EFFECT OF MICROSTRUCTURE EVOLUTION ON MECHANICAL PROPERTIES OF ULTRA-HIGH STRENGTH WEAR RESISTANCE STEEL |
JU Biao, WU Huibin(), TANG Di, PAN Xuefu |
National Engineering Research Center for Advanced Rolling Technology, University of Science and Technology Beijing, Beijing 100083 |
|
Cite this article:
JU Biao, WU Huibin, TANG Di, PAN Xuefu. EFFECT OF MICROSTRUCTURE EVOLUTION ON MECHANICAL PROPERTIES OF ULTRA-HIGH STRENGTH WEAR RESISTANCE STEEL. Acta Metall Sin, 2014, 50(9): 1055-1062.
|
|
Received: 27 November 2013
|
|
Fund: Supported by High Technology Research and Development Program of China (No.2012AA03A508) |
[1] |
Song W X. Physical Metallurgy. 2nd Ed., Beijing: Metallurgical Industry Press, 1989: 335
|
|
(宋维锡.金属学. 第2版, 北京: 冶金工业出版社, 1989: 335)
|
[2] |
Krauss G. Mater Sci Eng, 1999; A273-275: 40
|
[3] |
Hutchinson B, Hagström J, Karlsson O, Lindell D, Tornberg M, Lindberg F, Thuvander M. Acta Mater, 2011; 59: 5845
|
[4] |
Chatterjee S, Bhadeshia H. Mater Sci Technol, 2006; 22: 645
|
[5] |
Lee C G, Kim S J, Lee T H, Lee S. Mater Sci Eng, 2004; A371: 16
|
[6] |
Wang Y, Zhang K, Guo Z H, Chen N L, Rong Y H. Acta Metall Sin, 2012; 48: 641
|
|
(王 颖, 张 柯, 郭正洪, 陈乃录, 戎咏华. 金属学报, 2012; 48: 641)
|
[7] |
Speer J G, Matlock D K,De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611
|
[8] |
Edmonds D V, He K, Rizzo F C,De Cooman B C, Matlock D K, Speer J G. Mater Sci Eng, 2006; 438-440: 25
|
[9] |
Clarke A J, Speer J G, Miller M K, Hackenberg R E, Edmonds D V, Matlock D K, Rizzo F C, Clarke K D, De Moor E. Acta Mater, 2008; 56: 16
|
[10] |
Misra R D K, Nathani H, Hartmann J E, Siciliano F. Mater Sci Eng, 2005; A394: 339
|
[11] |
Wang Y M,Li M Y,Wei G. Control Rolling and Control Cooling of the Steel Plates. 2nd Ed., Beijing: Metallurgical Industry Press, 2010: 50
|
|
(王有铭,李曼云,韦 光. 钢材的控制轧制和控制冷却. 第2版, 北京: 冶金工业出版社, 2010: 50)
|
[12] |
Hutchinson C R, Zurob H S, Sinclair C W, Brechet Y J M. Scr Mater, 2008; 59: 635
|
[13] |
Hulka K, Kern A, Schriever U. Mater Sci Forum, 2005; 500-501: 519
|
[14] |
Hu R R, Cai Q W, Wu H B, Che Y J. J South China Univ Technol, 2013; 41: 1009
|
|
(胡日荣, 蔡庆伍, 武会宾, 车英健. 华南理工大学学报, 2013; 41: 1009)
|
[15] |
Xu Z Y. Mater Sci Forum, 2007; 561-565: 2283
|
[16] |
Rong Y H. Acta Metall Sin, 2011; 47: 1483
|
|
(戎咏华. 金属学报 2011; 47: 1483)
|
[17] |
Sahin Y, Erdogan M, Cerah M. Wear, 2008; 265: 196
|
[18] |
Xu X J, Xu W, Ederveen F H, Zwaag S. Wear, 2013; 301: 89
|
[19] |
Sarikaya M, Jhingan A K, Thomas G. Metall Trans, 1983; 14: 1121
|
[20] |
Lee W S, Su T T. J Mater Process Technol, 1999; 87: 198
|
[21] |
Park S G, Lee K H, Kim M C, Lee B S. Mater Sci Eng, 2013; A561: 277
|
[22] |
Zhong N, Wang X D, Wang L, Rong Y H. Mater Sci Eng, 2009; A506: 111
|
[23] |
Hashimoto S, Ikeda S, Sugimoto K I, Miyake S. ISIJ Int, 2004; 44: 1590
|
[24] |
Xu Z Y. Martensite Phase Transformation and Martensite. 2nd Ed.,Beijing: Science Press, 1999: 5
|
|
(徐祖耀. 马氏体相变与马氏体. 第2版, 北京: 科学出版社, 1999: 5)
|
[25] |
Chilton J M, Kelly P M. Acta Metall, 1968; 16: 637
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|