PLASTIC DEFORMATION MECHANISMS IN NANOTWINNED METALS

  • Lei LU ,
  • Zesheng YOU
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-11-05

  Revised date: 2013-11-05

  Online published: 2014-02-20

Supported by

Supported by National Basic Research Program of China (No.2012CB932202) and National Natural Science Foundation of China (Nos.51071153 and 51371171)

Abstract

A brief overview is provided about the plastic deformation mechanisms in nanotwinned metals. The unique two-dementional nanoscale twin lamellae lead to different dislocation slip systems activated during plastic deformation. It has been revealed that there are three distinctly different dislocation-mediated deformation mechanisms in nanotwinned metals, namely dislocation pile-up against and slip transfer across twin boundaries, Shockley partials gliding on twin boundaries leading to twin boundary migration, and threading dislocations slip confined by neighboring twin boundaries. It is further demonstrated that these three dislocation-mediated mechanisms are switchable upon changing in the loading direction with respect to twin boundaries.

Cite this article

Lei LU , Zesheng YOU . PLASTIC DEFORMATION MECHANISMS IN NANOTWINNED METALS[J]. Acta Metall Sin, 2014 , 50(2) : 129 -136 . DOI: 10.3724/SP.J.1037.2013.00697

References

[1] Lu L, Shen Y F, Chen X H, Qian L H, Lu K. Science, 2004; 304: 422
[2] Lu K, Lu L, Suresh S. Science, 2009; 324: 349
[3] Zhu T, Li J. Prog Mater Sci, 2010; 55: 710
[4] Shen Y F, Lu L, Lu Q H, Jin Z H, Lu K.Scr Mater, 2005; 52: 989
[5] Zhang X, Misra A, Wang H, Nastasi M, Embury J D, Mitchell T E, Hoagland R G, Hirth J P. Appl Phys Lett, 2004; 84: 1096
[6] Zhang X, Misra A, Wang H, Shen T D, Nastasi M, Mitchell T E, Hirth J P, Hoagland R G, Embury J D. Acta Mater, 2004; 52: 995
[7] Lu L, Schwaiger R, Shan Z W, Dao M, Lu K, Suresh S. Acta Mater, 2005; 53: 2169
[8] Chen X H, Lu L. Scr Mater, 2007; 57: 133
[9] Chen X H, Lu L, Lu K. Scr Mater, 2011; 64: 311
[10] Lu L, You Z S, Lu K. Scr Mater, 2012; 66: 837
[11] Shute C J, Myers B D, Xie S, Barbee Jr T W, Hodge A M, Weertman J R. Scr Mater, 2009; 60: 1073
[12] Shute C J, Myers B D, Xie S, Li S Y, Barbee Jr T W, Hodge A M, Weertman J R. Acta Mater, 2011; 59: 4569
[13] Hodge A M, Furnish T A, Shute C J, Liao Y, Huang X, Hong C S, Zhu Y T, Barbee Jr T W, Weertman J R.Scr Mater, 2012; 66: 872
[14] Pan Q S, Lu Q H, Lu L. Acta Mater, 2013; 61: 1383
[15] Singh A, Tang L, Dao M, Lu L, Suresh S. Acta Mater, 2011; 59: 2437
[16] Shen Y F, Lu L, Dao M, Suresh S. Scr Mater, 2006; 55: 319
[17] Lu L, Dao M, Zhu T, Li J. Scr Mater, 2009; 60: 1062
[18] Lu L, Zhu T, Shen Y, Dao M, Lu K, Suresh S. Acta Mater, 2009; 57: 5165
[19] Wu Z X, Zhang Y W, Srolovitz D J.Acta Mater, 2009; 57: 4508
[20] Wu Z X, Zhang Y W, Srolovitz D J. Acta Mater, 2011; 59: 6890
[21] Asaro R J, Kulkarni Y. Scr Mater, 2008; 58: 389
[22] Kulkarni Y, Asaro R J. Acta Mater, 2009; 57: 4835
[23] Dao M, Lu L, Shen Y F, Suresh S.Acta Mater, 2006; 54: 5421
[24] Jerusalem A, Dao M, Suresh S, Radovitzky R. Acta Mater, 2008; 56: 4647
[25] Asaro R J, Suresh S. Acta Mater, 2005; 53: 3369
[26] Zhang X, Wang H, Chen X H, Lu L, Lu K, Hoagland R G, Misra A. Appl Phys Lett, 2006; 88: 173116
[27] Hartley C S, Blachon D L A.J Appl Phys, 1978; 49: 4788
[28] Zhu T, Gao H. Scr Mater, 2012; 66: 843
[29] Hall E O. Proc Phys Soc London, 1951; 64B: 747
[30] Petch N J.J Iron Steel Int, 1953; 174: 25
[31] Jin Z H, Gumbsch P, Ma E, Albe K, Lu K, Hahn H, Gleiter H. Scr Mater, 2006; 54: 1163
[32] Jin Z H, Gumbsch P, Albe K, Ma E, Lu K, Gleiter H, Hahn H. Acta Mater, 2008; 56: 1126
[33] Shabib I, Miller R E. Modell Simul Mater Sci Eng, 2009; 17: 055009
[34] Shabib I, Miller R E. Acta Mater, 2009; 57: 4364
[35] Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607
[36] Li X, Wei Y, Lu L, Lu K, Gao H. Nature, 2010; 464: 877
[37] Merz M D, Dahlgren S D. J Appl Phys, 1975; 46: 3235
[38] Hodge A M, Wang Y M, Barbee Jr T W, Scr Mater, 2008; 59: 163
[39] Anderoglu O, Misra A, Wang J, Hoagland R G, Hirth J P, Zhang X. Int J Plast, 2010; 26: 875
[40] You Z S, Lu L, Lu K. Acta Mater, 2011; 59: 6927
[41] Misra A, Hirth J P, Hoagland R G. Acta Mater, 2005; 53: 4817
[42] Nix W. Metall Mater Trans, 1989; 20A: 2217
[43] Freund L B. J Appl Mech, 1987; 54: 553
[44] Matthews J W, Blakeslee A E. J Cryst Growth, 1975; 29: 273
[45] You Z, Li X, Gui L, Lu Q, Zhu T, Gao H, Lu L.Acta Mater, 2013; 61: 217
[46] Deng C, Sansoz F. Acta Mater, 2009; 57: 6090
[47] Deng C, Sansoz F. Nano Lett, 2009; 9: 1517
[48] Cao A J, Wei Y G, Mao S X. Appl Phys Lett, 2007; 90: 151909
[49] Hu Q, Li L, Ghoniem N M. Acta Mater, 2009; 57: 4866
[50] Li L, Ghoniem N M. Phys Rev, 2009; 79B: 075444
[51] Jang D, Li X, Gao H, Greer J R. Nat Nanotechnol, 2012; 7: 594
[52] Idrissi H, Wang B, Colla M S, Raskin J P, Schryvers D, Pardoen T. Adv Mater, 2011; 23: 2119
[53] Bufford D, Wang H, Zhang X.Acta Mater, 2011; 59: 93
[54] Lu K, Yan F K, Wang H T, Tao N R. Scr Mater, 2012; 66: 878
Outlines

/

〈 〉