STUDY OF ROLLING-REMELTING SIMA PROCESS FOR PREPARING THE SEMI-SOLID BILLET OF ZCuSn10 ALLOY

  • Jia WANG ,
  • Han XIAO ,
  • Longbiao WU ,
  • Dehong LU ,
  • Rongfeng ZHOU ,
  • Rong ZHOU
Expand
  • 1 Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093
    2 College of Mechanical Engineering, Sichuan University of Science and Engineering, Zigong 643000
    3 Research Center for Analysis and Measurement, Kunming University of Science and Technology, Kunming 650093

Received date: 2013-10-16

  Revised date: 2014-01-24

  Online published: 2014-05-20

Supported by

Applied Basic Research Key Project of Yunnan Province (No.2011FA007),Specialized Research Fund for Doctoral Program of Higher Education (No.20125314120013), Scientific Research Fund of Yunnan Provincial Education Department (No.2012Y543) and Development Research Fund from Sichuan University of Science and Engineering (No.2013PY05)

Abstract

Semi-solid billet of ZCuSn10 alloy is prepared by strain induced melt activation (SIMA) method which included the rolling and remelting process. Firstly, ZCuSn10 alloy is cast, and samples are cut from ingot casting. Secondly, the samples are rolled with 2~4 passes after holding at 450 ℃ for 15 min, then the new samples are cut from deformed alloy. Lastly, the new samples are reheated up to 850 ℃ or 875 ℃ for 15 min, then water quenching. Semi-solid microstructure is observed and compared with microstructure of ZCuSn10 alloy directly reheated after casting. The distribution of Sn element in microstructure under different conditions is measured by using EDS function of SEM, and the microstructure changes during the SIMA process are observed by means of OM and TEM. Based on the experiments, the microstructure evolution is synthetically analyzed and explained during the course of semi-solid billet of ZCuSn10 alloy prepared by SIMA method. The results indicate that semi-solid microstructure of ZCuSn10 alloy by rolling- remelting SIMA process is equal-fine grain, and spheroidization of solid particle is well. The optimum semi-solid microstructure is obtained when alloy deformed 19.7% is remelted at 875 ℃ for 15 min, the average grain diameter is 75.8 μm, shape factor is 1.62, and volume fraction of liquid phase is 17.28%. Deformation process plays a crucial role in grain refinement and spheroidization during SIMA process for preparing the semi-solid billet of ZCuSn10 alloy, as deformation and remelting temperature increases, the size and shape of solid phase in semi solid microstructure are smaller and more round, volume fraction of liquid phase increases. The main mechanism of SIMA process preparing semi-solid billet of ZCuSn10 alloy is that predeformation breaks dendrites and stores energy of deformation into dendrites, and promotes dendrites melting through remelting process. Meanwhile, liquid phase occupies sharp corners of solid particles by Sn element diffusing from liquid phase into α solid phase, so that fine, uniform and roundness α solid particles are gained.

Cite this article

Jia WANG , Han XIAO , Longbiao WU , Dehong LU , Rongfeng ZHOU , Rong ZHOU . STUDY OF ROLLING-REMELTING SIMA PROCESS FOR PREPARING THE SEMI-SOLID BILLET OF ZCuSn10 ALLOY[J]. Acta Metall Sin, 2014 , 50(5) : 567 -574 . DOI: 10.3724/SP.J.1037.2013.00654

References

[1] Spencer D B, Mehrabia R, Flemings M C. Metall Trans, 1972; 3: 1925
[2] Flemings M C. Metall Trans, 1991; 22A: 957
[3] Chen Q, Luo S J, Zhao Z D. J Alloys Compd, 2009; 447: 726
[4] Kiuchi M, Kopp R. CIRP Ann-Manuf Technol, 2002; 51: 653
[5] Kirkwood D H. Int Mater Rev, 1994; 39: 173
[6] Zhao J W, Wu S S, Wan L, Chen Q H, An P. Acta Metall Sin, 2009; 45: 314
[6] (赵君文, 吴树森, 万 里, 陈启华, 安 萍. 金属学报, 2009; 45: 314)
[7] Luo S J, Chen Q, Zhao Z D. Mater Sci Eng, 2009; A501: 146
[8] Liu Z, Mao W M, Zhao Z D. Acta Metall Sin, 2009; 45: 507
[8] (刘 政, 毛卫民, 赵振铎. 金属学报, 2009; 45: 507)
[9] Young K P, Kyonka C P, Courtois J A. US Pat, 4415374, 1983
[10] Lin H Q, Wang J G, Wang H Y, Jiang Q C. J Alloys Compd, 2007; 431: 141
[11] Dong J, Cui J Z, Le Q C, Lu G M. Mater Sci Eng, 2003; A345: 234
[12] Hassas-Irani S B, Zarei-Hanzaki A, Bazaz B, Roostaei A A. Mater Des, 2013; 46: 579
[13] Alipour M, Aghdam B G, Rahnoma H E, Emamy M. Mater Des, 2013; 46: 766
[14] Jiang J F, Wang Y, Qu J J. Mater Sci Eng, 2013; A560: 473
[15] Dodangeh A, Kazeminezhad M, Aashuri H. Mater Sci Eng, 2012; A558: 371
[16] Tao J Q, Cheng Y S, Huang S D, Peng F F, Yang W X, Lu M Q, Zhang Z M, Jin X. Trans Nonferrous Metall, 2012; 22(suppl 2): 428
[17] Chen Q, Zhao Z D, Zhao Z X, Hu C K, Shu D Y. J Alloys Compd, 2011; 509: 7303
[18] Tian R Z,Wang Z T. Handbook of Copper Alloy and its Processing. Changsha: Central South University Press, 2002: 259
[18] (田荣璋,王祝堂. 铜合金及其加工手册. 长沙: 中南大学出版社, 2002: 259)
[19] Metallographic Experiment Group of Central Laboratory of Luoyang Copper Processing Factory. Metallographic Atlas of Copper and Copper Alloy. Beijing: Metallurgical Industry Press, 1983: 74
[19] (洛阳铜加工厂中心试验室金相组. 铜及铜合金金相图谱. 北京: 冶金工业出版社, 1983: 74)
Outlines

/

〈 〉