INFLUENCE OF HEAT TREATMENT ON LOW-CYCLE FATIGUE BEHAVIOR OF EXTRUDED Mg-7%Zn-0.6%Zr-0.5%Y ALLOY

  • Siqian ZHANG ,
  • Wei WU ,
  • Lili CHEN ,
  • Xin CHE ,
  • Lijia CHEN
Expand
  • 1 School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
    2 Shenyang Aerosun-Futai Expansion Joint Co. Ltd, Shenyang 110141
null

Received date: 2013-12-02

  Revised date: 2014-03-31

  Online published: 2014-06-20

Abstract

The low-cycle fatigue tests have been conducted for the Mg-7%Zn-0.6%Zr-0.5%Y alloys (mass fraction) subjected to extrusion, aging (T5) and solution plus aging (T6) treatment, respectively. The influence of heat treatment on the fatigue deformation behavior of the alloy has also been systematically investigated. The results show that T5 and T6 treatment can improve the cyclic deformation resistance of Mg-7%Zn-0.6%Zr-0.5%Y alloys. T5 treatment can reduce the fatigue life of the alloy. However, T6 treatment can improve the fatigue life at high total strain amplitudes, and reduce the fatigue life at low total strain amplitudes. The relationship between elastic strain amplitude, plastic strain amplitude and reversals to failure of the alloys can be described by Basquin and Coffin-Manson equations, respectively. For the alloys subjected to both T5 and T6 treatments, the increase in the cyclic deformation resistance is mainly due to the formation of long period stacking ordered (LPSO) phase. The twins formed during the fatigue deformation may be responsible for the decrease in the fatigue life of the alloy subjected to T5 treatment.

Cite this article

Siqian ZHANG , Wei WU , Lili CHEN , Xin CHE , Lijia CHEN . INFLUENCE OF HEAT TREATMENT ON LOW-CYCLE FATIGUE BEHAVIOR OF EXTRUDED Mg-7%Zn-0.6%Zr-0.5%Y ALLOY[J]. Acta Metall Sin, 2014 , 50(6) : 700 -706 . DOI: 10.3724/SP.J.1037.2013.00781

References

[1] Avedsain M M, Baker H. Magnesium and Magnesium Alloys. Materials Park, Ohio: ASM International, 1999: 7
[2] Polmear I J. Mater Sci Technol, 1994; 10: 1
[3] Nishikawa Y. Funct Mater, 1999; 19(6): 21
[4] Horikir H, Kato A, Inoue A, Masumoto T. Mater Sci Eng, 1994; A179: 702
[5] Lee S, Lee S H, Kim D H. Metall Mater Trans, 1998; 29A: 1221
[6] Payne R J M, Bailey N. J Inst Met, 1960; 88: 417
[7] Unsworth W. Int J Mater Prod Technol, 1989; 4: 1359
[8] Drits M E, Sviderkaya Z A, Rokhlin L L, Nikitina N I. Met Sci Heat Treat, 1979; 21: 887
[9] Zhao H D, Qin G W, Ren Y P, Pei W L, Chen D, Guo Y. J Alloys Compd,?2011; 509: 627
[10] Wang J, Zhang D P, Fang D Q, Lu H Y, Tang D X, Zhang J H, Meng J. J Alloys Compd,?2008; 454: 194
[11] Luo S Q, Tang A T, Pan F S, Song K, Wang W Q. Trans Nonferrous Met Soc China,?2011; 21: 795
[12] Xu D K, Tang W N, Liu L, Xu Y B, Han E H. J Alloys Compd,?2007; 432: 129
[13] Coffin L F. Trans Am Soc Mech Eng, 1954; 76: 931
[14] Coffin L F. Met Trans, 1972; 3: 1777
[15] Basquin O H. Proc Am Soc Test Mater, 1990; 10: 626
[16] Suresh S, translated by Wang Z G. Fatigue of Materials. Beijing: National?Defence?Industry?Press, 1999: 158
[16] (Suresh S 著,王中光 译. 材料的疲劳. 北京: 国防工业出版社, 1999: 158)
[17] Eliezer A, Gutman E M, Abramov E, Unigovski Y. J Light Met, 2001; 1: 179
[18] Hilpert M, Wagner L. J Mater Eng Perform, 2000; 9: 402
[19] Xu D K, Liu L, Xu Y B, Han E H. J Alloys Compd,?2008; 454: 123
[20] Kawamura Y, Hayashi K, Inoue A, Masumoto T. Metall Trans, 2001; 42: 1172
[21] Jiang L, Jonas J J, Mishra R K, Luo A A, Sachdev A K, Godet S. Acta Mater, 2007; 55: 3899
[22] Kawamura Y, Hayashi K, Inoue A, Masumoto T. Mater Trans, 2001; 42: 1172
[23] Hagihara K, Yokotani N, Umakoshi Y. Intermetallics, 2010; 18: 267
[24] Yang X, Miura H, Sakai T. Mater Trans, 2003; 44: 197
[25] Tome C N, Agnew S R, Blumenthal W R, Bourke M A M, Kaschner G C, Rangaswamy P. Mater Sci Forum, 2003; 408-412: 263
[26] Christian J W, Mahajant S. Prog Mater Sci, 1995; 39: 1
[27] Jiang L, Jonas J J, Luo A A, Sachdev A K, Godet S. Mater Sci Eng, 2007; 445-446: 302
[28] Jain A, Duygulu O, Brown D W, Tome C N, Agnew S R. Mater Sci Eng, 2008; 486: 545
Outlines

/