Abstract

The Pb-free plastic encapsulated ball grid array (BGA) packages have been assembled to printed-circuit boards (PCBs) with SnPb solder material using reflowing process. Isothermal aging with 4, 9, 16 and 25 d was applied to the assembled packages and the microstructures of the solder joints in the BGA packages were observed using SEM. The electrical performance test was conducted before and after different periods of isothermal aging. The result showed that there were no failure in the BGA devices. It was found that intermetallic compounds (IMCs) in the PCB substrate side were Cu3Sn and Cu6Sn5 while Ni-Cu-Sn ternary compounds were in BGA substrate side. The thicknesses of IMCs on both sides increased with the time of isothermal aging. The IMC growth rate at PCB side was significantly greater than that at BGA substrate side. The aggregation of Pb-rich phase, cracks along substrate, broken IMCs, and voids, which have negative effects on the joints reliability, were observed in a few solder joints after long-term isothermal aging process.

Cite this article

HANG Chunjin , TIAN Yanhong , ZHAO Xin , WANG Chunqing . RESEARCH ON MICROSTRUCTURE OF Pb-FREE BGA SOLDER JOINT ASSEMBLED WITH Sn-Pb SOLDER DURING ISOTHERMAL AGING[J]. Acta Metall Sin, 2013 , 49(7) : 831 -837 . DOI: 10.3724/SP.J.1037.2012.00759

References

[1]Qu X, Chen Z X, Qi B, Lee T, Wang J J. Microelectron Reliab, 2007; 47: 2197
[2]Kim Y B, Noguchi H, Amagai H. Microelectron Reliab,2006; 46: 459
[3]Kannabiran A, Pannerselvam E T, Ramkumar S M. IEEE Trans Electron Packag Manuf, 2007; 30: 138
[4]Liang J, Downes S, Dariavach N, Shangguan D, Heinrich S M.J Electron Mater, 2004; 33: 1507
[5]Ha S S, Sung J Y, Yoon J W, Jung S B. Microelectron Eng, 2011; 88: 709
[6]Herkommer D, Punch J, Reid M. Microelectron Reliab,2010; 50: 116
[7]Zeng K J, Pierce M, Miyazaki H, Holdford B. J Electron Mater, 2012; 41: 253
[8]Snugovsky P, McCormick H, Bagheri S, Bagheri Z, Hamilton C,Romansky M. J Electron Mater, 2009; 38: 292
[9]Shang H X, Gao J X, Nicholson P I, Kenny S.Microelectron Reliab, 2011; 51: 994
[10]Khatibi G, Wroczewski W, Weiss B, Ipser H.Microelectron Reliab, 2009; 49: 1283
[11]Tu K N, Lee T Y, Jang J W, Li L, Frear D R, Zeng K,Kivilahti J K. Appl Phys, 2001; 89: 4843
[12]Nousiainen O, Putaala J, Kangasvieri T, Rautioaho R,Vahakangas J. J Electron Mater, 2006; 35: 1857
[13]Choubey A, Osterman M, Pecht M. IEEE Trans Device Mater Reliab, 2008; 8: 160
[14]Chuang T H, Cheng C Y, Chang T C. J Electron Mater, 2009; 38: 2762
[15]Koo J M, Jung S B. Microelectron Reliab, 2007; 47:2169
[16]Hsiao H Y, Liu C M, Lin H W, Liu T C, Lu C L, Huang Y S,Chen C, Tu K N. Science, 2012; 336: 1007
[17]Yost F G, Ganyard F P, Kamowsky M M. Metall Mater Trans, 1976; 7A: 1141
[18]Anderson I E, Walleser J W, Harringa J L, Laabs F, Kracher A. J Electron Mater, 2009; 38: 2770
[19]Zhong W H, Chan Y C, Alam M O, Wu B Y, Guan J F. J Alloys Compd, 2006; 414: 123
[20]Koo J M, Vu B Q, Kim Y N, Lee J B, Kim J W, Kim D U, Moon J N, Jung S B. J Electron Mater, 2008; 37: 118
[21]Laurila T, Vuorinen V, Kivilahti J K. Mater Sci Eng, 2005; R49: 1
[22]Lee T K, Ma H T, Liu K C, Xue J. J Electron Mater,2010; 39: 2564
[23]Xu L H, Pang J H L, Che F X. J Electron Mater,2008; 37: 880
[24]Lin H J, Chuang T H. Microelectron Reliab, 2011;51: 445
[25]Lin K S, Huang H Y, Chou C P. J Mater Eng Perform,2009; 18: 182
[26]Yoon J W, Noh B I, Lee Y H, Lee H S, Jung S B.Microelectron Reliab, 2008; 48: 1864
[27]Hang C J, Wang C Q, Mayer M, Tian Y H, Zhou Y, Wang H H.Microelectron Reliab, 2008; 48: 416

Outlines

/

〈 〉