EFFECTS OF O, N AND Ni CONTENTS ON HOT PLASTICITY OF 0Cr25Ni7Mo4N DUPLEX STAINLESS STEEL

  • Yulai CHEN ,
  • Tairan ZHANG ,
  • Yide WANG ,
  • Jingyuan LI
Expand
  • 1 Metallurgical Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083
    2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2014-01-27

  Revised date: 2014-04-28

  Online published: 2014-08-25

Supported by

Supported by National Natural Science Foundation of China (No.51174026), National Science and Technology Pillar Program during the Twelfth Five-Year Plan Period (No.2012BA-E04B02)

Abstract

In order to identity the effect of narrow composition control on the hot plasticity of duplex stainless steel, hot rolling test of OCr25Ni7Mo4N steels with various oxygen, nitrogen and nickel contents were performed at 1200 ℃ for 4 steps. The microstructures and inclusions were observed by OM, SEM and EBSD. The steels with the lowest oxygen, nitrogen and nickel contents showed excellent hot plasticity. The inclusions in the steel with 0.0059% oxygen were mainly Al2O3 and MgO·Al2O3, which distributed in the grain interior and did no harm to the hot plasticity of the steel. The steels containing 0.038% and 0.046% oxygen actually cracked at the sheet edge during hot rolling, which resulted from the large inclusion particles of Cr2O3 and MnO2 at the α/γ boundary. Furthermore, the reason for more serious cracking occurred in the steel containing 0.038% oxygen than that containing 0.046% oxygen was its relatively higher contents of nitrogen and nickel, making γ volume fraction of the steel as high as 60% in the hot rolling state. Excessive γ reduced its total strain, so that the inadequate stain did not induce the recrystallization of γ phase, which resulted in hot rolling cracking finally.

Cite this article

Yulai CHEN , Tairan ZHANG , Yide WANG , Jingyuan LI . EFFECTS OF O, N AND Ni CONTENTS ON HOT PLASTICITY OF 0Cr25Ni7Mo4N DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 2014 , 50(8) : 905 -912 . DOI: 10.11900/0412.1961.2014.00057

References

[1] Wu J. Duplex Stainless Steel. Beijing: Metallurgy Industry Press, 1999: 1
[1] (吴 玖. 双相不锈钢. 北京: 冶金工业出版社, 1999: 1)
[2] Fang Y L, Liu Z Y, Zhang W N, Wang G D, Song H M, Jiang L Z. Acta Metall Sin, 2010; 46: 641
[2] (方轶琉, 刘振宇, 张维娜, 王国栋, 宋红梅, 江来珠. 金属学报, 2010; 46: 641)
[3] Fan G W, Liu J, Han P D, Qiao G J. Mater Sci Eng, 2009; A515: 108
[4] Han Y, Zou D N, Chen Z Y, Fan G W, Zhang W. Mater Charact, 2011; 62: 198
[5] Chen L, Wang L M, Du X J. Acta Metall Sin, 2010; 46: 52
[5] (陈 雷, 王龙妹, 杜晓建. 金属学报, 2010; 46: 52)
[6] Iza-Mendia A, Pinol-Juez A, Urcola J J. Metall Mater Trans, 1998; 29A: 2975
[7] Alvarez-Armas I, Marinelli M C, Herenu S. Acta Mater, 2006; 54: 5041
[8] Jia N, Lin P R, Wang Y D. Acta Mater, 2008; 56: 782
[9] Weatherly G C, Hamble P, Borland D. Acta Metall, 1979; 27: 1815
[10] Dahmen U, Ferguson P, Westmacott K H. Acta Metall, 1984; 32: 803
[11] Qiu D, Zhang W Z. Acta Mater, 2007; 55: 6754
[12] Song Z, Zheng W, Feng H. J Iron Steel Res Int, 2013; 20: 83
[13] Song Z G, Wu J, Lin X J. J Iron Steel Res Int, 2011; 18: 64
[14] Fang Y L, Liu Z Y, Song H M. Mater Sci Eng, 2009; A526: 128
[15] Jiang Z L, Wu Y, Chen X Y, Bai F M, Liu X Y, Huang T G. J Mater Eng, 2002; (5): 30
[15] (姜忠良, 吴 严, 陈秀云, 白飞明, 刘秀赢, 黄铁光. 材料工程, 2002; (5): 30)
[16] Chen P D, Wang J H, Ma Z W. Phys Examination Test, 2012; 30(3): 11
[16] (陈培敦, 王俊海, 马正伟. 物理测试, 2012; 30(3): 11)
[17] Shen P, Yan H T, Yang Z, Yuan H. Hot Working Technol, 2013; 42(4): 50
[17] (申 鹏, 颜海涛, 杨 振, 袁 辉. 热加工工艺, 2013; 42(4): 50)
[18] Wu Z Z, Song Z G, Zheng W J, Chen B, Lu J S. Spec Steel, 2006; 27(4): 11
[18] (吴忠忠, 宋志刚, 郑文杰, 陈 斌, 陆建生. 特殊钢, 2006; 27(4): 11)
[19] Yang Q X, Wu J, Zhao H. Trans Mater Heat Treat, 2006; 26: 124
[19] (杨庆祥, 吴 晶, 赵 宏. 材料热处理学报, 2006; 26: 124)
Outlines

/

〈 〉