FIRST-PRINCIPLES CALCULATION OF ELECTRONIC STRUCTURE AND ELASTIC PROPERTY OF AB2 TYPE INTERMETALLICS IN Mg-Zn-Ca ALLOY

  • MAO Pingli ,
  • YU Bo ,
  • LIU Zheng ,
  • WANG Feng ,
  • JU Yang
Expand
  • School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870

Received date: 2013-05-13

  Revised date: 2013-07-22

  Online published: 2013-10-11

Abstract

Electronic structure and elastic properties of Mg2Sn, Mg2Ca and MgZn2 phases were investigated by means of first-principles calculations from CASTEP program based on density functional theory (DFT). The calculated lattice parameters were in good agreement with the experimental and literature values. The calculated heats of formation and cohesive energies show that Mg2Sn has the strongest alloying ability and structural stability. The density of states (DOS) of Mg2Sn, Mg2Ca and MgZn2 phases were calculated to analyze the mechanism of structural stability and mechanical properties. The calculated band structures show that Mg2Sn phase has the widest bandgap. The electron density difference indicate that bonding characteristics of Mg2Sn, Mg2Ca and MgZn2 phases were all covalent bond, ionic bond and metallic bond. The elastic constants of Mg2Sn, Mg2Ca and MgZn2 phases are calculated, the bulk moduli, shear moduli, Young's moduli and Poisson's ratio are then derived. Bulk moduli is assumed to be the ability of material resistance to volume change by applied stress, the larger bulk modulus of MgZn2 phase shows that it has stronger ability to resist deformation. Shear moduli is a measure of resistance to shear strain deformation under the deformation condition of shear stress, the larger shear moduli value of Mg2Sn phase indicates that it has the stronger ability to resist shear strain deformation. The calculated Poisson's ration shows that MgZn2 has the largest value, and then followed by Mg2Ca and Mg2Sn. Hence, the plasticity of MgZn2 phase is the best. The calculated Young's moduli of Mg2Sn phase has the largest value and MgZn2 phase has the smallest value. Hence, among the three phases Mg2Sn phase has the strongest stiffness. The ratio of the shear moduli to bulk moduli of phase can be used to demonstrate the brittle and ductile of materials. The critical value, which separates ductility from brittleness, is about 0.57. A higher G/Bu value is associated withbrittleness, otherwise is ductility. The calculated values of Mg2Sn, Mg2Ca and MgZn2 phases are 0.66, 0.53 and 0.18, respectively. The results show that Mg2Sn is brittle, Mg2Ca and MgZn2 are both ductile.

Cite this article

MAO Pingli , YU Bo , LIU Zheng , WANG Feng , JU Yang . FIRST-PRINCIPLES CALCULATION OF ELECTRONIC STRUCTURE AND ELASTIC PROPERTY OF AB2 TYPE INTERMETALLICS IN Mg-Zn-Ca ALLOY[J]. Acta Metall Sin, 2013 , 49(10) : 1227 -1233 . DOI: 10.3724/SP.J.1037.2013.00266

References

[1] Yang H Y, Guo X W, Wu G H, Wang S H, Ding W J. Surf Coat Technol, 2011; 205: 2907

[2] Liu Z, Zhang K, Zeng X Q. Magnesium-Based Light-Alloy Theoretical Basis and the Application.Beijing: Mechanical Industry Press, 2002: 1
(刘正, 张奎, 曾小勤. 镁基轻质合金理论基础及其应用. 北京: 机械工业出版社, 2002: 1)
[3] Song W, Wu Z G, He Y H, Huang B Y. Chin J Nonferrous Met, 2008; 18: 1971
(宋旼, 吴正刚, 贺跃辉, 黄伯云. 中国有色金属学报, 2008; 18: 1971)
[4] Zhou D W, Xu S H, Zhang F Q, Peng P, Liu J S. Acta Metall Sin, 2010; 46: 97
(周惦武, 徐少华, 张福全, 彭平, 刘金水. 金属学报, 2010; 46: 97)
[5] ЛякишевH П, translated by Guo Q W. Metal Binary System Manual. Beijing: Chemical Industry Press,2009: 914
(梁基谢夫 著, 郭青蔚译. 金属二元系相图手册. 北京:化学工业出版社, 2009: 914)
[6] Gao X, Nie J F. Scr Mater, 2007; 57: 655
[7] Zeng X Q, Zhang Y, Lu C, Ding W J, Wang Y X, Zhu Y P. J Alloys Compd, 2005; 395: 213
[8] Qin B, Yu W B, Li F P, Li C M. Foundry, 2010; 59: 886
(秦兵, 于文斌, 李坊平, 李春梅. 铸造, 2010; 59: 886)
[9] Li S H, Zhang C X, Guan S K, Wen C L, Tian H T, Yu W W, Meng H. J Mater Sci Eng, 2012; 30: 563
(李少华, 张春香, 关绍康, 文春领, 田海棠, 于雯雯, 孟辉. 材料科学与工程学报, 2012; 30: 563)
[10] Zhang B P, Wang Y, Geng L, Lu C X. Mater Sci Eng, 2012; A39: 56
[11] Tong L B, Zheng M Y, Hua X S, Wu K, Xu S W, Kamado S, Kojima Y. Mater Sci Eng, 2010; A527: 4250
[12] Geng L, Zhang B P, Li A B, Dong C C. Mater Lett, 2009; 63: 557
[13] Cheng L. Master Thesis, Chongqing University of technlolgy, 2011
(程亮. 重庆理工大学硕士学位论文, 2011)
[14] Xiang Q, Wu R Z, Zhang M L. J Alloys Compd, 2009; 477: 832
[15] Nayyeri G, Mahmudi R, Salehi F. Mater Sci Eng, 2010; A527: 5353
[16] Pan X Q, Chen J H, Yan H G, Su B, Wei J Y, Fan C. Mater Sci Technol, 2013; 29: 169
[17] Wang P, Li J P, Guo Y C, Yang Z, Xia F, Wang J L. Rare Met Mater Eng, 2012; 41: 2095
(王萍, 李建平, 郭永春, 杨忠, 夏峰, 王建利. 稀有金属材料与工程, 2012; 41: 2095)
[18] Liu Z, Zhang Y, Mao P L, Yang C H. Spec Cast Nonferrous Alloys, 2012; 32: 1000
(刘正, 张越, 毛萍莉, 杨春海. 特种铸造及有色合金, 2012; 32: 1000)
[19] Shi D M, Wen B, Melnik R, Yao S, Li T J. J Solid State Chem, 2009; 82: 2664
[20] Pack J D, Monkhors H J. Phys Rev, 1977; 16B: 1748
[21] Perdew J P, Burke K, Ernzerhof M. Phys Rev Lett, 1996; 77: 3865
[22] Fagan S B, Mota R, Baierle R J, Paiva G, Da Silva A J R, Fazzio A. J Mol Struct, 2001; 539: 101
[23] Zhang H, Shang S L, Saal J E, Saengdeejing A, Wang Y, Chen L Q, Liu Z K. Intermetallics, 2009; 17: 878
[24] Groseh G H, Range K J. J Alloys Compd, 1996; 235: 250
[25] Suzuki A, Saddock N D, Jomes J W, Pollock T M. Acta Mater, 2005; 53: 2823
[26] Yu W Y. Master Thesis, Xiangtan University, 2009
(余伟阳. 湘潭大学硕士学位论文, 2009)
[27] Huang K. Solid State Physics. Beijing: Higher Education Press, 1985: 68
(黄昆. 固体物理学. 北京:高等教育出社, 1985: 68)
[28] Li C H, Hoe J L, Wu P. J Phys Chem Solids, 2003; 64: 201
[29] Sahu B R. Mater Sci Eng, 1997; B49: 74
[30] Lin W, Xu J H, Freeman A J. Phys Rev, 1992; 45B: 10863
[31] Huang Z W, Zhao Y H, Hou H, Han P D. Physica, 2012; 407B: 1075
[32] Yu W Y, Wang N, Xiao X B, Tang B Y, Peng L M, Ding W J. Solid State Sci, 2009; 11: 1400
[33] Nye J F. Physical Properties of Crystals. Oxford: Clarendon Press, 1964: 1
[34] Davis L C, Whitten W B, Danielson G C. J Phys Chem Solids, 1967; 28: 439
[35] Corkill J L, Cohen M L. Phys Rev, 1993; 48B: 17138
[36] Seidenkranz T, Hegenbarth E. Phys Status Solidi, 1976; 33A: 205
[37] Li Y F, Gao Y M, Xiao B, Min T, Fan Z J, Ma S Q, Xu L L. J Alloys Compd, 2010; 502: 28
[38] Hill R. Phys Soc Sect, 1952; 65A: 349
[39] Hong S, Fu C L. Intermetallics, 1999; 7: 5
[40] Pugh S F. Philos Mag, 1954; 45: 823
[41] Mattesini M, Ahuja R, Johansson B. Phys Rev, 2003; 68B: 184108
[42] Fu C L, Wang X D, Ye Y Y. Intermetallics, 1999; 7: 179
Outlines

/

〈 〉