PARTIALLY TRANSIENT LIQUID PHASE-DIFFUSION BONDING ON Ti(C, N)-Al2O3 CERAMIC MATRIX COMPOSITES USING Zr/Cu/Zr AS INTERLAYER
Received date: 2013-11-28
Revised date: 2014-02-25
Online published: 2014-05-20
Supported by
Supported by National Natural Science Foundation of China (No.51175239), Jiangsu Provincial Research Foundation for Basic Research (No.BK2011494) and College Natural Science Foundation of Jiangsu Province (No.11KJA430005)
The partially transient liquid phase-diffusion bonding (PTLP-DB) on Ti(C, N)-Al2O3 ceramic matrix composites (CMC) was studied using the Zr foil/Cu foil/Zr foil sanwich as an interlayer. Effect of holding time during PTLP-DB on the element diffusion and reacted products at the interface was analyzed and the affected factors on the joint strength during PTLP-DB were explored. The effect of auxiliary pulse current during PTLP-DB between CMC on element diffusion at the interface and joint strength and its mechanism were also studied. The results showed that the optimum holding times were 15~30 min during PTLP-DB on CMC at 950 ℃. With a shorter holding time, the joint strength decreased due to the existance of unreacted Zr elements at the interface, while with a longer holding time, the joint strength decreased due to the overgrowth of CuZr intermetallics at the interface. With the auxiliary pulse current during PTLP-DB, the residual stress at the interface was greatly decreased, which inhibited the propagation of crack into the base materials. While, the auxiliary pulse current can promote the reaction between Cu and Zr and the formation of Zr-Cu intermetallics at the interface, which produced a weaked interface in the joints.
Key words: Ti(C; N)-Al2O3; PTLP-DB; element diffusion; joint strength; auxiliary pulse current
Mingfang WU , Hongjin KUANG , Fengjiang WANG , Hongxiang LIN , Guoxiang XU . PARTIALLY TRANSIENT LIQUID PHASE-DIFFUSION BONDING ON Ti(C, N)-Al2O3 CERAMIC MATRIX COMPOSITES USING Zr/Cu/Zr AS INTERLAYER[J]. Acta Metall Sin, 2014 , 50(5) : 619 -625 . DOI: 10.3724/SP.J.1037.2013.00777
| [1] | Ettmayera P, Kolaska H, Lengauer W, Dreyer K. Int J Refract Met Hard Mater, 1995; 13: 343 |
| [2] | Pan H Q, Liu Y J, Zhang D X, Itoh I. Mater Mech Eng, 2012; 36(3): 11 |
| [2] | (潘厚宏, 刘拥军, 张大向, 伊藤勲. 机械工程材料, 2012; 36(3): 11) |
| [3] | Wu M F, Zhou X L, Ma C, Yang P. Trans China Weld Inst, 2006; 27(12): 65 |
| [3] | (吴铭方, 周小丽, 马 骋, 杨 沛. 焊接学报, 2006; 27(12): 65) |
| [4] | Zhang L, Lu X, He X B, Qu X H. Rare Met Mater Eng, 2012; 41: 450 |
| [4] | (章 林, 路 新, 何新波, 曲选辉. 稀有金属材料与工程, 2012; 41: 450) |
| [5] | Song X G, Cao J, Wang Y F, Feng J C. Rare Met Mater Eng, 2012; 41: 1247 |
| [5] | (宋晓国, 曹 健, 王义峰, 冯吉才. 稀有金属材料与工程, 2012; 41: 1247) |
| [6] | Chen Z, Cao M S, Zhao Q Z. Mater Sci Eng, 2004; A380: 394 |
| [7] | Passerone A, Muolo M L. Mater Manuf Process, 2000; 15: 631 |
| [8] | Wang J, Li Y J, Ma H J, Liu P. Trans China Weld Inst, 2006; 27(9): 9 |
| [8] | (王 娟, 李亚江, 马海军, 刘 鹏. 焊接学报, 2006; 27(9): 9) |
| [9] | Li S J, Liang X B, Duan H P. Key Eng Mater, 2002; 217: 101 |
| [10] | Osendi M I, Pablos A, Miranzo P. Mater Sci Eng, 2001; A308: 53 |
| [11] | Atabaki M M, Idris J. J Manuf Sci Eng, 2012; 134: 015001 |
| [12] | Cook III G O, Sorensen C D. J Mater Sci, 2011; 46: 5305 |
| [13] | Zhou S, Li X, Xiong W, Zhou Y. J Wuhan Univ Tech-Mater Sci Ed, 2009; 24: 432 |
| [14] | Liu S, Olsen D L, Martin G P. Weld J, 1991; 70: 207 |
| [15] | Zhou Y, Gale W F, North T H. Int Mater Rev, 1995; 40: 181 |
| [16] | Zhang J X, Chandel R S, Chen Y Z, Seow H P. J Mater Process Technol, 2002; 122: 220 |
| [17] | Shen X Q, Li Y J, Puchko U A. Trans China Weld Inst, 2008; 29(12): 41 |
| [17] | (沈孝芹, 李亚江, Puchko U A. 焊接学报, 2008; 29(12): 41) |
| [18] | Zhou F, Li Z Z. Trans Nonferrous Met Soc China, 2001; 11: 273 |
| [18] | (周 飞, 李志章. 中国有色金属学报, 2001; 11: 273) |
| [19] | Kliauga A M, Travessa D, Ferrante M. Mater Charact, 2001; 46: 65 |
| [20] | Yin X H, Li M S, Zhou Y C. J Eur Ceramic Soc, 2007; 27: 3539 |
| [21] | Turchanin M A, Agraval P G, Abdulov A R. Powder Metall Met Ceram, 2008; 47: 78 |
| [22] | Harvey J P, Gheribi A E, Chartrand P. J Chem Phys, 2011; 135: 084502 |
| [23] | Yamaguchi K, Song Y C, Yoshida T, Itagaki K. J Alloys Compd, 2008; 452: 73 |
| [24] | Long Y, Li Y Y, Li X Q. Trans Nonferrous Met Soc China, 2006; 16: 2016 |
| [24] | (龙 雁, 李元元, 李小强. 中国有色金属学报, 2006; 11: 2016) |
| [25] | Yang X, Xi Z P, Liu Y, Tang H P. Rare Met Mater Eng, 2012; 41: 1065 |
| [25] | (杨 鑫, 奚正平, 刘 咏, 汤慧萍. 稀有金属材料与工程, 2012; 41: 1065) |
/
| 〈 |
|
〉 |