EFFECT OF HEAT TREATMENT BEFORE WELDING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED SiCp/Al-Cu-Mg COMPOSITE JOINTS

  • Dong WANG ,
  • Quanzhao WANG ,
  • Bol XIAO ,
  • Dingrui NI ,
  • Zongyi MA
Expand
  • 1 School of Chemistry and Materials Science, University of Science and Technology of China, Hefei 230026
    2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-11-11

  Revised date: 2014-01-07

  Online published: 2014-04-20

Supported by

Supported by National Basic Research Program of China (No.2012CB619600)

Abstract

Discontinuously reinforced aluminum matrix composites (AMCs) have been widely applied in structures of aerospace industry. Wide industrial applications of AMCs depend on effective joining methods, which are dependent on the use of a specific material and process. As a new solid-state welding technique, friction stir welding (FSW) has been attempted for joining the AMCs in last few years. However, few attentions have been paid to the effect of initial heat treatment tempers of the AMCs on the FSW joints. In this work, 6 mm thick SiCp/2009Al composite plates in both soft (solution temper) and hard (natural aging temper) conditions were successfully friction stir welded at a rotation rate of 800 r/min and a welding speed of 100 mm/min (named as Sol-FSW and T4-FSW samples). In the nugget zone (NZ) of both samples, the grain size and the distribution of the coarse Al2Cu phases were similar. In the heat affected zone, two low hardness zones (LHZs) were observed. LHZ I adjacent to the NZ had the lowest hardness. Both samples had the similar hardness in this zone. For the Sol-FSW sample, LHZ II far away from the NZ had a higher hardness and was closer to the NZ compared to that of the T4-FSW sample. The ultimate tensile strength of both the samples was similar and reached 83% of T4-tempered base metal. Both samples failed in LHZ I adjacent to the NZ due to the lowest hardness in this zone. This indicates that for the SiCp/2009Al composite under solution temper it is possible to produce similar joints to that under natural aging temper using FSW technique. FSW of the composites under soft condition is beneficial to enlarging the welding process window and reducing the tool wear.

Cite this article

Dong WANG , Quanzhao WANG , Bol XIAO , Dingrui NI , Zongyi MA . EFFECT OF HEAT TREATMENT BEFORE WELDING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED SiCp/Al-Cu-Mg COMPOSITE JOINTS[J]. Acta Metall Sin, 2014 , 50(4) : 489 -497 . DOI: 10.3724/SP.J.1037.2013.00719

References

[1] Lloyd D J. Int Mater Rev, 1994; 39: 1
[2] Tjong S C, Ma Z Y. Mater Sci Eng, 2000; R29: 49
[3] Xu S J, Xiao B L, Liu Z Y, Wang W G, Ma Z Y. Acta Metall Sin, 2012; 48: 882
[3] (许世娇, 肖伯律, 刘振宇, 王文广, 马宗义. 金属学报, 2012; 48: 882)
[4] Zhang Q, Wang Q Z, Xiao B L, Ma Z Y. Acta Metall Sin, 2012; 48: 135
[4] (张 琪, 王全兆, 肖伯律, 马宗义. 金属学报, 2012; 48: 135)
[5] Ellis M B D. Int Mater Rev, 1996; 41: 41
[6] Ni D R, Chen D L, Xiao B L, Wang D, Ma Z Y. Mater Des, 2013; 55: 64
[7] Wang D, Xiao B L, Wang Q Z, Ma Z Y. J Mater Sci Technol, 2014; 30: 54
[8] Srivatsan T S, Meslet A H, Petraroli M, Hotton B, Lam P C. Mater Sci Eng, 2002; A325: 202
[9] Shindo D J, Rivera A R, Murr L E. J Mater Sci, 2002; 37: 4999
[10] Liu H J, Fenga J C, Fujiib H, Nogi K. Int J Mach Tool Manuf, 2005; 45: 1635
[11] Prado R A, Murr L E, Shindo D J, Sota K F. Scr Mater, 2001; 45: 75
[12] Wang D, Wang Q Z, Xiao B L, Ma Z Y. Mater Sci Eng, 2014; A589: 271
[13] Marzoli L M, Strombeck A V, Dos Santos J F, Gambaro C, Volpone L M. Compos Sci Technol, 2006; 66: 363
[14] Wang D, Xiao B L, Wang Q Z, Ma Z Y. Mater Des, 2007; 28: 1440
[15] Feng A H, Xiao B L, Ma Z Y. Compos Sci Technol, 2008; 68: 2141
[16] Genevois C, Deschamps A, Denquin A, Cottignies B D. Acta Mater, 2005; 538: 2447
[17] McNelley T R, Swaminathan S, Su J Q. Scr Mater, 2008; 58: 349
[18] Inem B. Mater Sci Eng, 1995; A197: 91
[19] Charit I, Mishra R S. Scr Mater, 2008; 58: 367
[20] Jariyaboon M, Davenport A J, Ambat R, Connolly B J, Williams S W, Price D A. Corros Sci, 2007; 49: 877
[21] Mahoney M W, Rhodes C G, Flintoff J G, Spurling R A, Bingel W H. Metall Mater Trans, 1998; 29A: 1955
[22] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
[23] Wang S C, Starink M J. Int Mater Rev, 2005; 50: 193
[24] Rodrigo P, Poza P, Utrilla V, Urena A. J Alloys Compd, 2009; 479: 451
[25] Marceau R K W, Sha G, Lumley R N, Ringer S P. Acta Mater, 2010; 58: 1795
[26] Liu F C, Ma Z Y. Metall Mater Trans, 2005; 36A: 2378
[27] Zhang Z. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012
[27] (张 振. 中国科学院金属研究所博士学位论文, 沈阳, 2012)
[28] Jones M J, Heurtier P, Desrayaud C, Montheillet F, Allehaux D, Driver J H. Scr Mater, 2005; 52: 693
[29] Homma T, Moody M P, Saxey D W, Ringer S P. Metall Mater Trans, 2012; 43A: 2192
Outlines

/

〈 〉