ACTIVE/PASSIVE BEHAVIOR OF LOW CARBON STEEL IN DEAERATED BICARBONATE SOLUTION
Received date: 2013-08-18
Revised date: 2013-12-05
Online published: 2014-03-20
Supported by
Supported by National Natural Science Foundation of China (No.51071160)
As a kind of clean, efficient and relatively safe energy, nuclear energy has been widely used around the world. The high-level radioactive waste (HLRW) generated in the nuclear has also become a major risk, so the disposal safety of HLRW will be especially important. The planned concept of China's HLRW disposal program is a shaft-tunnel model located in saturated zones in granite. The metal container for sealing the HLRW is the key because its interaction with the ground water will lead to the leak of the HLRW during the long repository time. Beishan is a selected repository area and the ground water contains a bicarbonate (
Huailiang WEN , Junhua DONG , Wei KE , Wenjuan CHEN , Jingfeng YANG , Nan CHEN . ACTIVE/PASSIVE BEHAVIOR OF LOW CARBON STEEL IN DEAERATED BICARBONATE SOLUTION[J]. Acta Metall Sin, 2014 , 50(3) : 275 -284 . DOI: 10.3724/SP.J.1037.2013.00497
| [1] | Wang J, Su R, Chen W M, Guo Y H, Jin Y X, Wen Z J, Liu Y M. Chin J Rock Mech Eng, 2006; 25: 649 |
| [1] | (王 驹, 苏 锐, 陈伟明, 郭永海, 金远新, 温志坚, 刘月妙. 岩石力学与工程学报, 2006; 25: 649) |
| [2] | Gordon G M. Corrosion, 2002; 58: 811 |
| [3] | King F, Padovani C. Corros Eng Sci Technol, 2011; 46: 82 |
| [4] | Saheb M, Neff D, Dillmann P, Matthiesen H, Foy E. J Nucl Mater, 2008; 379: 118 |
| [5] | Yang J F, Dong J H, Ke W. Acta Metall Sin, 2011; 47: 1321 |
| [5] | (阳靖峰, 董俊华, 柯 伟. 金属学报, 2011; 47: 1321) |
| [6] | Taniguchi N, Honda A, Ishikawa H. MRS Symp Process, 1998; 506: 495 |
| [7] | Thomas J G N, Nurse T J, Walker R. Br Corros J, 1970; 5(2): 87 |
| [8] | Armstrong R D, Coates A C. J Electroanal Chem, 1974; 50: 303 |
| [9] | Castro E B, Valentine C R, Monia C A, Vilche J R, Arvia A J. Corros Sci, 1986; 26: 781 |
| [10] | Castro E B, Vilche J R, Arvia A J. Corros Sci, 1991; 32: 37 |
| [11] | Rozenfeld J L. Atmospheric Corrosion of Metals. Houston: NACE, 1972: 1 |
| [12] | Féron D, Crusset D, Gras J M. J Nucl Mater, 2008; 379: 16 |
| [13] | Videm K, Dugstad A. Mater Perform, 1989; 28(4): 46 |
| [14] | Davies D H, Burstein G T. Corrosion, 1980; 36: 416 |
| [15] | Valentini C R, Moina C A, Vilche J R, Arvia A J. Corros Sci, 1985; 25: 985 |
| [16] | Wersin P, Spahin K, Bruno J. SKB Technical Report (9402). Stockholm: Swedish Nuclear Fuel and Waste Management Co., 1994: 1 |
| [17] | Smart N R, Blackwood D J, Werme L. Corrosion, 2002; 58: 547 |
| [18] | Smart N R, Blackwood D J, Werme L. Corrosion, 2002; 58: 627 |
| [19] | Reardon E J. Environ Sci Technol, 1995; 29: 2936 |
| [20] | Dong J H, Nishimura T, Kodama T. MRS Symp Process, 2002; 713: 105 |
| [21] | Nishimura T, Dong J H. J Power Energy System, 2009; 3: 23 |
| [22] | Azoulay I, Rémazeilles C, Refait P. Corros Sci, 2012; 58: 229 |
| [23] | Marsh G P, Taylor K J, Bland I D, Westcott C, Tasker P W, Sharland S M. MRS Symp Process, 1985; 50: 421 |
| [24] | Hao L, Zhang S X, Dong J H, Ke W. Corros Sci, 2012; 59: 270 |
| [25] | Cox B, Wong Y M. J Nucl Mater, 1995; 218: 324 |
| [26] | Orazem M E, Tribollet B. Electrochemical Impedance Spectroscopy. New York: John Wiley & Sons, 2008: 246 |
| [27] | Cao C N,Zhang J Q. Introduction of Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 88 |
| [27] | (曹楚南,张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 88) |
| [28] | Almeida E, Morcillo M, Rosales B M, Marrocos M. Mater Corros, 2000; 51: 859 |
| [29] | Yamashita M, Miyuki H, Nagaro H, Misawa T. Corros Sci, 1994; 36: 283 |
/
| 〈 |
|
〉 |