MICROSTRUCTURES AND MECHANICAL PROPERTIES OF 0Cr13 FERRITIC STAINLESS STEEL PROCESSED BY EQUAL–CHANNEL ANGULAR PRESSING AND SUBSEQUENT ANNEALING TREATMENT

  • YANG Muxin YANG Gang LIU Zhengdong Du Xiqian HUANG Chongxiang
Expand
  • 1. Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093
    2. Institute for Structural Materials, Central Iron and Steel Research Institute, Beijing 100081
    3. College of Architecture and Environment, Sichuan University, Chengdu 610065

Received date: 2012-05-22

  Revised date: 2012-07-31

  Online published: 2012-12-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50971045 and 11172187) and Fundamental Research Funds for the Central Universities (No.0212SCU04A05)

Abstract

In comparison with austenitic stainless steel, the ferritic stainless steel has obvious advantage in price due to its lower nickel content. However, the relatively poor ductility and toughness limit its applications. To overcome these shortcomings, a new thermo–mechanical approach, involving processing by severe plastic deformation and proper annealing treatment to introduce a bimodal grain size distribution, was adopted for achieving high work–hardening capability, superior strength–ductility combination and good impact toughness in metallic materials. In this work, the combined effects of severe plastic deformation and partially recrystallization on the microstructures and mechanical properties of a ferritic stainless steel were investigated and compared with the traditional forging and annealing process. An solution–treated ferritic stainless steel (0Cr13, AISI 405) was subjected to equal–channel angular pressing (ECAP, an important kind of severe plastic deformation) for two passes at room temperature and subsequent annealing treatments. Optical microscope (OM) and transmission electron microscopy (TEM) observations showed that ultrafine-grained (UFG) structure was obtained in the ECAP–processed sample. After subsequent annealing at 650—750 ℃ for 1 h, partial recrystallization occurred and the remaining island–like UFG grains (10%—35% volume fraction) distributed uniformly. Statistical measurements indicated that the microstructures of the annealed ECAP samples exhibited a bimodal grain size distribution including relatively coarse recrystallized grains (CRGs) and remaining ultrafine grains (UFGs). The average grain size for CRGs determined from OM observations was 5.1—8.3 μm and the average grain size for UFGs measured from TEM observations was 418—525 nm. By contrast, the annealed forged sample (700℃) exhibited a unimodal grain size distribution with average grain size of about 74 μm. Tensile and impact tests showed that the strength of 0Cr13 ferritic stainless steel could be improved greatly through grain refinement by ECAP process, and the strength–ductility combination could be modulated via sacrificing some strength for ductility by subsequent annealing treatment. In comparison with the conventional sample (forging+annealing at 700 ℃), the tested steel processed by the optimal processing involving ECAP deformation and annealing treatment at 700℃ showed higher yield strength, uniform ductility and static toughness (enhanced by 10%, 35% and 70% respectively), simultaneously a comparable impact toughness (212 J/cm2). The refined microstructure and higher work–hardening capacity were responsible for the improved mechanical properties of the annealed ECAP samples and the strengthening mechanisms were discussed based on the experimental results.

Cite this article

YANG Muxin YANG Gang LIU Zhengdong Du Xiqian HUANG Chongxiang . MICROSTRUCTURES AND MECHANICAL PROPERTIES OF 0Cr13 FERRITIC STAINLESS STEEL PROCESSED BY EQUAL–CHANNEL ANGULAR PRESSING AND SUBSEQUENT ANNEALING TREATMENT[J]. Acta Metall Sin, 2012 , 48(12) : 1422 -1430 . DOI: 10.3724/SP.J.1037.2012.00291

References

[1] Fujita T. Translated by Ding W H, Zhang X J, Chen Y Z. Heat Treatment of Stainless Steels. Beijing: China Machine Press, 1983: 106

(藤田辉夫著, 丁文华, 张绪江, 陈玉璋译. 不锈钢的热处理. 北京: 机械工业出版社, 1983: 106)

[2] Lu S Y, Zhang T K, Kang X F, Yang C Q, Wang X. Stainless Steel. Beijing: Atomic Energy Press, 1995: 77

(陆世英, 张廷凯, 康喜范, 杨长强, 王 熙. 不锈钢. 北京: 原子能出版社, 1995: 77)

[3] Wen Y Q. Ultra–Fine Grained Steels–Microstructural Refinement Theory and Controlled Technology of Steels. Beijing: Metallurgical Industry Press, 2003: 7

(翁宇庆. 超细晶钢-钢的组织细化理论与控制技术. 北京: 冶金工业出版社, 2003: 7)

[4] Song R, Ponge D, Raabe D, Speer J G, Matlock D K. Mater Sci Eng, 2006; A441: 1

[5] Wen D C. Mater Trans, 2006; 47: 2779

[6] Song R, Ponge D, Raabe D. Acta Mater, 2005; 53: 4881

[7] Calcagnotto M, Ponge D, Raabe D. Mater Sci Eng, 2010; A527: 7832

[8] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103

[9] Wu S D, An X H, Han W Z, Qu S, Zhang Z F. Acta Metall Sin, 2010; 46: 257

(吴世丁, 安祥海, 韩卫忠, 屈伸, 张哲峰. 金属学报, 2010; 46: 257)

[10] Yang G, Yang M X, Liu Z D, Wang C. J Iron Steel Res Inter, 2011; 18: 40

[11] Zhu Y T, Liao X Z. Nat Mater, 2004; 3: 351

[12] Wang Y M, Chen M W, Zhou F H, Ma E. Nature, 2002; 419: 912

[13] Wang Y M, Ma E, Chen M W. Appl Phys Lett, 2001; 80:2395

[14] Ma E. JOM, 2006; 58: 49

[15] Yang G, Huang C X, Wang C, Zhang L Y, Hu C, Zhang Z F, Wu S D. Mater Sci Eng, 2009; A515: 199

[16] Wang J T, Xu C, Du Z Z, Qu G Z, Langdon T G. Mater Sci Eng, 2005; A410: 312

[17] Yang M X, Yang G, Liu Z D, Wang C, Hu C, Huang C X. Acta Metall Sin, 2012; 48: 164

(杨沐鑫, 杨钢, 刘正东, 王昌, 胡超, 黄崇湘. 金属学报, 2012; 48: 164)

[18] JIS G. Cold–Rolled Stainless Steel Plate and Steel Belt Technical Standards. Tokyo: JSA, 2005: 20

[19] Zhao Y H, Bingert J F, Liao X Z, Cui B Z, Han K, Sergueeva A V, Mukherjee A K, Valiev R Z, Langdon T G, Zhu Y T. Adv Mater, 2006; 18: 2949

[20] William D, Callister Jr. Fundamentals of Materials Science and Engineering. 5th ed. New York: John Wiley &Sons Inc, 2001:185

[21] Fang D R, Duan Q Q, Huang C X, Wu S D, Zhang Z F, Li J J, Zhao N Q. Acta Metall Sin, 2007; 43: 1251

(房大然, 段启强, 黄崇湘, 吴世丁, 张哲峰, 李家俊, 赵乃勤. 金属学报, 2007; 43: 1251)

[22] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S X. Acta Mater, 2006; 54: 655

[23] ASTM E 112–96. Standard Test Methods for Determining Average Grain Size. West Conshohocken: ASTM International, 2004: 10

[24] Huang C X, Yang G, Gao Y L, Wu S D, Zhang Z F. Mater Sci Eng, 2008; A485: 643

[25] Huang C X, Yang G, Wang C, Zhang Z F, Wu S D. Metall Mater Trans, 2011; 42 A: 2061

[26] Wang C F, Wang M Q, Shi J, Hui W J, Dong H. Scr Mater, 2008; 58: 492

Outlines

/

〈 〉