HIGH POWER PULSED MAGNETRON SPUTTERING DISCHARGE BEHAVIOR OF VARIOUS TARGET MATERIALS
Received date: 2014-06-26
Revised date: 2014-04-04
Online published: 2014-10-25
Supported by
Supported by National Natural Science Foundation of China (Nos.51301004 and U1330110)
Great interesting is induced by high power pulsed magnetron sputtering (HPPMS) for its high ionization of the sputtered materials, while the complex discharge puts of its applications in industry. The HPPMS discharge behaviors of various materials with different sputtering yields (Cu, Cr, Mo, Ti, V and C) were studied. The discharges of all the materials show a phasic discharge characteristic of five continuous stages. However, the target voltage of the same discharge stage of the material increases firstly, and decreases then with the increase of the sputtering yields, exhibiting a missing of certain discharge stage. The statistics of the mean values, peaks and platforms of the target currents show that self-sputtering and stable platform happen easily to the materials with high sputtering yields which is suitable for the thin films deposition by HPPMS, whereas gas discharge is dominated in the discharge of the materials with low sputtering yields, which is difficult in the using of HPPMS. Additional, the target current is mainly contributed to the platform (metal discharge) to the materials with high sputtering yields and the peaks (gas discharge) to the materials with low sputtering yields, respectively.
Zhongzhen WU , Xiubo TIAN , Feng PAN , K Y R FU , K P CHU . HIGH POWER PULSED MAGNETRON SPUTTERING DISCHARGE BEHAVIOR OF VARIOUS TARGET MATERIALS[J]. Acta Metall Sin, 2014 , 50(10) : 1279 -1284 . DOI: 10.11900/0412.1961.2014.00160
| [1] | Wan L J, Chen B Q, Guo K X. Acta Metall Sin, 1988; 24: 443 |
| [1] | (万立骏, 陈宝清, 郭可信. 金属学报, 1988; 24: 443) |
| [2] | Li Z G, Yu H L, Wu Y X, Miyake S. Acta Metall Sin, 2006; 42: 993 |
| [2] | (李铸国, 俞海良, 吴毅雄, 三宅正司. 金属学报, 2006; 42: 993) |
| [3] | Kouznetsov V, Maca′k K, Schneider J M. Surf Coat Technol, 1999; 122: 290 |
| [4] | Bohlmark J, Gudmundsson J T, Alami J, Latteman M, Helmersson U. IEEE Trans Plasma Sci, 2005; 33: 346 |
| [5] | Bohlmark J, Lattemann M, Gudmundsson J T, Ehiasarian A P, Gonzalvo Y A, Brenning N, Helmersson U. Thin Solid Films, 2006; 515: 1522 |
| [6] | Horwat D, Anders A. J Phys, 2008; 41D: 135210 |
| [7] | Ehiasarian A P, Gonzalvo Y A, Whitmore T D. Plasma Processes Polym, 2007; 4: S309 |
| [8] | Huang M D, Lin G Q, Dong C. Acta Metall Sin, 2003; 39: 510 |
| [8] | (黄美东, 林国强, 董 闯. 金属学报, 2003; 39: 510) |
| [9] | Xiao J Q, Lang W C, Zhao Y H, Gong J, Sun C, Wen L S. Acta Metall Sin, 2011; 47: 566 |
| [9] | (肖金泉, 郎文昌, 赵彦辉, 宫 骏, 孙 超, 闻立时. 金属学报, 2011; 47: 566 |
| [10] | Duan W Z. Master Thesis, Harbin Institute of Technology, 2010 |
| [10] | (段伟赞. 哈尔滨工业大学硕士学位论文, 2010) |
| [11] | Gudmundsson J T, Brenning N, Lundin D, Helmersson U. J Vac Sci Technol, 2012; 30A: 030801 |
| [12] | Christie D J. Czech J Phys, 2006; 56: B93 |
| [13] | Wu Z Z, Tian X B, Cheng S D, Gong C Z, Yang S Q. Acta Metall Sin, 2012; 48: 283 |
| [13] | (吴忠振, 田修波, 程思达, 巩春志, 杨士勤. 金属学报, 2012; 48: 283) |
| [14] | Daniel L, Nils B, Daniel J, Larsson P, Wallin E, Lattemann M, Raadu M A, Helmersson U. Plasma Sources Sci Technol, 2009; 18: 045008 |
| [15] | Magnus F, Sveinsson O B, Olafsson S, Gudmundsson J T. J Appl Phys, 2011; 110: 083306 |
| [16] | Yushkov G Y, Anders A. IEEE Trans Plasma Sci, 2010; 38: 3028 |
| [17] | Nakano T, Murata C, Baba S. Vacuum, 2010; 84: 1368 |
| [18] | Anders A. J Appl Phys, 2007; 102: 113303 |
| [19] | Capek J, Hala M, Zabeida O, Klemberg-Sapieha J E, Martinu L. J Appl Phys, 2012; 111: 023301 |
| [20] | Sigmund P. Phys Rev, 1969; 184: 383 |
| [21] | Wu Z Z, Tian X B, Duan W Z, Gong C Z, Yang S Q. Chin J Mater Res, 2010; 24: 561 |
| [21] | (吴忠振, 田修波, 段伟赞, 巩春志, 杨士勤. 材料研究学报, 2010; 24: 561) |
| [22] | Matsunami N, Yamamura Y, Yukikazu I, Noriaki I, Yukio K, Miyagawa S, Morita K, Shimizu R, Tawara H. At Data Nucl Data Tables, 1984; 31: 1 |
| [23] | Tian X B, Wu Z Z, Shi J W, Li X P, Gong C Z, Yang S Q. Chin Vac, 2010; 47(3): 44 |
| [23] | (田修波, 吴忠振, 石经纬, 李希平, 巩春志, 杨士勤. 真空, 2010; 47(3): 44) |
| [24] | Wu Z Z, Tian X B, Pan F,Fu R K Y, Chu P K. Acta Phys Sin, 2014; 17: 175201 |
| [24] | (吴忠振, 田修波, 潘 锋, Ricky K.Y Fu, 朱剑豪. 物理学报, 2014; 17: 175201) |
| [25] | Vozniy O V, Duday D, Lejars A, Wirtz T. Plasma Sources Sci Technol, 2011; 20: 06500801 |
| [26] | Vitelaru C, Lundin D, Stancu G D, Brenning N, Bretagne J, Minea T. Plasma Sources Sci Technol, 2012; 21: 025010 |
| [27] | Horwat D, Anders A. J Appl Phys, 2010; 108: 123306 |
| [28] | Anders A. Appl Phys Lett, 2008; 92: 201501 |
| [29] | Wiatrowski A, Posadowski W M, Radzimski Z J. J Phys: Conference Ser, 2008; 100: 062004 |
| [30] | Vetushka A, Ehiasarian A P. J Phys, 2008; 41D: 015204 |
/
| 〈 |
|
〉 |