SOLIDIFICATION BEHAVIOR AND GRAIN SIZE OF SAND CASTING Mg-6Al-xZn ALLOYS

  • Danhui HOU ,
  • Songmao LIANG ,
  • Rongshi CHEN ,
  • Chuang DONG
Expand
  • 1 Institute of Material Science and Engineering, Dalian University of Techonlogy, Dalian 116024
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    3 Institute of Metallurgy, Clausthal University of Technology, Clausthal-Zellerfeld, Germany, 38678
null

侯丹辉, 男, 1982年生, 博士生

Received date: 2013-09-05

  Revised date: 2013-09-05

  Online published: 2014-05-20

Supported by

National Basic Research Program of China (No.2013CB632202) and National Natural Science Foundation of China ( Nos.51105350 and 51301173)

Abstract

The solidification behavior and microstructure evolution of sand cast Mg-6Al-xZn alloy (named as AZ6x alloys, x=0, 2, 4, 6, mass fraction, %) were characterized by two-thermocouple thermal analysis technology and SEM. The grain sizes of the alloys were quantitatively determined by EBSD technology. Thermodynamic calculations were applied in Pandat software for phase diagram calculation, Scheil model solidification simulation and growth restriction factor values (GRF or values). The results show that solidification of AZ6x alloys follows non-equilibrium solidification paths. Besides the γ-Mg17Al12 phase, which is the only secondary phase in AZ60 alloy, another Φ-Mg21(Al, Zn)17 phase appears in the as-cast microstructure of AZ62 to AZ66 alloys. With the increase of the Zn content, the amount of γ-Mg17Al12 phase decreases and while increase the amount of Φ-Mg21(Al, Zn)17 phase. Calculated equilibrium phase diagram shows that in the AZ60~AZ64 alloys both γ-Mg17Al12 phase and Φ-Mg21(Al, Zn)17 phase can be dissolved into α-Mg under proper heat treatment conditions. However, Φ-Mg21(Al, Zn)17 phase in AZ66 alloy can not be completely dissolved into a-Mg for any temperature. The results also indicate that higher Zn content alloys have higher values and smaller grain size, and lower solid fraction at dendrite coherency point (?sDCP). The relationship of values, grain size and ?sDCP has been also discussed.

Cite this article

Danhui HOU , Songmao LIANG , Rongshi CHEN , Chuang DONG . SOLIDIFICATION BEHAVIOR AND GRAIN SIZE OF SAND CASTING Mg-6Al-xZn ALLOYS[J]. Acta Metall Sin, 2014 , 50(5) : 601 -609 . DOI: 10.3724/SP.J.1037.2013.00558

References

[1] Luo A A. J Magnesium Alloys, 2013; 1: 2
[2] Ma Y Q, Chen R S, Han E H. Mater Lett, 2007; 61: 2527
[3] Maxwell I, Hellawell A. Acta Metall, 1975; 23: 229
[4] Greer A L, Bunn A M, Tronche A, Evans P V, Bristow D J. Acta Mater, 2000; 48: 2823
[5] St John D H, Qian M, Easton M A, Cao P, Hildebrand Z. Metall Mater Trans, 2005; 36A: 1669
[6] Schmid-Fetzer R, Kozlov A. Acta Mater, 2011; 59: 6133
[7] Veldman N L M, Dahle A K, St John D H, Arnberg L. Metall Mater Trans, 2001; 32A: 147
[8] Liang S M, Chen R S, Blandin J J, Suery M, Han E H. Mater Sci Eng, 2008; A480: 365
[9] Arnberg L, Chai G, Backerud L. Mater Sci Eng, 1993; A173: 101
[10] Dahle A K, Arnberg L. Mater Sci Eng, 1997; A225: 38
[11] Chai G, B?ckerud L, R?lland T, Arnberg L. Metall Mater Trans, 1995; 26A: 965
[12] Malekan M, Shabestari S G. Metall Mater Trans, 2009; 40A: 3196
[13] Liang S M. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009
[13] (梁松茂. 中国科学院金属研究所博士学位论文, 沈阳, 2009)
[14] B?ckerud L, Krol E, Tamminen J. Solidification Characteristics of Aluminium Alloys. Vol.1, Oslo: Skan Aluminium, 1986: 65
[15] Chang H W, Qiu D, Taylor J A, Easton M A, Zhang M X. J Magnesium Alloys, 2013; 1: 115
[16] Kierkus W T, Solokowski J H. AFS Trans, 1999; 107: 161
[17] Cao W, Chen S L, Zhang F, Wu K, Yang Y, Chang Y A, Schmid-Fetzer R, Oates W A. Calphad, 2009; 33: 328
[18] Liang P, Tarfa T, Robinson J A, Wagner S, Ochin P, Harmelin M G, Seifert H J, Lukas H L, Aldinger F. Thermochim Acta, 1998; 314: 87
[19] Ohno M, Schmid-Fetzer R. Z Metallkd, 2005; 96: 857
[20] Ohno M, Mirkovi? D, Schmid-Fetzer R. Mater Sci Eng, 2006; A421: 328
[21] Ohno M, Schmid-Fetzer R. Int J Mater Res, 2006; 97: 526
[22] Ohno M, Mirkovi? D, Schmid-Fetzer R. Acta Mater, 2006; 54: 3883
[23] Thorvaldsen A, Aliravci C A. In: Proc International Symposium, Montreal, Canada: Metallurgical of CIM, 1992: 277
[24] Tamura Y, Yagi J, Haitani T, Motegi T, Kono N, Tamehiro H, Saito H. Mater Trans, 2003; 44: 552
[25] Liang S M, Ma Y Q, Chen R S, Han E H. Mater Trans, 2008; 49: 986
Outlines

/

〈 〉