MICROSTRUCTURE, MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF 1300 MPa GRADE 0.14C-2.72Mn-1.3Si STEEL
Revised date: 2014-03-17
Online published: 2014-10-25
Supported by
Supported by National Natural Science Foundation of China (No.51271035) and Fundamental Research Funds for the Central Universities (No.FRF-TP-10-001A)
Multiphase microstructure which contains ferrite, lath martensite, tempered martensite and a specific proportion of retained austenite with chemical composition of Mn between low Mn and medium Mn (0.14C-2.72Mn-1.3Si, mass fraction, %) belong to C-Si-Mn series was produced using continuous annealing simulator. By means of dilatometric simulation, SEM, TEM, EBSD and XRD, microstructures of the steels in different heat treatments were characterized. The results illustrate that the tested steel sheet gained good comprehensive properties with yield strength of 672 MPa, tensile strength up to 1333 MPa, total elongation A50 of 13% after annealing at 800 ℃, which can be explained by the refined microstructure, appropriate proportion of phases and a specific proportion of retained austenite. This work has deeply analyzed the work hardening behavior, discussed the change of instantaneous work hardening rate n. The multi-stage work hardening behavior was studied by modified C-J analysis, and explored the influence of ( is the volume fraction of martensite, is the equivalent diameter of martensite) and fraction of ferrite on it. The results show that n increases with the rise of true strain and then decreases, but has a different feature in the decrease for the different tested steels; the multi-stage work hardening behavior studied by modified C-J analysis shows 2 or 3 stages because of the different martensite volume fraction. The strain scope of combined action of ferrite and martensite △e is affected by the volume fraction of ferrite: △e is small when the temperature is low, and then △e is large when temperature increases, while the △e maybe small when temperature continue to rise. Above all, the high instantaneous work hardening rate which is helpful for the improvement of strength, plasticity and toughness can be attributed to the proportion, morphology and distribution of ferrite and martensite, which is also the consequence of coordination and combination action of each factor.
Zhengzhi ZHAO , Tingting TONG , Aimin ZHAO , Qing HE , Rui DONG , Fuqing ZHAO . MICROSTRUCTURE, MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF 1300 MPa GRADE 0.14C-2.72Mn-1.3Si STEEL[J]. Acta Metall Sin, 2014 , 50(10) : 1153 -1162 . DOI: 10.11900/0412.1961.2014.00113
| [1] | Hayami S, Furukawa T. Microalloying 75. New York: Union Carbide Corp, 1977: 311 |
| [2] | Matsumura O, Sakuma Y, Takechi H. Scr Metall, 1987; 21: 1301 |
| [3] | Sugimoto K, Misu M, Kobayashi M, Shirasawa H. ISIJ Int, 1993; 33: 775 |
| [4] | Bouaziz O, Guelton N. Mater Sci Eng, 2001 A319-321: 246 |
| [5] | Barnett M R. Mater Sci Eng, 2007; A464: 1 |
| [6] | Speer J G, Matlock D K, De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611 |
| [7] | Matlock D K, Brautigam V E, Speer J G. Mater Sci Forum, 2003; 426-432: 1089 |
| [8] | Jiang H T, Tang D, Mi Z L, Chen Y L. J Univ Sci Technol Beijing, 2010; 32: 201 |
| [8] | (江海涛, 唐 荻, 米振莉, 陈雨来. 北京科技大学学报, 2010; 32: 201) |
| [9] | Nouri A, Saghafian H, Kheirandish S. J Iron Steel Res Int, 2010; 17(5): 44 |
| [10] | Fan Y, Wang M L, Zhang H, Tao H B, Zhao P, Li S Q. J Univ Sci Technol Beijing, 2013; 35: 607 |
| [10] | (范 倚, 王明林, 张 慧, 陶红标, 赵 沛, 李士琦. 北京科技大学学报, 2013; 35: 607) |
| [11] | Zhong N, Wang X D, Wang L, Rong Y H. Mater Sci Eng, 2009; A506: 111 |
| [12] | Li Z, Zhao A M, Tang D, Mi Z L, Jiao D H. J Univ Sci Technol Beijing, 2012; 34: 132 |
| [12] | (李 振, 赵爱民, 唐 荻, 米振莉, 焦殿辉. 北京科技大学学报, 2012; 34: 132) |
| [13] | Zhang L Y, Wu D, Li Z. J Iron Steel Res Int, 2012; 19(2): 42 |
| [14] | Koh-ichi S, Daiki F, Nobuo Y. Procedia Eng, 2010; 2: 359 |
| [15] | Speich G R, Demarest V A, Miller R L. Metall Trans, 1981; 12A: 1419 |
| [16] | Sayed A A, Kheirandish Sh. Mater Sci Eng, 2012; A532: 21 |
| [17] | Rosenberg G, Sinaiová I, Juhar ?. Mater Sci Eng, 2013; A582: 347 |
| [18] | Yan S, Liu X H, Liu W J, Lan H F, Wu H Y. Acta Metall Sin, 2013; 49: 917 |
| [18] | (闫 述, 刘相华, 刘伟杰, 蓝慧芳, 吴红艳. 金属学报, 2013; 49: 917) |
| [19] | Wang C Y, Shi J, Cao W Q, Dong H. Acta Metall Sin, 2011; 47: 720 |
| [19] | (王存宇, 时 捷, 曹文权, 董 瀚. 金属学报, 2011; 47: 720) |
| [20] | Mohammad R A, Ekrami A. Mater Sci Eng, 2008; A477: 30 |
| [21] | Kang Y L, Kuang S, Yin X D. Automob Technol Mater, 2006; (5): 1 |
| [21] | (康永林, 邝 霜, 尹显东. 汽车工艺与材料, 2006; (5): 1) |
| [22] | Ren Y Q, Xie Z J, Shang C J. Acta Metall Sin, 2012; 48: 1074 |
| [22] | (任勇强, 谢振家, 尚成嘉. 金属学报, 2012; 48: 1074) |
| [23] | Li Y L. J Chongqing Univ (Nat Sci), 2001; 24(3): 58 |
| [23] | (李玉兰. 重庆大学学报(自然科学版), 2001; 24(3): 58) |
| [24] | Colla V, Sanctis D M, Dimatteo A. Metall Mater Trans, 2009; 40: 2557 |
| [25] | Nie W J, Shang C J, Guan H L, Zhang X B, Chen S H. Acta Metall Sin, 2012; 48: 298 |
| [25] | (聂文金, 尚成嘉, 关海龙, 张晓兵, 陈少慧. 金属学报, 2012; 48: 298) |
| [26] | Zhao Z Z, Ye J Y, Wang Z G, Zhao A M. J Shenyang Univ Technol, 2013; 35: 36 |
| [26] | (赵征志, 叶洁云, 汪志刚, 赵爱民. 沈阳工业大学学报, 2013; 35: 36) |
| [27] | Seyedrezai H, Pilkey A K, Boyd J D. Mater Sci Eng, 2014; A594: 178 |
| [28] | Mazinani M, Poole W J. Metall Mater Trans, 2007; 38A: 328 |
| [29] | Lanzillotto C A N, Pickering F B. Met Sci, 1982; 16: 371 |
| [30] | Ashby M F. Philos Mag, 1966; 14: 1157 |
| [31] | Ashby M F. Philos Mag, 1970; 21: 399 |
/
| 〈 |
|
〉 |