MICROSTRUCTURE AND MECHANICAL PROPERTY OF LASER WELDED JOINT FOR HYPOEUTECTOID U-Nb ALLOY

  • Yubin LI ,
  • Wei WANG ,
  • Jianjun HE ,
  • Zhiqiang ZHANG ,
  • Tongyan ZHANG
Expand
  • China Academy of Engineering physics, Mianyang 621900
null

李玉斌, 男, 1972年生, 博士

Received date: 2013-08-15

  Revised date: 2013-11-24

  Online published: 2014-03-20

Supported by

Supported by Development Fund of China Academy of Engineering Physics (No.2011B0301055)

Abstract

The microstructures and mechanical properties of hypoeutectoid U-Nb alloy laser welded joint were investigated by optical microscopy (OM), X-ray diffractometer (XRD), transmission electron microscopy (TEM), split hopkinson pressure bar (SHPB) and other analysis apparatus. The results show that the microstructure of hypoeutectoid U-Nb alloy base metal is α-U+γ-U lamellar pearlite under isothermal heat treatment, while the laser welding seam is composed of α' lath martensite for pre-heated or α' twin martensite for no pre-heated with orthogonal crystal structure. The quasi-static tensile strength of welded joint (about 400 MPa) is much less than base metal and microstructures of weld, for the main reason of incomplete penetration weld and low fracture toughness. Between dynamic impact loading for base and welded joint, the strain rate of welded joint is lower than base metal, and the yield strength of welded joint is higher. Also, the compressive stress-strain curves indicated that the flow stresses for welded joint increased with the increase of strain rate and the obvious effect of strain rate hardening has been observed. At strain rate of 2000 s-1, selected plastic deformation taking place in welded joint is due to the tremendous difference mechanic properties between weld seam and base metal, and the adiabatic shear band(ASB) only appears in the rest of welded joint.

Cite this article

Yubin LI , Wei WANG , Jianjun HE , Zhiqiang ZHANG , Tongyan ZHANG . MICROSTRUCTURE AND MECHANICAL PROPERTY OF LASER WELDED JOINT FOR HYPOEUTECTOID U-Nb ALLOY[J]. Acta Metall Sin, 2014 , 50(3) : 379 -386 . DOI: 10.3724/SP.J.1037.2013.00493

References

[1] Wilkinson W D. Uranium Metal. Volume II, New York: Interscience Publisher, 1962: 13
[2] Koike J, Kassner M E, Tate R E. J Phase Equil, 1998; 19: 253
[3] Burke J J, Colling D A, Gorum A E. Physical Metallurgy of Uranium Alloys. New York: Brook Hill Publishing Company, 1976: 22
[4] Wood D H, Dini J W. J Nucl Mater, 1983; 114: 199
[5] Chancellor W, Wolfenden A. J Nucl Mater, 1990; 171: 389
[6] Turner P W, Lundin C D. Weld J, 1970; 49: 579
[7] Tatarivo V R, krasnorutskii V S, Rubashko V G. At Energy J, 1977; 43: 122
[8] Sunwoo A. Scr Mater, 1997; 37: 691
[9] Wood D H, Mara G L. Weld J, 1977; 56: 88
[10] Elmer J W, Teruya A T, Errill P E. Lawrence Livermore National Laboratory Report. LM, US: Lawrence Livermore National Lab, UCRL-ID-141043, 2000
[11] Elmer J W, Teruya A T, Errill P E. Lawrence Livermore National Laboratory Report. LM, US: Lawrence Livermore National Lab, UCRL-JC-144232, 2001
[12] Gleen L, James L. Lawrence Livermore National Laboratory Report. LM, US: Lawrence Livermore National Lab, UCRL-87469, 1982
[13] Scott T B, Petherbridge J R, Findlay I, Glascott J, Allen G C. J Alloys Compd, 2009; 475: 766
[14] Petherbridge J R, Scott T B, Glascott J, Allen G C, Findlay I. J Alloys Compd, 2009; 476: 543
[15] Field R D, McCabe R J, Alexander D J, Teter D F. J Nucl Mater, 2009; 392: 105
[16] Smerd R, Winkler S, Salisbury C, Worswick M, Lloyd D, Finn M. Int J Impact Eng, 2005; 32: 541
[17] Ishikawa K, Watanabe H, Mukai T. Mater Lett, 2005; 59: 1511
[18] Gong X, Fan J L, Huang B Y, Tian J M. Mater Sci Eng, 2010; A527: 7565
[19] Dong D Y, Liu Y, Wang L, Su L G. Acta Metall Sin, 2013; 49: 159
[19] (董丹阳, 刘 杨, 王 磊, 苏亮进. 金属学报, 2013; 49: 159)
[20] Gourdin W H, Lassila D H. Acta Metall Mater, 1991; 39: 2337
[21] Chen Z Y, Cai H N, Wang F C, Tan C W, Zhan C K, Liu C M. Acta Metall Sin, 2009; 45: 143
[21] (陈志永, 才鸿年, 王富耻, 谭成文, 詹从堃, 刘楚明. 金属学报, 2009; 45: 143)
[22] Gong S L, Zhang J X, Pei Y, Yu Q. J Xi'an Jiaotong Univ, 2000; 34: 81
[22] (巩水利, 张建勋, 裴 怡, 于 琴. 西安交通大学学报, 2000; 34: 81)
[23] Xu Z J, Li Y L, Liu M S, Li P Z, Wu Y G. Acta Metall Sin, 2008; 44: 98
[23] (许泽建, 李玉龙, 刘明爽, 李朋洲, 吴云刚. 金属学报, 2008; 44: 98)
[24] Zhang J, Tan C W, Ren Y, Wang F C, Cai H N. Trans Nonferrous Met Soc China, 2011; 21: 39
[25] Cui Z Q,Qin Y C. Metallography and Heat Treatment. 2nd Ed., Beijing: China Machine Press, 2004: 266
[25] (崔忠圻,覃耀春. 金属学与热处理. 北京: 机械工业出版社, 2004: 266)
[26] Kollie T G, Anderson R C, Carpenter D A, Smith D D. J Nucl Mater, 1984; 120: 160
Outlines

/

〈 〉