DEPENDENCE OF PRIMARY PHASE AND ITS GROWTH DIRECTION ON SOLIDIFICATION PROCESS IN DIRECTIONALLY SOLIDIFIED Ti-46Al-2Cr-2Nb ALLOY

  • ZHANG Yuan ,
  • LI Xinzhong ,
  • LIU Guohuai ,
  • SU Yanqing ,
  • GUO Jingjie ,
  • FU Hengzhi
Expand
  • School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001

Received date: 2013-05-21

  Revised date: 2013-07-01

  Online published: 2013-09-11

Abstract

GE alloy Ti-(46--48)Al-2Cr-2Nb (atomic fraction) is well known for its high strength and improved ductility. The primary phase and its growth direction are important in controlling the lamellar direction of GE alloys. However it is greatly affected by solidification conditions. In this work, primary phase and its growth direction have been investigated by carrying out Bridgman-type directional solidification with different growth lengths ranging from 5 to 30 mm on Ti-46Al-2Cr-2Nb alloy. It is found that the primary phase is β at the beginning of directional solidification with constant temperature gradient (G=18 K/mm) and growth rate (v=20 μm/s). With the increase of growth length, Al gradually concentrates in the liquid between primary dendrites, which leads to the peritectic reaction L+β→α. With further increase of the growth length, growth competition between primary β phase and peritectic α phase is promoted, leading to gradual transition of primary phases from β  phase to α phase. The growth direction of primary phase in different stages of solidification has been characterized by EBSD analysis. The results indicate that primary β phase has a growth direction parallel to its preferential growth direction <100>β at the initial stage of solidification. By comparing the growth directions of the α2 grains formed from primary β phase and peritectic α phase,it is found that peritectic α phase related to primary β phase by the {110}β //{0001}α orientation relationship. Therefore, as the primary phase has transformed to α phase, the growth direction deviates from its preferential growth direction <0001>α at an angle of 45.9°. The growth direction of α  phase formed after the primary phase transformation is determined not only by the kinetic factors of solidification, but also by the β phase exiting at the beginning of directional solidification. These results provide fundamental references for understanding and controlling the lamellar orientation of GE alloys.

Cite this article

ZHANG Yuan , LI Xinzhong , LIU Guohuai , SU Yanqing , GUO Jingjie , FU Hengzhi . DEPENDENCE OF PRIMARY PHASE AND ITS GROWTH DIRECTION ON SOLIDIFICATION PROCESS IN DIRECTIONALLY SOLIDIFIED Ti-46Al-2Cr-2Nb ALLOY[J]. Acta Metall Sin, 2013 , 49(9) : 1061 -1068 . DOI: 10.3724/SP.J.1037.2013.00279

References

[1]Yamaguchi M, Johnson D R, Lee H N, Inui H.Intermetallics, 2000; 8: 511
[2]Kim S E, Lee Y T, Oh M H, Inui H, Yamaguchi M.Intermetallics, 2000; 8: 399
[3]Zollinger J, Lapin J, Daloz D, Combeau H.Intermetallics, 2007; 15: 1343
[4]Johnson D R, Inui H, Muto S, Omiya Y, Yamanaka T.Acta Mater, 2006; 54: 1077
[5]Lapin J, Pelachova T, Domankova M.Intermetallics, 2011; 19: 814
[6]Liu R C, Wang Z, Liu D, Bai C G, Cui Y Y, Yang R.Acta Metall Sin, 2013; 49: 641
(刘仁慈, 王震, 刘冬, 柏春光, 崔玉友, 杨锐.金属学报, 2013; 49: 641)
[7]Yamanaka T, Johnson D R, Inui H, Yamaguchi M.Intermetallics, 1999; 7: 779
[8]Xiao Z X. PhD Dissertation, Beihang University,2011
(肖志霞. 北京航空航天大学博士学位论文, 2011)
[9]Kim M C, Oh M H, Lee J H, Inui H, Yamaguchi M, Wee D M.Mater Sci Eng, 1997; A239-240: 570
[10]Li X Z, Sun T, Yu C X, Su Y Q, Cao Y Z, Guo J J, Fu H Z.Acta Metall Sin, 2009; 45: 1479
(李新中, 孙涛, 于彩霞, 苏彦庆, 曹勇智, 郭景杰, 傅恒志.金属学报, 2009; 45: 1479)
[11]Yang L L, Zheng L J, Xiao Z X, Yan J, Zhang H. Acta Metall Sin, 2010; 46: 879
(杨莉莉, 郑立静, 肖志霞, 闫洁, 张虎. 金属学报, 2010;46: 879)
[12]Xiao Z X, Zheng L J, Yang L L, Yan J, Zhang H. Acta Metall Sin, 2010; 46: 1223
(肖志霞, 郑立静, 杨莉莉, 闫洁, 张虎. 金属学报, 2010;46: 1223)
[13]Thomas M, Bacos M T. High Temp Mater, 2011; 3: 7
[14]Nie G. PhD Dissertation, Harbin Institute of Technology, 2012
(聂革. 哈尔滨工业大学博士学位论文, 2012)
[15] Xiao Z X, Zheng L J, Yan J, Yang L L, Zhang H. J Cryst Growth, 2011; 324: 309
[16]Xiao Z X, Zheng L J, Wang L, Yang L L, Zhang H. J Wuhan Univ Technol, 2011; 26: 197
[17]Fan J L. PhD Dissertation, Harbin Institute of Technology, 2012
(樊江磊. 哈尔滨工业大学博士学位论文, 2012)
[18]Daloz D, Hecht U, Zollinger J, Combeau H, Hazotte A, Zaloznik M. Intermetallics, 2011; 19: 749
[19]Fu H Z, Guo J J, Liu L, Li J S. Directional Solidification and Processing of Advanced Materials. Beijing:Science Press, 2008: 356
(傅恒志, 郭景杰, 刘林, 李金山. 先进材料定向凝固. 北京:科学出版社, 2008: 356)
[20]Charpentier M, Daloz D, Gautier E, Lesoult G, Hazotte A,Grange M. Metall Mater Trans, 2003; 34A: 2139
[21]Li Y X, Wu A P. Principle of Materials Processing.Beijing: Tsinghua University Press, 2005: 93
(李言祥, 吴爱萍. 材料加工原理. 北京: 清华大学出版社, 2005: 93)
[22]Glicksman E. Principles of Solidification: An Introduction to Modern Casting and Crystal Growth Concepts. New York: Springer, 2011: 347
[23]Su Y Q, Liu C, Li X Z, Guo J J, Li B S, Jia J, Fu H Z.Intermetallics, 2005; 13: 267
[24]Liu D M. PhD Dissertation, Harbin Institute of Technology,2012
(刘冬梅. 哈尔滨工业大学博士学位论文, 2012)
[25]Esaka H, Daimon H, Natsume Y, Ohsasa K, Tamura M G.Mater Trans, 2002; 43: 1312
[26]Singh A K, Muraleedharan K, Banerjee D. Scr Mater,2003; 48: 767

Outlines

/

〈 〉