Original Articles

LOCALIZED CORROSION OF ALUMINUM ALLOY 2024 EXPOSED TO SALT LAKE ATMOSPHERIC ENVIRONMENT IN WESTERN CHINA

  • Binbin WANG ,
  • Zhenyao WANG ,
  • Gongwang CAO ,
  • Yanjie LIU ,
  • Wei KE
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-07-16

  Revised date: 2013-07-16

  Online published: 2014-01-11

Supported by

Supported by National Natural Science Foundation of China No.51131007 and Foundation Project of National Defense Technology No.H102011B002

Abstract

Localized corrosion behavior of aluminum alloy 2024 with/without cladding exposed to salt lakes atmospheric environment in western china for 4 a was investigated. The depth of pitting, corrosion products, morphology of surface and cross-section, and corrosion potential were analyzed by SEM/EDS, OM, XRD and electrochemical analysis system. The results showed that 2024 suffered severe pitting corrosion. The cladding layer of aluminum alloy 2024 exposed for 2 a had been penetrated. Depth of pitting of aluminum alloy 2024 without cladding after 2 a exposure had reached 320 μm; meanwhile, few pitting that penetrated the whole substrate of aluminum alloy 2024 without cladding had been observed. A main corrosion product of aluminum alloy 2024 with/without cladding—[Mg1-xAlx(OH)2]x+ (Cl-, CO2-)x·mH2O (layered double hydroxides, LDH) was determined. Also, the results of electrochemistry indicated that the corrosion potential of aluminum alloy 2024 decreased gradually with the concentration of Cl- increasing. The effects of factors of salt lake atmospheric environments, corrosion product and Cl- concentration on the corrosion behavior of 2024 with/without cladding were discussed.

Cite this article

Binbin WANG , Zhenyao WANG , Gongwang CAO , Yanjie LIU , Wei KE . LOCALIZED CORROSION OF ALUMINUM ALLOY 2024 EXPOSED TO SALT LAKE ATMOSPHERIC ENVIRONMENT IN WESTERN CHINA[J]. Acta Metall Sin, 2014 , 50(1) : 49 -56 . DOI: 10.3724/SP.J.1037.2013.00417

References

[1] Liu J A,Xie S S. Exploitation and Application of Aluminium Alloy. Beijing: Metallurgical Industry Press, 2011: 71
[1] (刘静安,谢水生. 铝合金材料应用与开发. 北京: 冶金工业出版社, 2011: 71)
[2] Vargel C. Corrosion of Aluminium. Paris: Dunod, 2004: 235
[3] Cao C N. Material Natural Environmental Corrosion of China. Beijing: Chemical Industry Press, 2005: 108
[3] (曹楚南. 中国材料的自然环境腐蚀. 北京: 化学工业出版社, 2005: 108)
[4] Lashermes M, Guilhuaudis A, Reboul M, Trentelivers G. In: Ailor W H ed., Atmospheric Corrosion, New York: John Wiley and Sons, 1982: 353
[5] Dean S W, Anthony W H. In: Dean S W, Lee T ed., Degradation of Metals in Atmosphere STP 965, Philadelphia: American Society of Testing and Materials, 1988: 191
[6] Sun S Q, Zheng Q F, Li D F, Wen J G.Corros Sci, 2009; 51: 719
[7] Sun S Q, Zheng Q F, Li D F, Hu S Q, Wen J G.Corros Sci, 2011; 53: 2527
[8] Cheng Y L, Zhang Z, Cao F H, Li J F, Zhang J Q, Wang J M, Cao C N. Corros Sci, 2004; 46: 1649
[9] Shi Y Y, Zhang Z, Su J X, Cao F H, Zhang J Q.Electrochim Acta, 2006; 51: 4977
[10] Wang Z Y, Ma T, Han W, Yu G C. Chin JNonferrous Met, 2007; 17: 326
[11] Zhang Z, Song S Z, Mo S F.Acta Metall Sin, 2004; 40: 754
[11] (张 正, 宋诗哲, 墨淑芬. 金属学报, 2004; 40: 754)
[12] Chang H, Han E H, Wang J Q, Ke W.Acta Metall Sin, 2005; 41: 556
[12] (常 红, 韩恩厚, 王俭秋, 柯 伟. 金属学报, 2005; 41: 556)
[13] Sheng H, Dong C F, Xiao K, Li X G.Acta Metall Sin, 2012; 48: 414
[13] (生 海, 董超芳, 肖 葵, 李晓刚. 金属学报, 2012; 48: 414)
[14] An B G, Zhang X Y, Song S Z, Li H X, Han E H. J Chin Soc Corros Prot, 2003; 23: 167
[14] (安百刚, 张学元, 宋诗哲, 李洪锡, 韩恩厚. 中国腐蚀与防护学报, 2003; 23: 167)
[15] Zhang X Y, Sun Z H, Liu M H, Tang Z H, Li B.J Chin Soc Corros Prot, 2007; 27: 354
[15] (张晓云, 孙志华, 刘明辉, 汤智慧, 李 斌. 中国腐蚀与防护学报, 2007; 27: 354)
[16] Sun S Q, Zhao Y B, Zheng Q F, Li D F. J Chin Soc Corros Prot, 2012; 32: 195
[16] (孙霜青, 赵予兵, 郑弃非, 李德富. 中国腐蚀与防护学报, 2012; 32: 195)
[17] Blanc C, Lavelle B, Mankowski G.Corros Sci, 1997; 39: 495
[18] Buchheit R G, Grant R P, Hlava P F, Mckenzie B, Zender G L. J Electrochem Soc, 1997; 144: 2621
[19] Guillaumin V, Mankowski G.Corros Sci, 1999; 41: 421
[20] Obispo H M, Murr L E, Arrowood R M, Trillo E A.J Mater Sci, 2000; 35: 3479
[21] Zheng X Y,Zhang M G,Xu C,Li B X. Saline Mark of China. Beijing: Science Technology Press, 2002: 1
[21] (郑喜玉,张明刚,徐 昶,李秉孝. 中国盐湖志. 北京: 科学技术出版社, 2002: 1)
[22] Wang Z Q. Pickled Soil of China. Xi'an: Shanxi Renmin Press, 1994: 251
[22] (王遵亲. 中国盐渍土. 西安: 陕西人民出版社, 1994: 251)
[23] Xiao Y D, Wang G Y, Li X G, Lin A, Zhang S P, Qin X Z, Wang Z Y.J Chin Soc Corros Prot, 2003; 23: 248
[23] (萧以德, 王光雍, 李晓刚, 林 安, 张三平, 秦晓洲, 王振尧. 中国腐蚀与防护学报, 2003: 23: 248)
[24] Zheng Q F, Sun S Q, Wen J G, Li D F.Chin J Nonferrous Met, 2009; 19: 353.
[24] (郑弃非, 孙霜青, 温军国, 李德富. 中国有色金属学报, 2009; 19: 353)
[25] Blücher D B, Svensson J E, Johansson L G.Corros Sci, 2006; 48: 1848
[26] Zheng Q F, Sun S Q, Wen G J, Li D F. J Chin Soc Corros Prot, 2010; 30: 72
[26] (郑弃非, 孙霜青, 温军国, 李德富. 中国腐蚀与防护学报, 2010; 30: 72)
[27] Wang B B, Wang Z Y, Han W, Ke W. Corros Sci, 2012; 59: 63
[28] Gou G J, Ma P H, Chu M X.Acta Phys Chim Sin, 2004; 20: 1357
[29] Wang B B, Wang Z Y, Han W, Wang C, Ke W. Chin J Nonferrous Met, 2013; 23: 1199
[30] Buchheit R G, Martinez M A, Montes L P.J Electrochem Soc, 2000; 147: 119.
[31] Cole I S, Azmat N S, Kanta A, Venkatraman M.Int Mater Rev, 2009; 54: 117
[32] Wexler A S, Seinfeld J H. Atmos Environ,?1991; 25A: 2731
[33] Ge Z Z, Wexler A S, Johnston M V. J Colloid Interf Sci,?1996; 183: 68
[34] Ge Z Z, Wexler A S, Johnston M V. J Phys Chem,?1998; 102: 173
[35] Kelly J T, Wexler A S, Chan C K, Chan M N.Atmos Environ, 2008; 42: 3717
[36] Kelly J T, Wexler A S.Atmos Environ, 2006; 40: 4450
[37] Prosek T, Lversen A, Taxén C, Thierry D.Corrosion, 2009; 65: 105
[38] Xiao H S, Dong J L, Wang L Y, Zhao L J, Wang F, Zhang Y H.Environ Sci Technol, 2008; 42: 8698
[39] Wise M E, Biskos G, Martin S T, Russell L M, Buseck P R.Aerosol Sci Technol, 2005; 39: 884
[40] Paredes S P, Valenzuela M A, Fetter G, Flores S O. J Phys ChemSolids, 2011; 72: 914
Outlines

/

〈 〉