Original Articles

MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg-4Zn-2Al-2Sn ALLOYS EXTRUDED AT LOW TEMPERATURES

  • Dongqing ZHAO ,
  • Jixue ZHOU ,
  • Yunteng LIU ,
  • Xuguang DONG ,
  • Jing WANG ,
  • Yuansheng YANG
Expand
  • 1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2 Institute of New Materials Research, Shandong Academy of Sciences, Jinan 250014

Received date: 2013-06-25

  Revised date: 2013-06-25

  Online published: 2014-01-11

Supported by

Supported by National Key Technology R&D Program (No.2011BAE22B01-1), International Science & Technology Cooperation Program of China (No.2011DFA50903) and Natural Science Foundation of Shandong Province (No.ZR2010EQ021)

Abstract

Due to the high demand of light-weight alloys in automotive applications, wrought magnesium (Mg) alloys, applied as automotive sheet and extrusions, are attracting great attention. However, some inherent disadvantages of common wrought Mg alloys have limited their application, such as poor corrosion resistance, poor creep resistance and low formability. It is well known that Sn can provide thermally stable Mg2Sn particles in the matrix of magnesium alloys. Our previous study shows that the Mg-4Zn-2Al-2Sn alloy has potential to be developed into a wrought Mg alloy. Currently, the microstructure, texture and mechanical properties of Mg-4Zn-2Al-2Sn alloy extruded at temperatures of 225, 250 and 275 ℃ have been investigated, where complete dynamic recrystallization occurred during extrusion and the average grain size was reduced to 4.4, 7.1 and 10.5 μm, respectively. The amount and morphology of the second phases were directly influenced by the extrusion temperature. Extruded at 225 ℃, irregular Mg2Sn phase in size of 20~60 nm precipitated in the grains. With the extrusion temperature increasing to 275 ℃, Mg2Sn of about 500 nm and micron-size Mg32(Al, Zn)49 precipitates were observed. The {0002} texture was formed at 225 and 250 ℃ during the extrusion. While the temperature increased to 275 ℃, due to the activation of prismatic slip system, { 1 0 1 - 0 } < 0002 > texture of prismatic plane parallel to extrusion direction was also observed. When compressive stress loaded along the extrusion direction, the { 1 0 1 - 0 } < 0002 > texture suppressed the activation of the tensile twinning { 1 0 1 - 2 } < 1 0 1 - 1 > , which leads to a decrease of asymmetry between tension and compression.

Cite this article

Dongqing ZHAO , Jixue ZHOU , Yunteng LIU , Xuguang DONG , Jing WANG , Yuansheng YANG . MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg-4Zn-2Al-2Sn ALLOYS EXTRUDED AT LOW TEMPERATURES[J]. Acta Metall Sin, 2014 , 50(1) : 41 -48 . DOI: 10.3724/SP.J.1037.2013.00352

References

[1] Kashefi N, Mahmudi R.Mater Des, 2012; 39: 200
[2] Song D H, Lee S W, Park Y D, Park Y H, Cho K M, Park I M. Mater Sci Forum, 2007; 539-543: 1790
[3] Chen Z H,Yan H G,Chen J H,Quan Y J,Wang H M,Chen D. Magnesium Alloys. Beijing: Chemical Industry Press, 2004: 202
[3] (陈振华,严红革,陈吉华,全亚杰,王慧敏,陈 鼎. 镁合金. 北京: 化学工业出版社, 2004: 202)
[4] Sasaki T T, Yamamoto K, Honma T, Kamado S, Hono K. Scr Mater, 2008; 59: 1111
[5] Liu C M,Zhu X R,Zhou H T. Magnesium Alloy Phase Diagrams. Nanjing: Southeast University Press, 2006: 49
[5] (刘楚明,朱秀荣,周海涛. 镁合金相图集. 南京: 东南大学出版社, 2006: 49)
[6] Bronfin B, Aghion E, Buch F V, Schumann S, Katzir M. US Pat,7041179B2, 2006
[7] Dong X G, Fu J W, Yang Y S. Acta Metall Sin, 2013; 49: 621
[7] (董旭光, 付俊伟, 杨院生. 金属学报, 2013; 49: 621)
[8] Lim H K, Kim D H, Lee J Y, Kim W T, Kim D H.J Alloys Compd, 2009; 468: 308
[9] Chen J H, Chen Z H, Yan H G, Zhang F Q, Kun L.J Alloys Compd, 2008; 461: 209
[10] Zhao D Q, Dong X G, Zhang X E, Gao A J, Zhou J X, Yang Y S. Mater Sci Forum, 2013; 747-748: 398
[11] Kang D H, Park S S, Kim N J. Mater Sci Eng, 2005; A413-414: 555
[12] Henes S, Gerold V. ZMetallk, 1962; 53: 743
[13] Rabkin E.Scr Mater, 1998; 39: 1631
[14] Li W B, Easterling K E.Acta Metall Mater, 1990; 38: 1045
[15] Mendis C L, Ohishi K, Kawamura Y, Honma T, Kamado S, Hono K.Acta Mater, 2009; 57: 749
[16] Park S S, You B S, Yoon D J.J Mater Process Technol, 2009; 209: 5940
[17] Shahzad M, Wagner L.Mater Sci Eng, 2009; A506: 141
[18] Yang P, Hu Y S, Cui F E. ChinJ Mater Res, 2004; 18: 52
[18] (杨 平, 胡轶嵩, 崔凤娥. 材料研究学报, 2004; 18: 52)
[19] Park S S, Tang W N, You B S. Mater Lett, 2010; 64: 31
[20] Wang Y N, Huang J C.Acta Mater, 2007; 55: 897
[21] Barnett M R.Scr Mater, 2008; 59: 696
[22] Stanford N, Barnett M R.Mater Sci Eng, 2009; A516: 226
[23] Jain J, Poole W J, Sinclair C W, Gharghouri M A.Scr Mater, 2010; 62: 301
Outlines

/

〈 〉