ANALYSIS ON GRAIN BOUNDARY EFFECTS OF COLUMNAR GRAINED ELECTRICAL STEEL

  • Yuanyuan SHAO ,
  • Ping YANG ,
  • Weimin MAO
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2013-07-29

  Revised date: 2013-12-01

  Online published: 2014-03-20

Supported by

Supported by National Natural Science Foundation of China (No.51071024)

Abstract

Columnar grains show their special characteristics of morphological and crystallographic anisotropies, and thus markedly influence the microstructure and texture evolution during rolling and annealing process in electrical steel. The rolling and annealing microstructure and texture of three columnar grained samples with the long axes arranged along different directions were investigated by means of XRD and EBSD techniques, and the effects of columnar grain boundaries were analyzed from the view point of geometry-induced interaction and orientation-induced interaction. The results indicated that, prominent microstructure and texture gradients caused by the surface shearing during hot rolling inherited to subsequent cold rolling and annealing in columnar grained samples. The difference in morphological anisotropy of initial columnar grain boundaries in the three samples were eliminated after hot rolling, while a same type structure of anisotropic grain boundaries was formed. However, the crystallographic anisotropies of the samples were changed before cold rolling, and it caused that the evolution of the microstructure and texture during subsequent cold rolling and annealing was different with directly cold rolling process in previous work. This feature produced a graded microstructure and texture relationship between hot rolled samples and finally annealed samples. In this work, it mainly focused on the {100}-oriented regions at grain boundaries, because the {100} texture was most beneficial to the magnetic property of electrical steel.

Cite this article

Yuanyuan SHAO , Ping YANG , Weimin MAO . ANALYSIS ON GRAIN BOUNDARY EFFECTS OF COLUMNAR GRAINED ELECTRICAL STEEL[J]. Acta Metall Sin, 2014 , 50(3) : 259 -268 . DOI: 10.3724/SP.J.1037.2013.00459

References

[1] Shin H J, An J K, Park S H, Lee D N. Acta Meter, 2003; 51: 4693
[2] Gao Z Y, Zhang Z Y, Li Y D, Li W Q. Angang Technol, 2010; (3): 40
[2] (高振宇, 张智义, 李亚东, 李文权. 鞍钢技术, 2010; (3): 40)
[3] Huh M Y, Engler O. Mater Sci Eng, 2001; A308: 74
[4] Huh M Y, Lee J H, Park S H, Engler O, Raabe D. Steel Res Int, 2005; 76: 797
[5] Littmann M F. Metall Trans, 1975; 6A: 1041
[6] Liu H T, Liu Z Y, Cao G M, Li C G, Wang G D. J Magn Mang Mater, 2011; 323: 2648
[7] Cheng L, Yang P, Fang Y P, Mao W M. J Magn Magn Mater, 2012; 324: 4068
[8] Ding L, Shao Y Y, Yang P, Mao W M. In: Chen Z ed, Proceeding 12nd Electrical Steel Academic Annual Conference of China, Wuhan: Wuhan Publishing House, 2012: 124
[8] (丁 磊,邵媛媛,杨 平,毛卫民. 陈 卓主编, 第十二届电工钢学术年会论文集, 武汉: 武汉出版社, 2012: 124)
[9] Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 782
[9] (张 宁, 杨 平, 毛卫民. 金属学报. 2012; 48: 782)
[10] Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 307
[10] (张 宁, 杨 平, 毛卫民. 金属学报. 2012; 48: 307)
[11] Yang P, Shao Y Y, Zhang N, Cheng L, Mao W M. Mater Sci Forum, 2013; 753: 173
[12] Shimizu Y, Ito Y, Iida Y. Metall Trans, 1986; 17A: 1323
[13] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1992; 32: 1319
[14] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1993; 33: 783
[15] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1994; 34: 1008
[16] Liu H T, Liu Z Y, Cao G M, Li C G, Wang G D. Mater Charact, 2011; 62: 463
[17] Zhang N, Yang P, Mao W M. Mater Lett, 2013; 93: 363
[18] Wagner P. PhD Dissertation, Rheinisch-Westfaelische Technische Hochschule Aachen, 1994
[19] Shao Y Y, Yang P, Fu Y J, Mao W M. J Iron Steel Res Int, 2013; 20: 99
[20] D?rmann C. PhD Dissertation, Rheinisch-Westfaelische Technische Hochschule Aachen, 1983
Outlines

/

〈 〉