THE DECOMPOSITION BEHAVIOR OF PRIMARY MC CARBIDE IN NICKEL BASE DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ444
Revised date: 2013-12-25
Online published: 2014-09-25
Supported by
Supported by National Natural Science Foundation of China (No.51001101)
Hot-corrosion directionally solidified Nickel base superalloy DZ444 is generally used as the candidate material for blade of gas turbine, which required excellent alloy microstructural stability. As one of the constitutional phase of the alloy, primary MC carbides are often thermally unstable, and its degradation reactions can happen when the alloys are in services or thermally exposed in high temperature circumstances. There existed several different kinds of MC decompostion reactions in some traditional Ni-based superalloys. To figure out the thermal stability of primary MC carbide in the DZ444 alloy and better understand its degradation mechanism, some related discussions to the thermal stability and degeneration process of primary MC carbide and its effects on the microstructure were made. In this work, microstructures of DZ444 alloy after long-term exposure up to 1×104 h at 800, 850 and 900 ℃ have been observed by OM, SEM and TEM. The results show that the thermal stability of MC was low. As long-term exposure proceeds, MC decompostion became more and more serious. Firstly, a typical sandwich microstructure (SM) gradually formed and thickened in the MC/g interface; secondly, h phase precipitated in the SM/MC interface; lastly, h-M6C and h-M23C6 locally precipitated inside the h phase. Finally, SM structure, h phase, h-M6C and h-M23C6 successively formed in MC degeneration areas at three stages of its decomposition process. Basically, MC decompostion process could be described with such raction formula as follows: MC+g→SM-M23C6+SM-M6C+SM-g'→SM-M23C6+SM-M6C+SM-g'+h→SM-M23C6+SM-M6C+SM-g'+h+h-M6C+h-M23C6. Generally, the type of secondary carbide from MC degeneration was M23C6, and, with the increase of long-term exposure temperature and time, the amount of secondary M6C carbide slightly increased. Besides, MC degeneration might result in the precipitation of transgranular M23C6 carbide and s phase in the vicinity of MC degeneration areas, and the coarsening of grain boundary (GB).
Xuan XIAO , Chao ZENG , Jieshan HOU , Xuezhi QIN , Jianting GUO , Lanzhang ZHOU . THE DECOMPOSITION BEHAVIOR OF PRIMARY MC CARBIDE IN NICKEL BASE DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ444[J]. Acta Metall Sin, 2014 , 50(9) : 1031 -1038 . DOI: 10.11900/0412.1961.2013.00836
| [1] | Wang J, Zhou L Z, Sheng L Y, Guo J T. Mater Des, 2012; 39: 55 |
| [2] | Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Mater Sci Eng, 2012; A543: 121 |
| [3] | Guo J T. Materials Science and Engineering for Superalloys I. Beijing: Science Press, 2008: 4 |
| [3] | (郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 4) |
| [4] | Collins H E, Quigg R J. Trans ASM, 1968; 61: 139 |
| [5] | Wu Q Y, Song H, Swindeman R W, Shingledecker J P, Vasudevan V K. Metall Mater Trans, 2008; 39A: 2569 |
| [6] | Zhao S Q, Xie X S, Gaylord S D, Shailesh P J. Mater Des, 2006; 27: 1120 |
| [7] | Hou J S, Zhou L Z, Yuan C, Tang Z, Guo J T, Qin X Z, Liaw P K. Mater Sci Eng, 2013; A560: 25 |
| [8] | Choi B G, Kim I S, Kim D H, Jo C Y. Mater Sci Eng, 2008; A478: 329 |
| [9] | Huang X B, Kang Y, Zhou H H, Zhang Y, Hu Z Q. Mater Lett, 1998; 36: 210 |
| [10] | Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2003; A361: 191 |
| [11] | He L Z, Zheng Q, Sun X F, Hou G C, Guan H R, Hu Z Q. Mater Sci, 2005; 40: 2959 |
| [12] | Qin X Z, Guo J T, Yuan C, Chen C L, Hou J S, Ye H Q. Mater Sci Eng, 2008; A485: 75 |
| [13] | Hou J S, Guo J T, Yang G X, Zhou L Z, Qin X Z, Ye H Q. Mater Sci Eng, 2008; A498: 449 |
| [14] | Stevens R A, Flewitt P E J. Mater Sci Eng, 1979; 37: 237 |
| [15] | Nazmy M, Staubli M. Scr Metall Mater, 1990; 24: 135 |
| [16] | Wang J, Zhou L Z, Qin X Z, Sheng L Y, Hou J S, Guo J T. Mater Sci Eng, 2012; A553: 14 |
| [17] | Lvov G, Levit V I, Kaufman M J. Metall Mater Trans, 2004; 35A: 1672 |
| [18] | Sims C T, Stoloff N S, Hagel W C. Superalloys II. New York: John Wiley & Sons Inc., 1987: 122 |
| [19] | Tawancy H M, Abbas N M, Al-Mana A I, Rhysjones T N. J Mater Sci, 1994; 29: 2445 |
| [20] | Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Acta Metall Sin, 2010; 46: 216 |
| [20] | (秦学智, 郭建亭, 袁 超, 侯介山, 周兰章, 叶恒强. 金属学报. 2010; 46: 216) |
| [21] | Qin X Z. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007 |
| [21] | (秦学智. 中国科学院金属研究所博士学位论文, 沈阳, 2007) |
| [22] | Cyril W, Water B, Robert F M. J Metall Trans AIME, 1950; 188: 558 |
| [23] | Fujiwara K, Horita Z. Acta Mater, 2002; 50: 1578 |
| [24] | Minamino Y, Jung S B, Yamane T, Hirao K. Metall Trans, 1992; 23A: 2784 |
| [25] | Karunaratne M S A, Carter P, Reed R C. Acta Metall, 2001; 49: 861 |
| [26] | Watanable M, Horita Z, Smith D J, McCartney M R, Sano T, Nemoto M. Acta Metall, 1994; 42: 3381 |
/
| 〈 |
|
〉 |