A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY

  • Chaoyang SUN ,
  • Jie HUANG ,
  • Ning GUO ,
  • Jing YANG
Expand
  • School of Mechanical Engineering, University of Science and Technology Beijing, Beijing 100083

Revised date: 2014-02-21

  Online published: 2014-09-25

Supported by

Supported by Joint Fund of National Natural Science Foundation of China and Chinese Academy of Engineering Physics (No.U1330121), National Natural Science Foundation of China (No.51105029) and Beijing Science Foundation of China (No.3112019)

Abstract

Based on the evolution of dislocation density and volume fraction of twins, a physically based constitutive model of Fe-22Mn-0.6C twinning induced plasticity (TWIP) steel has been developed. By taking the influence of slip inside twins on the plastic deformation and the difference of the average Taylor factors between the twinned regions and matrix regions into account, the plastic strain at the representative element was presented as the weighted sum of matrix slip, twinning and slip in twinned regions in this model. A linear function between yield stress and strain rate with natural logarithm was established by considering the effect of strain rate on thermally activated stress. And then, The Euler method was adopted and the parameters of this model were obtained in order to describe as accurately as the experimental results. The results from the model are in good agreement with the experimental results and the average relative error is only 0.84%. Compared with the model free of slip and the model free of the difference of Taylor factor at twinned regions, the average relative error is reduced 1.1% and 2.9%, respectively. The interaction between two twins and the sliding mechanism and its impact on the macro-deformation were investigated. The results show that there is a negative correlation between gliding rate and twinning rate and slip rate decreases with the increase of twinning rate. When the twins become saturated, the twin rate decreases rapidly, being opposite to the slip rate. The yield stress increases and the rate of strain hardening remains approximately unchanged with the increase of strain rate.

Cite this article

Chaoyang SUN , Jie HUANG , Ning GUO , Jing YANG . A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY[J]. Acta Metall Sin, 2014 , 50(9) : 1115 -1122 . DOI: 10.11900/0412.1961.2014.00079

References

[1] Mi Z L, Tang D, Yan L, Guo J. J Mater Sci Technol, 2005; 21: 451
[2] Grassel O, Kruger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391
[3] Vercammen S, Blanpain B, De Cooman B C, Wollants P. Acta Mater, 2004; 52: 2005
[4] Frommeyer G, Brux U, Neumann P. ISIJ Int, 2003; 43: 438
[5] Bouaziz O. Scr Mater, 2012; 66: 982
[6] Wang S H, Liu Z Y, Zhang W N, Wang G D. Acta Metall Sin, 2009; 45: 573
[6] (王书晗, 刘振宇, 张维娜, 王国栋. 金属学报, 2009; 45: 573)
[7] Renard K, Jacques P J. Mater Sci Eng, 2012; A542: 8
[8] Bouaziz O, Allain S, Scott C P, Cugy P, Barbier D. Curr Opin Solid State Mater Sci, 2011; 15: 141
[9] Gutierrez-Urrutia I, Raabe D. Acta Mater, 2011; 59: 6449
[10] Yang P, Lu F Y, Meng L, Cui F E. Acta Metall Sin, 2010; 46: 657
[10] (杨 平, 鲁法云, 孟 利, 崔凤娥. 金属学报, 2010; 46: 657)
[11] Bouaziz O, Guelton N. Mater Sci Eng, 2001; A319: 246
[12] Allain S, Chateau J P, Bouaziz O. Mater Sci Eng, 2004; A387: 143
[13] Kim J, Estrin Y, Beladi H, Timokhina I, Chin K, Kim S, De Cooman B C. Metall Mater Trans, 2012; 43A: 479
[14] Johnson G R, Cook W H. Eng Fract Mech, 1985; 21: 31
[15] Zerilli F J, Armstrong R W. J Appl Phys, 1987; 61: 1816
[16] Salem A A, Kalidindi S R, Doherty R D, Semiatin S L. Metall Mater Trans, 2006; 37A: 259
[17] Salem A A, Kalidindi S R, Doherty R D. Acta Mater, 2003; 51: 4225
[18] Yu Y, Pan X X, Xie R Z, Zhang F J, Hu W J. Chin J Theory Appl Mech, 2012; 44: 334
[18] (余 勇, 潘晓霞, 谢若泽, 张方举, 胡文军. 力学学报, 2012; 44: 334)
[19] Wu Z Q, Tang Z Y, Li H Y, Zhang H D. Acta Metall Sin, 2012; 48: 593
[19] (吴志强, 唐正友, 李华英, 张海东. 金属学报, 2012; 48: 593)
[20] Koyama M, Sawaguchi T, Lee T, Lee C S, Tsuzaki K. Mater Sci Eng, 2011; A528: 7310
[21] Remy L. Acta Metall, 1978; 26: 443
[22] Voyiadjis G Z, Abed F H. Mech Mater, 2005; 37: 355
[23] Estrin Y, Mecking H. Acta Metall, 1984; 32: 57
[24] Mecking H, Kocks U F. Acta Metall, 1981; 29: 1865
[25] Ismael A M, Ahmed H, Johannes R. Mater Sci Eng, 2009; A504: 40
[26] Allain S, Chateau J P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387-389: 246
[27] Wang W H. Master Thesis, University of Science and Technology Beijing, 2012
[27] (王伟华. 北京科技大学硕士学位论文, 2012)
Outlines

/