MICROSTRUCTURES AND LOW-CYCLE FATIGUE BEHAVIOR OF Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) ALLOY

  • Xin CHE ,
  • Xingkui LIANG ,
  • Lili CHEN ,
  • Lijia CHEN ,
  • Feng LI
Expand
  • 1 School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
    2 New Northeast Electric (Shenyang) High Voltage Switchgear Co. Ltd, Shenyang 110025
    3 Shenyang Aerosun-Futai Expansion Joint Co. Ltd, Shenyang 110141

Revised date: 2013-12-27

  Online published: 2014-09-25

Supported by

Supported by Science and Technology Research of Education Department of Liaoning Province (No.L2013056)

Abstract

The Al-Si-Cu-Mg cast aluminum alloys have high mechanical properties and good cast performance. Due to their excellent comprehensive properties, the Al-Si-Cu-Mg cast aluminum alloys have wide application, and have become one of the most important structural materials applied in the equipment manufacturing industry. Actually, many key components in practical engineering application are often subjected to the alternating load, and thus the fatigue failure has become an important factor which concerns the safety and economy for those structures used in various engineering fields. Although some researches for the fatigue behavior of aluminum alloys have been performed, mainly focus on the regularity understanding. Especially, the influences of rare earth elements and heat-treat condition on the low-cycle fatigue behavior of aluminum alloys have not been comprehensively revealed. Obviously, the investigation concerning the microstructure and fatigue property of the Al-Si-Cu-Mg cast aluminum alloys can not only provide the theoretical basis for the development of new type cast aluminum alloys but also the reliable theoretical foundation for the safety design and reasonable use of these alloys. In order to determine the influence of rare earth element Sc on the low-cycle fatigue behavior of casting Al-9.0%Si-4.0%Cu-0.4%Mg alloy with T6 treated state, the cyclic stress response behavior, fatigue life behavior and cyclic deformation mechanism of the Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) cast aluminum alloys with T6 treated states under low-cycle fatigue loading condition were investigated. The results show that at the low total strain amplitude, the Al-9.0%Si-4.0%Cu-0.4%Mg alloy exhibits the cyclic strain hardening during whole fatigue deformation, while the Al-9.0%Si-4.0%Cu-0.4%Mg-0.3%Sc alloys exhibit the cyclic strain hardening in the initial stage of fatigue deformation and then the stable cyclic stress response in the later stage of fatigue deformation. At the higher total strain amplitudes, the Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) alloys exhibit the cyclic strain hardening. The addition of Sc can effectively enhance the cyclic deformation resistance and prolong the fatigue lives of the Al-9.0%Si-4.0%Cu-0.4%Mg alloy with T6 treated state. At the lower total strain amplitudes, the cyclic deformation mechanism of the Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) alloys with T6 treated state is the plane slip, while at the higher total strain amplitudes, the cyclic deformation mechanism becomes the wavy slip.

Cite this article

Xin CHE , Xingkui LIANG , Lili CHEN , Lijia CHEN , Feng LI . MICROSTRUCTURES AND LOW-CYCLE FATIGUE BEHAVIOR OF Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) ALLOY[J]. Acta Metall Sin, 2014 , 50(9) : 1046 -1054 . DOI: 10.11900/0412.1961.2013.00843

References

[1] Wang X, Chen G Q, Li B, Wu L M, Jiang D M. Rare Met, 2010; 29(1): 66
[2] Mo D F, He G Q, Hu Z F, Zhang W H. J Mater Eng, 2010; (7): 92
[2] (莫德峰, 何国球, 胡正飞, 张卫华. 材料工程, 2010; (7): 92)
[3] Wang G Q, Bian X F, Wang W M, Zhang J Y. Mater Lett, 2003; 57: 4083
[4] Moizumi K, Mine K, Tezuka H, Sato T. Mater Sci Forum, 2002; 396-402: 1371
[5] Caceres C H, Griffiths J R, Reiner P. Acta Mater, 1996; 44: 15
[6] Wang Q G, Caceres C H, Griffiths J R. Metall Mater Trans, 2003;34A: 2901
[7] Cheng Z Z, Xie C H, Zhu C X. Light Met, 2010; (7): 58
[7] (陈振中, 解传浩, 朱成香. 轻金属, 2010; (7): 58 )
[8] Bray G H, Glazov M, Rioja R J, Li D, Gangloff R P. Int J Fatigue, 2001; 23: 265
[9] Manson S S. Exp Mech, 1965; 5: 193
[10] Nieslony A, Dsoki C E, Kaufmann H, Krug. Int J Fatigue, 2008; 30: 1967
[11] Miura Y, Joh C H, Katsube T. Mater Sci Forum, 2000; 331-337: 1031
[12] Zhou K, Li Y Q. Chin J Nonferrous Met, 1997; 7: 97
[12] (周 昆, 李云卿. 中国有色金属学报, 1997; 7: 97)
[13] Kendig K L, Miracle D B. Acta Mater, 2002; 50: 4165
[14] Li F, Wang Y, Chen L J, Zheng L, Zhou J Y. J Mater Sci, 2005; 40: 1529
[15] Kendig K L, Miracle D B. Acta Mater, 2004; 50: 4165
[16] Sj?lander E, Seifeddine S. J Mater Process Technol, 2010; 210: 1249
[17] Kim M, Hong Y, Cho H. Met Mater Int, 2004; 10: 513
[18] Zhou M Z. PhD Dissertation, Central South University, Changsha, 2010
[18] (周明哲. 中南大学博士学位论文, 长沙, 2010)
[19] Dvydov V G, Rostova T D, Zakharov V V, Filatov Y A, Yelagin V I. Mater Sci Eng, 2000; A280: 30
[20] Watanabe C, Jin C Y, Monzen R, Kitagawa K. Mater Sci Eng, 2004; A387-389: 552
[21] Lados D A, Apelian D. Mater Sci Eng, 2004; A385: 200
[22] Lee F T, Major J F, amuel F H. Metall Mater Trans, 1995; 26A: 1553
[23] Li M J, Hu H Y, Xing X S. Acta Phys Sin, 2003; 52: 2092
[23] (李眉娟, 胡海云, 邢修三. 物理学报, 2003; 52: 2092 )
[24] Yin Z M, Pan Q L, Zhang Y H, Jiang F. Mater Sci Eng, 2000; A280: 151
[25] Saisrinadh K V, Singh V. Metall Mater Trans, 2007; 38A: 1868
[26] Chen L J, Wu W, Liaw P K. Acta Metall Sin, 2006; 42: 952
[26] (陈立佳, 吴 崴, Liaw P K. 金属学报, 2006; 42: 952)
[27] Singh V, Sundararaman M, Chen W, Wahi R P. Metall Trans, 1991; 22A: 499
Outlines

/