INFLUNECE OF STACKING FAULT ENERGY ON THE MICROSTRUCTURES, TENSILE AND FATIGUE PROPERTIES OF NANOSTRUCTURED Cu-Al ALLOYS

  • Xianghai AN ,
  • Shiding WU ,
  • Zhefeng ZHANG
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-09-18

  Revised date: 2013-09-18

  Online published: 2014-02-20

Supported by

Supported by National Natural Science Foundation of China (Nos.50890173, 50931005, 51101162 and 51331007)

Abstract

Influences of stacking fault energy (SFE) on the microstructures, tensile properties and fatigue behaviors of nanostructured (NS) Cu-Al alloys prepared by severe plastic deformation (SPD) were systematically summerized. With the reduction of SFE, it is found that the dominant formation mechanism of nanostructures gradually transformed from the dislocation subdivision to the twin fragmentation and the grain sizes also decrease; while microstructural homogeneity is achieved more readily in the materials with either high or low SFE than in the materials with medium SFE. The strength of NS Cu-Al significantly increases with decreasing the SFE, while there is an optimal SFE for the ductility of these materials. More significantly, the strength-ductility synergy of Cu-Al alloys is prominently enhanced with reducing the SFE. Finally, simultaneous improvements of low-cycle fatigue and high-cycle fatigue properties of NS Cu-Al alloys were achieved with decreasing the SFE. This can be attributed to the enhanced microstructure stability and the reduced strain localization in shear bands. With the reduction of SFE, the fatigue damage micro-mechanism was also transformed from grain boundary (GB) migration to other GB activities such as, atom shuffling, GB sliding and GB rotation.

Cite this article

Xianghai AN , Shiding WU , Zhefeng ZHANG . INFLUNECE OF STACKING FAULT ENERGY ON THE MICROSTRUCTURES, TENSILE AND FATIGUE PROPERTIES OF NANOSTRUCTURED Cu-Al ALLOYS[J]. Acta Metall Sin, 2014 , 50(2) : 191 -201 . DOI: 10.3724/SP.J.1037.2013.00591

References

[1] Gleiter H. Prog Mater Sci, 1989; 33: 223
[2] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[3] Valiev R Z, Langdon T G.Prog Mater Sci, 2006; 51: 881
[4] Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
[5] Iwahashi Y, Horita Z, Nemoto M, Langdon T G. Acta Mater, 1997; 45: 4733
[6] Iwahashi Y, Horita Z, Nemoto M, Langdon T G. Acta Mater, 1998; 46: 3317
[7] Tao N R, Lu K. Scr Mater, 2009; 60: 1039
[8] Mughrabi H, H?ppel H W, Kautz M. Scr Mater, 2004; 51: 807
[9] Zhu Y T, Liao X Z. Nat Mater, 2004; 3: 351.
[10] Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427
[11] Considère A. Annales Ponts Chaussées, 1885; 9: 574
[12] Mughrabi H, H?ppel H W. Int J Fatigue, 2010; 32: 1413
[13] H?ppel H W, Zhou Z M, Mughrabi H, Valiev R Z. Philos Mag, 2002; 82A: 1781
[14] Wong M K, Kao W P, Lui J T, Chang C P, Kao P W. Acta Mater, 2007; 55: 715
[15] Malekjani S, Hodgson P D, Cizek P, Hilditch T B. Acta Mater, 2011; 59: 5358
[16] Lu K, Lu L, Suresh S. Science, 2009; 324: 349
[17] Estrin Y, Vinogradov A. Acta Mater, 2013; 61: 782
[18] Torre F D, Lapovok R, Sandlin J, Thomson P F, Davies C H J, Pereloma E V. Acta Mater, 2004; 52: 4819
[19] Qu S, An X H, Yang H J, Huang C X, Yang G, Zang Q S, Wang Z G, Wu S D, Zhang Z F. Acta Mater, 2009; 57: 1586
[20] An X H, Wu S D, Zhang Z F. Mater Sci Forum, 2011; 667-669: 379
[21] Wu S D, An X H, Han W Z, Qu S, Zhang Z F. Acta Metall Sin, 2010; 46: 257
[21] (吴士丁, 安祥海, 韩卫忠, 屈 伸, 张哲峰. 金属学报, 2010; 46: 257)
[22] Balogh L, Ungár T, Zhao Y H, Zhu Y T, Horita Z, Xu C, Langdon T G. Acta Mater, 2008; 56: 809
[23] An X H, Lin Q Y, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2011; 64: 249
[24] Mohamed F A. Acta Mater, 2003; 51: 4107
[25] Komura S, Horita Z, Nemoto M, Langdon T G. J Mater Res, 1999; 14: 4044
[26] An X H, Lin Q Y, Wu S D, Zhang Z F. Mater Sci Eng, 2010; A527: 4510
[27] An X H, Lin Q Y, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Philos Mag, 2011; 91: 3307
[28] An X H, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2010; 63: 560
[29] Han W Z, Zhang Z F, Wu S D, Li S X. Philos Mag, 2008; 88: 3011
[30] Zhang Y, Tao N R, Lu K. Scr Mater, 2009; 60: 211
[31] Hong C S, Tao N R, Huang X, Lu K. Acta Mater, 2010; 58: 3103
[32] An X H, Lin Q Y, Qu S, Yang G, Wu S D, Zhang Z F. J Mater Res, 2009: 24: 3636
[33] An X H, Han W Z, Huang C X, Zhang P, Yang G, Wu S D, Zhang Z F. Appl Phys Lett, 2008; 92: 201915
[34] An X H, Lin Q Y, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2011; 64: 954
[35] Zhang Y, Tao N R, Lu K. Acta Mater, 2011; 59: 6048
[36] Zhao Y H, Zhu Y T, Liao X Z, Horita Z, Langdon T G. Appl PhysLett, 2006; 89: 121906
[37] Zhang P, An X H, Zhang Z J, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2012; 67: 871
[38] Zhao Y H, Guo Y Z, Wei Q, Dangelewicz A M, Xu C, Zhu Y T, Langdon T G, Zhou Y Z, Lavernia E J. Scr Mater, 2008; 59: 627
[39] Wang Y M, Chen M, Zhou F, Ma E. Nature, 2002; 419: 912
[40] An X H, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2012; 66: 227
[41] An X H, Qu S, Wu S D, Zhang Z F. J Mater Res, 2011; 26: 407
[42] Lu L, Shen Y, Chen X, Qian L, Lu K. Science, 2004; 304: 422
[43] Lu L, Chen X, Huang X, Lu K.Science, 2009; 323: 607
[44] Shen Y, Lu L, Lu Q H, Jin Z H, Lu K. Scr Mater, 2005; 52: 989
[45] An X H, Wu S D, Zhang Z F. 2013, submitted
[46] Zhang Z F, Wang Z G. Acta Mater, 2003; 51: 347
[47] Zhang Z F, Wang Z G. Prog Mater Sci, 2008; 53: 1025
[48] An X H, Lin Q Y, Wu S D, Zhang Z F. Scr Mater, 2013; 68: 988
[49] Detor A J, Schuh C A. Acta Mater, 2007; 55: 4221
[50] Sch?fer J, Albe K. Scr Mater, 2012; 66: 315
[51] Pan Q S, Lu Q H, Lu L. Acta Mater, 2013; 61: 1383
[52] Schi?tz J. Mater Sci Eng, 2004; A375: 975
[53] Sangid M D, Pataky G J, Sehitoglu H, Rateick R G, Niendorf T, Maier H J. Acta Mater, 2011; 59: 7340
[54] Chowdhury P B, Huseyin Sehitoglu H, Rateick R G, Maier H J. Acta Mater, 2013; 61: 2531
[55] Farkas D, Willemann M, Hyde B. Phys Rev Lett, 2005; 94: 165502
[56] Wu S D, Wang Z G, Jiang C B, Li G Y, Alexandrov I V, Valiev R Z. Scr Mater, 2003; 48: 1605
[57] Zhang Z F, Wu S D, Li Y J, Liu S M, Wang Z G. Mater Sci Eng, 2005; A412: 279
[58] Zhang Z J, An X H, Zhang P, Yang M X, Yang G, Wu S D, Zhang Z F. Scr Mater, 2013; 68: 389
[59] Pang J C, Li S X, Wang Z G, Zhang Z F. Mater Sci Eng, 2013; A564: 331
[60] Lukà? P, Kunz L, Svoboda M. Metall Mater Trans, 2007; 38A: 910
Outlines

/

〈 〉