SHORT-TERM PROCESS OF RECYCLING CEMENTED CARBIDE SCRAPS AND PREPARATION OF HIGH PERFORMANCE HARD METALS

  • Yao WANG ,
  • Xuemei LIU ,
  • Xiaoyan SONG ,
  • Chongbin WEI ,
  • Haibin WANG ,
  • Xilong WANG
Expand
  • Key Laboratory of Advanced Functional Materials, College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124
null

王 瑶, 男, 1988年生, 硕士生

Revised date: 2013-09-13

  Online published: 2014-05-20

Supported by

National High Technology Research and Development Program of China (No.SS2013AA031401), National Natural Science Foundation of China (No.51174009),Natural Science Foundation of Beijing (Nos.2131001 and 2133062) and Fund of State Key Laboratory of New Metal Materials (No.2012-Z08)

Abstract

Recycling of cemented carbide scraps is drawing more and more attention to companies and countries all over the world. However, the recycling method has always been a problem where there are many factors involved. The feasibility, recycling rate, energy consumption and the environment conservation are all significant factors for the recycling method that need to be considered. In this work, using the cemented carbides scraps as the raw material, the recycled WC-16%Co (mass fraction) composite powder was synthesized by oxidation, reduction and carbonization reactions. Then the recycled composite powder was sintered to prepare the hard metal bulks by sinter-HIP (hot isostatic pressing). The results indicate that with the carbon addition increases, the content of Co6W6C in the composite powders decreases while the total carbon and free carbon increase. When the carbon addition is 16.60%, the high-performance hard metal bulks can be obtained, with a fracture toughness of 23.05 MPa·m1/2 and a transverse rupture strength of 4020 MPa. Moreover, the Co phase distributes more homogeneously in the recycled hard metals. The larger mean free path of the Co phase and the lower contiguity degree of the WC grains lead to the high performance of the recycled hard metal materials.

Cite this article

Yao WANG , Xuemei LIU , Xiaoyan SONG , Chongbin WEI , Haibin WANG , Xilong WANG . SHORT-TERM PROCESS OF RECYCLING CEMENTED CARBIDE SCRAPS AND PREPARATION OF HIGH PERFORMANCE HARD METALS[J]. Acta Metall Sin, 2014 , 50(5) : 633 -640 . DOI: 10.3724/SP.J.1037.2013.00585

References

[1] Fag Z Z, Wang X, Ryu T, Hwang K S, Sohn H Y. Int J Refract Met Hard Mater, 2009; 27: 288
[2] Wei C B, Song X Y, Fu J, Liu X M, Wang H B, Gao Y, Wang Y. Cryst Eng Comm, 2013; 15: 3305
[3] Liu S, Yi D Q, Li Y X, Zou D. Acta Metall Sin (Engl Lett), 2002; 15: 448
[4] Kim H C, Shon I J, Yooh J K, Doh J M. Int J Refract Met Hard Mater, 2007; 25: 46
[5] Xiong Y H, Lau K, Zhou X Y, Schoenung J M. J Clean Prod, 2008; 16: 1118
[6] Venkateswaran S, Schubert W D, Lux B. Int J Refract Met Hard Mater, 1996; 14: 263
[7] Zhang Q X, Zhang J X. Rare Met Cem Carbides, 1995; (4): 48
[7] (张齐勋, 张家雄. 稀有金属与硬质合金, 1995; (4): 48)
[8] Lee J C, Kim E Y,?Kim J H,?Kim W, Kim B S, Pandey B D. Int J Refract Met Hard Mater, 2011; 29: 365
[9] Hu Y J, Sun P M, Li H G, Chen A L. Rare Met Cem Carbides, 2004; 32(3): 53
[9] (胡宇杰, 孙培梅, 李洪桂, 陈爱良. 稀有金属与硬质合金, 2004; 32(3): 53)
[10] Sun B Q. Rare Met Cem Carbides, 1998; (3):12
[10] (孙宝琦. 稀有金属与硬质合金, 1998; (3): 12)
[11] Liu W B, Song X Y, Zhang J X, Zhang G Z, Liu X M. Int J Refract Met Hard Mater, 2009; 27: 115
[12] Zhang W B, Sha C S, Du Y, Wen G H, Xie W, Wang S Q. Acta Metall Sin, 2011; 47: 1307
[12] (张伟彬, 沙春生, 杜 勇, 温光华, 谢 文, 王社权. 金属学报, 2011; 47: 1307)
[13] Cao Z M, Song X Y, Qiao Z Y. Rare Met, 2008; 32: 216
[13] (曹战民, 宋晓艳, 乔芝郁. 稀有金属, 2008; 32: 216)
[14] Wei C B, Song X Y, Fu J, Lv X S, Wang H B, Gao Y, Zhao S X, Liu X M. J Mater Sci Technol, 2012; 28: 837
[15] Zhao S X, Song X Y, Liu X M, Wei C B, Wang H B, Gao Y. Acta Metall Sin, 2011; 47: 1188
[15] (赵世贤, 宋晓艳, 刘雪梅, 魏崇斌, 王海滨, 高 杨. 金属学报, 2011; 47: 1188)
[16] Joost R, Pirso J, Viljus M, Letunovits S, Juhani K. Est J Eng, 2012; 18: 127
[17] Liu W B, Song X Y, Zhang J X, Zhang G Z, Liu X M. Mater Chem Phy, 2008; 109: 235
[18] Konyashin I, Hlawatschek S, Ries B, Lachmann F, Dorn F, Sologubenko A, Weirich T. Int J Refract Met Hard Mater, 2009; 27: 234
[19] Christensen M, Wahnstr?m G. Phys Rev, 2003; 67B: 115415
[20] Jia K, Fischer T E, Gallois B. Nanostruct Mater, 1998; 10: 875
[21] Fang Z Z. Int J Refract Met Hard Mater, 2005; 23: 119
[22] Fang Z Z, Lockwood G, Griffo A. Metall Mater Trans, 1999; 30A: 3231
[23] Wang X, Hwang K S, Koopman M, Fang Z Z, Zhang L H. Int J Refract Met Hard Mater, 2013; 36: 46
[24] Song S H, Li J C. Acta Metall Sin, 1987; 23: 521
[24] (宋士泓, 李健纯. 金属学报, 1987; 23: 521)
[25] Liu M L, Huang X Y, Duan S T, Shao D Q, Cui Y M, Yao Z M. Acta Metall Sin, 1982; 18: 689
[25] (刘曼朗, 黄孝瑛, 段石田, 邵大琴, 崔玉梅, 姚振梅. 金属学报, 1982; 18: 689)
Outlines

/

〈 〉