millán J, Choi P, Sietsma J, Raabe D. Acta Mater, 2011; 59: 364
[20] Kolli R P, Mao Z G, Seidman D N, Keane D T. Appl Phys Lett, 2007; 91: 241903
[21] Wang X J, Zhou C B, Zhang W R, Liu W Q. Shanghai Met, 2012; 34(4): 20
[21] (王晓姣, 周昌兵, 张伟荣, 刘文庆. 上海金属, 2012; 34(4): 20)
[22] Bacon D J, Harry T. Acta Mater, 2002; 50: 195
[23] Miracle D B. Acta Metall Mater, 1993; 41: 649
[24] Kolli R P, Seidman D N. Acta Mater, 2008; 56: 2073
[25] Thompson S W, Krauss G. Metall Mater Trans, 1996; 27A: 1573
[26] Thompson S W, Krauss G, Tseng C C. J Mater Sci Lett, 1998; 17: 2075
[27] Ricks R A, Howell P R, Honeycombe W K. Met Sci, 1980; 14: 562
Outlines

/

〈 〉