MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR PROCESSED ULTRAFINE-GRAINED AND NANOSTRUCTURED Cu-Al ALLOYS

  • Peng XUE ,
  • Bolü XIAO ,
  • Zongyi MA
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-10-18

  Revised date: 2013-10-18

  Online published: 2014-02-20

Supported by

Supported by National Natural Science Foundation of China (Nos.51071150, 51301178 and 51331008)

Abstract

Ultrafine-grained (UFG) and nanostructured (NS) materials have attracted considerable interest due to their special microstructure and mechanical properties. Severe plastic deformation is one of the optimum approaches to fabricate bulk, dense and contamination-free UFG and NS metallic materials. However, high density of dislocations and unstable microstructure were usually induced in these UFG and NS metallic materials, resulting in poor tensile plasticity and fatigue properties. In this study, bulk UFG and NS Cu-Al alloys were successfully prepared via friction stir processing (FSP) with additional forced water cooling. FSP Cu-Al alloys exhibited uniform recrystallized microstructure with equiaxed ultrafine grains, and the grain sizes reduced gradually as the stacking fault energy (SFE) decreased. Abundant nano-twin layers formed in the ultrafine grains of FSP Cu-Al alloys with low SFEs, which further refined the ultrafine grains and NS microstructure was achieved. The strength of the FSP Cu-Al alloys increased clearly with decreasing the SFEs due to the gradually refined microstructure, but the uniform elongation increased initially and then decreased in the Cu-Al alloy with the lowest SFE.

Cite this article

Peng XUE , Bolü XIAO , Zongyi MA . MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR PROCESSED ULTRAFINE-GRAINED AND NANOSTRUCTURED Cu-Al ALLOYS[J]. Acta Metall Sin, 2014 , 50(2) : 245 -251 . DOI: 10.3724/SP.J.1037.2013.00661

References

[1] Valiev R. Nat Mater, 2004; 3: 511
[2] Zhu Y T, Liao X Z. Nat Mater, 2004; 3: 351
[3] Tao N R, Lu K. J Mater Sci Technol, 2007; 23: 771
[4] Mughrabi H, H?ppel H W. Int J Fatigue, 2010; 32: 1413
[5] Goto M, Han S Z, Euh K, Kang J H, Kim S S. Acta Mater, 2010; 58: 6249
[6] An X H. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, 2012
[6] (安祥海. 中国科学院金属研究所博士学位论文, 沈阳, 2012)
[7] Mishra R S, Mahoney M W, McFadden S X, Mara N A, Mukherjee A K. Scr Mater, 1999; 42: 163
[8] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
[9] Ma Z Y. Metall Mater Trans, 2008; 39A: 642
[10] Xue P, Xiao B L, Ma Z Y. Mater Sci Eng, 2012; A532: 106
[11] Su J Q, Nelson T W, Sterling C J. Scr Mater, 2005; 52: 135
[12] Xue P, Xiao B L, Ma Z Y. Scr Mater, 2013; 68: 751
[13] Chang C I, Du X H, Huang J C. Scr Mater, 2007; 57: 209
[14] Xue P, Xiao B L, Wang W G, Zhang Q, Wang D, Wang Q Z, Ma Z Y. Mater Sci Eng, 2013; A575: 30
[15] Xue P, Xiao B L, Ma Z Y. J Mater Sci Technol, 2013; 29: 1111
[16] An X H, Lin Q Y, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2011; 64: 954
[17] Qu S, An X H, Yang H J, Huang C X, Yang G, Zang Q S, Wang Z G, Wu S D, Zhang Z F. Acta Mater, 2009; 57: 1586
[18] Zhang P, An X H, Zhang Z J, Wu S D, Li S X, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2012; 67: 871
[19] Murr L E. Interfacial Phenomena in Metals and Alloys. Massachusetts: Addison-Wesley Publishing Company, 1975: 142
[20] Zhang Y, Tao N R, Lu K. Acta Mater, 2011; 59: 6048
[21] Torre F D, Lapovok R, Sandlin J, Thomson P F, Davies C H J, Pereloma E V. Acta Mater, 2004; 52: 4819
[22] Meyers M A,Chawla K K. Mechanical Behavior of Materials. 2nd Ed., Cambridge: Cambridge University Press, 2009: 337
[23] McNelley T R, Swaminathan S, Su J Q. Scr Mater, 2008; 58: 349
[24] Jata K V, Semiatin S L. Scr Mater, 2000; 43: 743
[25] Su J Q, Nelson T W, Sterling C J. J Mater Res, 2003; 18: 1757
[26] Feng A H, Ma Z Y. Acta Mater, 2009; 57: 4248
[27] An X H, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2012; 66: 227
Outlines

/

〈 〉