EFFECTS OF WELDING THERMAL CYCLE AND AGING TREATMENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTY OF A Ni-Fe BASE SUPERALLOY

  • Dong WU ,
  • Xin WANG ,
  • Wenchao DONG ,
  • Shanping LU
Expand
  • 1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2 China Academy of Engineering Physics, Mianyang 621900

Received date: 2013-06-26

  Revised date: 2013-06-26

  Online published: 2014-03-20

Supported by

Supported by High Technology Research and Development Program of China (No.2012AA03A501)

Abstract

Increasing the steam temperature and pressure of boilers in super-ultracritical power plant is an important approach to increase the plant efficiency. The steam temperature of the most efficient coal power plant is now around 620 ℃, representing an increase of about 80 ℃ in the past 40 years, which owes to the high temperature properties improvement of boiler components, such as the superheater and the reheater. Nickel base superalloy, for example Inconel 740 and Inconel 617, is being developed by some countries for the material requirement of 700 ℃ super-ultracritical power plants. Meanwhile, weldability investigation is necessary for the developing materials since welding plays a key role on the construction of coal power plant boilers. In this work, the weldability of a kind of Ni-Fe base superalloy, one of the candidate materials for the high temperature components of 700 ℃ ultra-supercritical coal plant is studied. By welding thermal simulator (Gleeble 1500) experiments, the variation and evolution of mechanical properties and microstructure were analyzed for this Ni-Fe base superalloy, under welding thermal cycle treatment condition and aging treatment condition after welding thermal cycle. After the welding thermal cycle with a peak temperature of 1249 ℃, both the yield strength and tensile strength for solutioned Ni-Fe base superalloy at 25 and 700 ℃ were decreased, along with the increasing of ductility. After aging treatment to the Ni-Fe base superalloy experienced a welding thermal cycle, the yield strength and tensile strength at 25 ℃ were similar with those of the aged base metal. At 700 ℃, the strength of the heat affected zone (HAZ) after aging treatment is higher than that of the aged Ni-Fe base superalloy. Microstructure analysis showed that the γ' phase and MC carbide in Ni-Fe base superalloy dissolved during the high temperature welding thermal simulation experimental process. The solution of carbides in the grain boundaries caused a loss of a pinning effect on the migration of grain boundary and a decreasing of the strength. After the aging treatment to the Ni-Fe base superalloy experienced a high temperature welding thermal cycle, γ' and M23C6 carbide were precipitated. The precipitation of M23C6 at the grain boundaries during aging treatment was mainly due to the supply of the carbon from the MC which had been dissolved partially during former welding thermal cycle.

Cite this article

Dong WU , Xin WANG , Wenchao DONG , Shanping LU . EFFECTS OF WELDING THERMAL CYCLE AND AGING TREATMENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTY OF A Ni-Fe BASE SUPERALLOY[J]. Acta Metall Sin, 2014 , 50(3) : 313 -322 . DOI: 10.3724/SP.J.1037.2013.00355

References

[1] Zhang H J, Zhou R C, Hou S F, Guo Y. Proc CSEE, 2011; 31: 108
[1] (张红军, 周荣灿, 侯淑芳, 郭 岩. 中国电机工程学报, 2011; 31: 108)
[2] Bugge J, Kaer S, Blum R. Energy, 2006; 31: 1437
[3] Wang J, Dong J X, Zhang M C, Xie X S. World Iron Steel, 2011; 11(2): 26
[3] (王 珏, 董建新, 张麦仓, 谢锡善. 世界钢铁, 2011; 11(2): 26)
[4] Hu P. Electric Power Construction, 2005; 26(6): 26
[4] (胡 平. 电力建设, 2005; 26(6): 26)
[5] Guo Y, Zhou R C, Hou S F, Zhang H J. Proc CSEE, 2010; 30: 86
[5] (郭 岩, 周荣灿, 侯淑芳, 张红军. 中国电机工程学报, 2010; 30: 86)
[6] Zhao S Q, Xie X S, Smith G D, Patel S J. Mater Des, 2006; 27: 1120
[7] Cowen C J, Danielson P E, Jablonski P D. J Mater Eng Perform, 2011; 20: 1078
[8] Evans N D, Maziasz P J, Swindeman R W, Smith G D. Scr Mater, 2004; 51: 503
[9] Park Y S, Ham H S, Cho S M, Bae D H. In: Guagliano M, Vergani L eds., Proc 11th Int Conf on the Mechanical Behavior of Materials (ICM11), Amsterdam: Elsevier Science BV, 2011: 2645
[10] Mankins W L, Hosier J C, Bassford T H. Metall Mater Trans, 1974; 5B: 2579
[11] Guo J T, Du X K. Acta Metall Sin, 2006; 41: 1221
[11] (郭建亭, 杜秀魁. 金属学报, 2006; 41: 1221)
[12] Masuyama F. ISIJ Int, 2001; 41: 612
[13] Viswanathan R, Bakker W. J Mater Eng Perform, 2001; 10: 81
[14] Shi X. Electr Weld Mach, 2010; 40(2): 4
[14] (史 轩. 电焊机, 2010; 40(2): 4)
[15] Zhong W L,Wang W,Liang Y C,Lin J D,Lin Q R,Liu H W,Yu Y R. High Temperature Steam Oxidation of Supercritical Plant Metal. Beijing: China Electric Power Press, 2010: 30
[15] (钟万里,王 伟,梁永纯,林介东,林清如,刘洪文,虞月荣. 超临界机组金属高温蒸汽氧化. 北京: 中国电力出版社, 2010: 30)
[16] Ramirez J E. Weld J, 2012; 91: 122
[17] Mo W L, Lu S P, Li D Z, Li Y Y. J Mater Sci Technol, 2013; 29: 458
[18] Mo W L, Lu S P, Li D Z, Li Y Y. Mater Sci Eng, 2013; A582: 326
[19] Xu S, Dickson J I, Koul A K. Metall Mater Trans, 1998; 29A: 2687
[20] Shulga A V. J Alloys Compd, 2007; 436: 155
[21] Li Y Q,Liu J Y. Interstitial Phase of Superalloy. Beijing: Metallurgical Industry Press, 1990: 276
[21] (李玉清,刘锦岩. 高温合金间隙相. 北京: 冶金工业出版社, 1990: 276)
[22] Richards N L, Chaturvedi M C. Int Mater Rev, 2000; 45: 109
[23] Hu R, Bai G H, Li J S, Zhang J Q, Zhang T B, Fu H Z. Mater Sci Eng, 2012; A548: 83
[24] Jena A K, Chaturvedi M C. J Mater Sci, 1984; 19: 3121
[25] Garosshen T J, Mccarthy G P. Metall Trans, 1985; 16A: 1213
Outlines

/

〈 〉