PHASE FIELD MODEL FOR MICROSTRUCTURE EVOLUTION OF SUBGRAIN IN DEFORMATION ALLOY

  • GAO Yingjun LUO Zhirong HUANG Lilin HU Xiangying
Expand
  • 1. Key Lab of Engineering Disaster Prevention and Structural Safety of China Ministry of Education, Guangxi University, Nanning 530004
    2. College of Physics Science and Engineering, Guangxi University, Nanning 530004
    3. International Center for Materials Physics, Chinese Academy of Science, Shenyang 110016

Received date: 2012-05-10

  Revised date: 2012-07-29

  Online published: 2012-10-11

Supported by

Supported by National Science Foundation of China (Nos.51161003 and 50661001)

Abstract

It is well know that static recrystallization (SRX), which occurs during post–deformation annealing, is greatly affected by the deformation formed during cold working. Therefore, to investigate and predict the SRX microstructure and SRX texture numerically with high accuracy, it is necessary to simulate the SRX process taking the deformation microstructure into consideration. A model that couples the crystal plasticity finite element method and microstructure evolution model is believed to be the most promising approach for SRX microstructure design. In this paper, the subgrain structure evolution is firstly studied by using the multi–state phase field (MSPF) model coupling with the lattice deformation model including the stored energy distribution of deformed alloy. The initial subgrain growth through the mechanism of mergence and swallow during recrystallization process are simulated by MSPF. The different amount of deformation effecting on subgrain distribution and subgrain growth rate are studied systematically. The calculated results show that in the region with higher stored energy, for example, around grain boundaries, there are very dense finer subgrains which recrystallize earliestly in the higher stored energy region during recrystallization process, and grow up by mergencing and swallowing, while the distribution of subgrains inside the deformation grain is relative uniform and with relative large subgrains which grow up slowly. The distribution of grains obtained by the weighted frequency shows that the grain distribution changes from small to large grain is fast for the larger deformed alloy, while the change is slow for the less deformed alloy. All the results are agreement with experimental ones.

Cite this article

GAO Yingjun LUO Zhirong HUANG Lilin HU Xiangying . PHASE FIELD MODEL FOR MICROSTRUCTURE EVOLUTION OF SUBGRAIN IN DEFORMATION ALLOY[J]. Acta Metall Sin, 2012 , 48(10) : 1215 -1222 . DOI: 10.3724/SP.J.1037.2012.00265

References

[1] Yang X Y, Zhu Y K, Zhang L. Chin J Mater Res, 2010; 24: 169

(杨续跃, 朱亚坤, 张 雷. 材料研究学报, 2010; 24: 169)

[2] Yang X Y, Jiang Y P. Acta Metall Sin, 2010; 46: 451

(杨续跃, 姜育培. 金属学报, 2010; 46: 451)

[3] Humphreys F J, HatherlyM. Recrystallization and Related Annealing Phenomena. Oxford: Elsevier Science, 1995: 1

[4] Wu X X, Yang X Y, Zhang L, Zhang Z L. Acta Metall Sin, 2011; 47: 140

(吴新星, 杨续跃, 张雷, 张之岭. 金属学报, 2011; 47: 140)

[5] Kim K H, Suh B C, Bac J H. Scr Mater, 2010; 63: 716

[6] Chun Y B, Hwang S K. Acta Mater, 2008; 56: 369

[7] Huang M X, Pedro E J, Castillo R D, Bouaziz O, Zwaag S. Acta Mater, 2009; 57: 3431

[8] Baudin T, Julliard F, Paillard P, Penelle R. Scr Mater, 2000; 43: 63

[9] Choi S H, Cho J H. Mater Sci Eng, 2005; A405: 86

[10] Sepehrband P, Esmaeli S. Scr Mater, 2010; 63: 4

[11] Zheng C W, Lan Y J, Xiao N M, Li D Z, Li Y Y. Acta Metall Sin, 2006; 42: 474

(郑成武, 兰勇军, 肖纳敏, 李殿中, 李依依. 金属学报, 2006; 42: 474)

[12] Raabe D, Hautchrli L. Comput Mater Sci, 2005; 34: 299

[13] Raabe D. Annu Rev Mater Res, 2002; 32: 53

[14] Radhakrishnan B, Sarma G. Philos Mag, 2004; 84: 2341

[15] Takaki T, Yamanaka A, Higa Y, Tomita Y. Mater Trans, 2008; 49: 2559

[16] Gao Y J, Luo Z R, Hu X Y, Huang C G. Acta Metall Sin, 2010; 46: 1161

(高英俊, 罗志荣, 胡项英, 黄创高. 金属学报, 2010; 46: 1161)

[17] Takaki T, Tomita Y. Int J Mech Sci, 2010; 52: 320

[18] Fan D, Chen L Q. Acta Mater, 1997; 45: 3297

[19] Wang M T, Zong B Y, Wang G. Comput Mater Sci, 2009; 45: 217

[20] Gao Y J, Luo Z R, Zhang S Y, Huang C G. Acta Metall Sin, 2010; 46: 1473

(高英俊, 罗志荣, 张少义, 黄创高. 金属学报, 2010; 46: 1473)

[21] Zhao P. Fundamental Course of Materials Science. Harbin: Harbin Institute of Technology Press, 1998: 148

(赵品. 材料科学基础教程. 哈尔滨: 哈尔滨工业大学出版社, 1998: 148)

[22] Oono Y, Pori S. Phys Rev Lett, 1987; 58: 836

[23] Sitdikov O, Sakai T, Avtokratova E, Kaibyshev R, Tsuzaki K, Watanabe Y. Acta Mater, 2008; 56: 821

[24] Pennock G M, Drury M R, Spiers C J. J Struct Geology, 2005; 27: 2159

[25] Xu S W. Master Thesis, Harbin Institute of Technology, 2006

(徐世伟. 哈尔滨工业大学硕士学位论文, 2006)

Outlines

/

〈 〉