MICROSTRUCTURES AND PROPERTIES OF 0Cr32Ni7Mo4N DUPLEX STAINLESS STEEL AFTER VARIOUS FORMING PROCESSES

  • Hong HE ,
  • Jingyuan LI ,
  • Liyan QIN ,
  • Yide WANG ,
  • Fei FANG
Expand
  • 1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2 Taiyuan Iron & Steel (Group) Co. Ltd., Taiyuan 030002

Received date: 2013-07-10

  Revised date: 2013-07-10

  Online published: 2014-01-11

Supported by

Supported by National Natural Science Foundation of China (No.51174026), National Science and Technology Supported Program of the 12th Five-year Plan (No.2012BAE04B02)

Abstract

Duplex stainless steels consist of a two phase microstructure involving α-ferrite and γ-austenite. These alloys have a remarkable combination of mechanical properties together with good corrosion resistance under critical working conditions and are suitable for marine and petro-chemical applications. However, the poor hot workability of these materials makes the industrial processing of flat products particularly critical. Many investigations focus on the mechanisms and behaviors of hot deformation on these materials. Several factors are frequently reported give rise to hot cracking: phase proportions, size and morphology of both phases, softening mechanisms in constituting phases, microstructural evolution during hot work, and strain partitioning between α and γ. On the contrary, few studies have been carried on cold rolling performance. Hot cracking should be avoid during forming process of duplex stainless steel, the more effective way of manufacturing in such materials is also needs research. In this work, the formability of 0Cr32Ni7Mo4N duplex stainless steel was studied in the hot rolling and directly cold rolling processes. The deformation mechanism of α and γ phase at room temperature, the microstructure evolution after hot rolling, cold rolling and solution treatment were investigated. Mechanical properties and corrosion resistance of two kinds of cold-rolled sheets were tested. The metallography and corrosion morphology were observed by OM and SEM. The results show that cracks emerged along the edge of hot-rolled plate even it was reheated three times, and it has good cold rolling formability after cutting edge of the plate. On the other hand the as-cast billet solution-treated at 1100 ℃ has good cold rolling performance. Deformation mechanism of α phase at room temperature is that multi-slip system form dislocation cell structure, while single slip model and mechanical twins appear in γ phase. As the temperature of heat-treatment raised, microstructure became more homogeneous and the amount of precipitate particles decreased. The experimental results show that the tensile strength of cold-rolled sheet after heat-treatment reaches 1082.9 MPa and the elongation is 29.3%. Critical pitting potential of the specimen in 3.5%NaCl liquor is 1060 mV; weight loss after intergranular corrosion in 65%HNO3 solution is 0.05 g/(m2·h).

Cite this article

Hong HE , Jingyuan LI , Liyan QIN , Yide WANG , Fei FANG . MICROSTRUCTURES AND PROPERTIES OF 0Cr32Ni7Mo4N DUPLEX STAINLESS STEEL AFTER VARIOUS FORMING PROCESSES[J]. Acta Metall Sin, 2014 , 50(1) : 1 -10 . DOI: 10.3724/SP.J.1037.2013.00393

References

[1] Sato Y S, Nelson T W, Sterling C J, Steel R J, Pettersson C O.Mater Sci Eng, 2005; A397: 376
[2] Han Y, Zou D N, Chen Z Y, Fan G W, Zhang W.Mater Charact, 2011; 62: 198
[3] Badji R, Bouabdallah M, Bacroix B, Kahloun C, Belkessa B, Maza H. Mater Charact, 2008; 59: 447
[4] Silva E M, Albuquerque V H C, Leite J P, Varela A C G, Moura E P D, Tavares J M.Mater Sci Eng, 2009; A516: 126
[5] Chai G C, Kivisakk U, Tokaruk J, Eidhagen J.Stainless Steel World, 2009; (03): 27
[6] Pinol-Juez A, Iza-Mendia A, Gutierrez I.Metall Mater Trans, 2000; 31A: 1671
[7] Martin G, Yerra S K, Bréchet Y, Véron M, Mithieux J, Chéhab B, Delannay L, Pardoen T.Acta Mater, 2012; 60: 4646
[8] Fang Y L, Liu Z Y, Song H M, Jiang L Z.Mater Sci Eng, 2009; A526: 128
[9] Jorge A M, Reis G S, Balancin O.Mater Sci Eng, 2011; A528: 2259
[10] Qin Y F, Jiang L Z, Song H M, Zhang W, Hu J C, Jin X J.J Iron Steel Res, 2010; 22(8): 45
[10] (秦焰锋, 江来珠, 宋红梅, 张 伟, 胡锦程, 金学军. 钢铁研究学报, 2010; 22(8): 45)
[11] Marinelli M C, Degallaix S, Alvarez-Armas I.Mater Sci Eng, 2006; A435: 305
[12] Farnoush H, Momeni A, Dehghani K, Mohandesi J A, Keshmiri H. Mater Des, 2010; 31: 220
[13] Fan G W, Liu J, Han P D, Qiao G J.Mater Sci Eng, 2009; A515: 108
[14] Bartali A, Evrard P, Aubin V, Heren U, Alvarez-Armas I, Armas A F, Degallaix-Moreuil S.Proc Eng, 2010; 2: 2229
[15] Wang S T, Yang K, Shan Y Y, Li L F.Acta Metall Sin, 2007; 43: 171
[15] (王松涛, 杨 柯, 单以银, 李来风. 金属学报, 2007; 43: 171)
[16] Nibur K A, Bahr D F.Scr Mater, 2003; 49: 1055
[17] Song R B, Xiang J Y, Hou D P.J Univ Sci Technol Beijing, 2013; 35: 55
[17] (宋仁伯, 项建英, 侯东坡. 北京科技大学学报, 2013; 35: 55)
[18] Xiang H L, Huang W L, Liu D, He F S.Acta Metall Sin, 2010; 46:304
[18] (向红亮, 黄伟林, 刘 东, 何福善. 金属学报, 2010; 46: 304)
[19] Weisbrodt-Reisch A, Brummer M, Hadler B, Wolbank B, Werner E A.Mater Sci Eng, 2006; A416: 1
[20] Zhao Z Y, Xu L, Li G P, Xue R D, Zheng J H.Trans Mater Heat Treat, 2010; 31: 75
[20] (赵志毅, 徐 林, 李国平, 薛润东, 郑建华. 材料热处理学报, 2010; 31: 75)
[21] Moura V S, Lima L D, Pardal J M, Kina A Y, Corte R R A, Tavares S S M.Mater Charact, 2008; 59: 1127
[22] Do Nascimento A M, Ierardi M, Kina A Y, Tavares S. Mater Charact, 2008; 59: 1736
[23] Kim S, Lee I, Kim J, Jang S, Park Y, Kim K, Kim Y.Corros Sci, 2012; 64: 164
[24] Tan H, Jiang Y, Deng B, Sun T, Xu J, Li J. Mater Charact, 2009; 60: 1049
[25] Ortiz N, Curiel F F, López V H, Ruiz A.Corros Sci, 2013; 69: 236
Outlines

/

〈 〉