EFFECT OF MICROSTRUCTURE EVOLUTION ON MECHANICAL PROPERTIES OF ULTRA-HIGH STRENGTH WEAR RESISTANCE STEEL

  • Biao JU ,
  • Huibin WU ,
  • Di TANG ,
  • Xuefu PAN
Expand
  • National Engineering Research Center for Advanced Rolling Technology, University of Science and Technology Beijing, Beijing 100083

Received date: 2013-11-27

  Revised date: 2013-11-27

  Online published: 2014-09-25

Supported by

Supported by High Technology Research and Development Program of China (No.2012AA03A508)

Cite this article

Biao JU , Huibin WU , Di TANG , Xuefu PAN . EFFECT OF MICROSTRUCTURE EVOLUTION ON MECHANICAL PROPERTIES OF ULTRA-HIGH STRENGTH WEAR RESISTANCE STEEL[J]. Acta Metall Sin, 2014 , 50(9) : 1055 -1062 . DOI: 10.11900/0412.1961.2013.00775

References

[1] Song W X. Physical Metallurgy. 2nd Ed., Beijing: Metallurgical Industry Press, 1989: 335
[1] (宋维锡.金属学. 第2版, 北京: 冶金工业出版社, 1989: 335)
[2] Krauss G. Mater Sci Eng, 1999; A273-275: 40
[3] Hutchinson B, Hagstr?m J, Karlsson O, Lindell D, Tornberg M, Lindberg F, Thuvander M. Acta Mater, 2011; 59: 5845
[4] Chatterjee S, Bhadeshia H. Mater Sci Technol, 2006; 22: 645
[5] Lee C G, Kim S J, Lee T H, Lee S. Mater Sci Eng, 2004; A371: 16
[6] Wang Y, Zhang K, Guo Z H, Chen N L, Rong Y H. Acta Metall Sin, 2012; 48: 641
[6] (王 颖, 张 柯, 郭正洪, 陈乃录, 戎咏华. 金属学报, 2012; 48: 641)
[7] Speer J G, Matlock D K,De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611
[8] Edmonds D V, He K, Rizzo F C,De Cooman B C, Matlock D K, Speer J G. Mater Sci Eng, 2006; 438-440: 25
[9] Clarke A J, Speer J G, Miller M K, Hackenberg R E, Edmonds D V, Matlock D K, Rizzo F C, Clarke K D, De Moor E. Acta Mater, 2008; 56: 16
[10] Misra R D K, Nathani H, Hartmann J E, Siciliano F. Mater Sci Eng, 2005; A394: 339
[11] Wang Y M,Li M Y,Wei G. Control Rolling and Control Cooling of the Steel Plates. 2nd Ed., Beijing: Metallurgical Industry Press, 2010: 50
[11] (王有铭,李曼云,韦 光. 钢材的控制轧制和控制冷却. 第2版, 北京: 冶金工业出版社, 2010: 50)
[12] Hutchinson C R, Zurob H S, Sinclair C W, Brechet Y J M. Scr Mater, 2008; 59: 635
[13] Hulka K, Kern A, Schriever U. Mater Sci Forum, 2005; 500-501: 519
[14] Hu R R, Cai Q W, Wu H B, Che Y J. J South China Univ Technol, 2013; 41: 1009
[14] (胡日荣, 蔡庆伍, 武会宾, 车英健. 华南理工大学学报, 2013; 41: 1009)
[15] Xu Z Y. Mater Sci Forum, 2007; 561-565: 2283
[16] Rong Y H. Acta Metall Sin, 2011; 47: 1483
[16] (戎咏华. 金属学报 2011; 47: 1483)
[17] Sahin Y, Erdogan M, Cerah M. Wear, 2008; 265: 196
[18] Xu X J, Xu W, Ederveen F H, Zwaag S. Wear, 2013; 301: 89
[19] Sarikaya M, Jhingan A K, Thomas G. Metall Trans, 1983; 14: 1121
[20] Lee W S, Su T T. J Mater Process Technol, 1999; 87: 198
[21] Park S G, Lee K H, Kim M C, Lee B S. Mater Sci Eng, 2013; A561: 277
[22] Zhong N, Wang X D, Wang L, Rong Y H. Mater Sci Eng, 2009; A506: 111
[23] Hashimoto S, Ikeda S, Sugimoto K I, Miyake S. ISIJ Int, 2004; 44: 1590
[24] Xu Z Y. Martensite Phase Transformation and Martensite. 2nd Ed.,Beijing: Science Press, 1999: 5
[24] (徐祖耀. 马氏体相变与马氏体. 第2版, 北京: 科学出版社, 1999: 5)
[25] Chilton J M, Kelly P M. Acta Metall, 1968; 16: 637
Outlines

/

〈 〉