ELECTROCHEMICAL CORROSION BEHAVIOR OF PCB-HASL IN NaHSO3/Na2SO3 SOLUTION
Received date: 2014-02-25
Revised date: 2014-02-25
Accepted date: 2014-05-27
Online published: 2014-10-25
Supported by
Supported by National Natural Science Foundation of China (No.51271032)
With the innovation of electronic technology, integration and miniaturization become the future developing direction of printed circuit board (PCB). Meanwhile, the corrosion problems of PCB also stand out more clearly, and even trace amounts of corrosion products will have a serious impact on the reliability of PCB. Under the actual condition for use, like sulfur-containing industrial environment, due to the diurnal temperature variations or/and the temperature field fluctuations for PCB itself, condensation phenomenon is likely to occur. Furthermore, as a result of the moisture absorption effect of granular deposit or supersaturated humidity, a layer of electrolyte solution will be formed on the surface of PCB, causing electrochemical corrosion. In this work, electrochemical impedance spectroscopy (EIS) and scanning Kelvin probe (SKP) techniques were used to study the corrosion behavior and mechanism of hot air solder leveling printed circuit boards (PCB-HASL) in a simulated electrolyte 0.1 mol/L NaHSO3 and 0.1 mol/L NaHSO3/Na2SO3 solutions with different pH values, and the influences of immersion time and pH value on the change of corrosion mechanism were discussed. Meanwhile, with the aids of OM, SEM combined with EDS, the nucleation and propagation processes of corrosion products on the surface of PCB-HASL were observed and analyzed. SEM and EDS results showed that the corrosion behavior of PCB-HASL in acid simulation solution was similar to pitting corrosion, and the corrosion pits were in a state of accelerated expansion at the early immersion stage. The corrosion products mainly consisted of oxides and sulfates of Sn. EIS and SKP analysis indicated that the PCB-HASL surface could be activated by NaHSO3 solution and pitting nucleation process only occurred at the early immersion stage. In the neutral or alkaline solution system of NaHSO3/Na2SO3, pitting corrosion couldn't occur, and the transmission of the electrolyte to the electrode interface through the oxide film was the control step of the corrosion reaction.
Key words: PCB; HASL; NaHSO3 solution; electrochemical corrosion; SKP
Kangkang DING , Kui XIAO , Shiwen ZOU , Chaofang DONG , Ruitao ZHAO , Xiaogang LI . ELECTROCHEMICAL CORROSION BEHAVIOR OF PCB-HASL IN NaHSO3/Na2SO3 SOLUTION[J]. Acta Metall Sin, 2014 , 50(10) : 1269 -1278 . DOI: 10.11900/0412.1961.2014.00087
| [1] | Leygraf C, Graedel T.Atmospheric Corrosion. New York: John Wiley&Sons Inc, 2000: 142 |
| [2] | Zhao Y, Lin C J, Li Y, Du R G, Wang J R. Acta Phys-Chim Sin, 2007; 23: 1342 |
| [2] | (赵 岩, 林昌健, 李 彦, 杜荣归, 王景润. 物理化学学报, 2007; 23: 1342) |
| [3] | Huang H L, Dong Z H, Chen Z Y, Guo X P. Corros Sci, 2011; 53: 1230 |
| [4] | Zou S W, Li X G, Dong C F, Ding K K, Xiao K. Electrochim Acta, 2013; 114: 363 |
| [5] | Xiao K, Zou S W, Dong C F, Wu J S, Li X G. Sci Technol Rev, 2011; 29: 25 |
| [5] | (肖 葵, 邹士文, 董超芳, 吴俊升, 李晓刚. 科技导报, 2011; 29: 25) |
| [6] | Qi H, Ganesan S, Pecht M. Microelectron Reliab, 2008; 48: 663 |
| [7] | Shibutani T, Yu Q, Shiratori M, Pecht M G. Microelectron Reliab, 2008; 48: 1033 |
| [8] | Fukuda Y, Osterman M, Pecht M. Microelectron Reliab, 2007; 47: 88 |
| [9] | Park Y W, Sankara Narayanan T S N, Lee K Y. Tribol Int, 2008; 41: 616 |
| [10] | Ammar I A, Darwish S, Khalil M W, Galal A. Materialwissenschaft und Werkstofftechnik, 1983; 14: 330 |
| [11] | Jouen S, Hannoyer B, Piana O. Surf Interf Anal, 2002; 34: 192 |
| [12] | Muller J. PhD Dissertation, Université Paris Est Marne-La-Vallée, 2010 |
| [13] | Lundren G, Wernfors G, Yamaguchi T. Acta Crystallogr, 1982; 38B: 2357 |
| [14] | Ahmed M A K, Fjellvag H, Kjekshus A. Acta Chem Scand, 1998; 52: 305 |
| [15] | Zou S W, Li X G, Dong C F, Li H Y, Xiao K. Acta Metall Sin, 2012; 48: 687 |
| [15] | (邹士文, 李晓刚, 董超芳, 李慧艳, 肖 葵. 金属学报, 2012; 48: 687) |
| [16] | Sun M, Xiao K, Dong C F, Li X G, Zhong P. Acta Metall Sin, 2011; 47: 442 |
| [16] | (孙 敏, 肖 葵, 董超芳, 李晓刚, 钟 平. 金属学报, 2011; 47: 442) |
| [17] | Li P H. Master Thesis, University of Science and Technology Beijing, 2011 |
| [17] | (李朴华. 北京科技大学硕士学位论文, 2011) |
| [18] | Rohwerder M, Turcu F. Electrochim Acta, 2007; 53: 290 |
| [19] | Cao C N,Zhang J Q.An Introduction to Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 54 |
| [19] | (曹楚南,张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 54) |
| [20] | Chen Z Y. PhD Dissertation, Huazhong University of Science & Technology, Wuhan, 2010 |
| [20] | (陈振宇. 华中科技大学博士学位论文, 武汉, 2010) |
| [21] | Cao B. Master Thesis, Nanjing Technology University, 2007 |
| [21] | (曹 斌. 南京工业大学硕士学位论文, 2007) |
| [22] | Zhao W M, Wang Y, Xue J, Wu K Y. Acta Metall Sin, 2005; 41: 178 |
| [22] | (赵卫民, 王 勇, 薛 锦, 吴开源. 金属学报, 2005; 41: 178) |
| [23] | Pourbaix M. Atlas of Electrochemical Equilibria in Aqueous Solutions. NewYork: Pergamon Press, 1966: 15 |
| [24] | Sasaki T, Kanagawa R, Ohtsuka T, Miura K. Corros Sci, 2003; 45: 847 |
| [25] | Yan Z, Xian A P. Trans Nonferrous Met Soc, 2012; 22: 1398 |
| [25] | (颜 忠, 冼爱平. 中国有色金属学报, 2012; 22: 1398) |
| [26] | Mori M, Miura K, Sasaki T, Ohtsuka T. Corros Sci, 2002; 44: 887 |
| [27] | Chang H, Chen H T, Li M Y, Wang L, Fu Y G. J Electron Mater, 2009; 38: 2170 |
/
| 〈 |
|
〉 |