COMPOSITION DESIGN OF HIGH–STRENGTH MARTENSITIC PRECIPITATION HARDENING STAINLESS STEELS BASED ON A CLUSTER MODEL

  • WANG Qing ZHA Qianfeng LIU Enxue DONG Chuang WANG Xuejun TAN Chaoxin JI Chunjun
Expand
  • 1. Key Laboratory of Materials Modification of Ministry of Education, Dalian University of Technology, Dalian 116024
    2. School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
    3. Shenyang Blower Works Group Corporation, Shenyang 110869
    4. School of Energy and Power Engineering, Dalian University of Technology, Dalian 116024

Received date: 2012-02-07

  Revised date: 2012-05-28

  Online published: 2012-10-11

Supported by

Supported by National Natural Science Foundation of China (Nos.51171035 and 50901012) and Liaoning Province Postdoctoral Startup Fund

Abstract

The present work investigates composition characteristics of martensitic precipitation hardening stainless steels using a cluster–plus–glue–atom model. In this kind of steels based on the basic ternary Fe–Ni–Cr, the lowest solubility limit of high–temperature austenite corresponds to the cluster formula [NiFe12]Cr3, where NiFe12 is a cuboctahedron centered by Ni and surrounded by 12 Fe atoms in fcc structure and Cr serves as glue atoms. New multi–component alloys were designed by adding C, Mo, Nb and Cu into the basic [NiFe12]Cr3 with self–magnification of cluster formula and similar element substitution. These alloys were prepared by copper mould suction casting method, then solid–solution treated at 1323 K for 2 h followed by water–quenching, and finally aged 753 K for 4 h. The experimental results show that the microstructures and properties of the serial solid–solution treated and aged alloys vary with alloying elements and their contents. Among them, the {[(Ni13Cu3)Fe192](Cr45Mo2.5Nb0.5)}C1 alloy has higher microhardness and tensile strengths, the hardness is 397 HV, yield strength is 971 MPa and ultra strength is 1093 MPa after aging treatment. {[(Ni13Cu3)Fe192](Cr45Mo2.5Nb0.5)}C1 exhibits good corrosion–resistance in 3.5%NaCl solution.

Cite this article

WANG Qing ZHA Qianfeng LIU Enxue DONG Chuang WANG Xuejun TAN Chaoxin JI Chunjun . COMPOSITION DESIGN OF HIGH–STRENGTH MARTENSITIC PRECIPITATION HARDENING STAINLESS STEELS BASED ON A CLUSTER MODEL[J]. Acta Metall Sin, 2012 , 48(10) : 1201 -1206 . DOI: 10.3724/SP.J.1037.2012.00053

References

[1] Zhao X C, Song W S, Yang Z Y, Liang J X, Li W H. High Strength and Super–high Strength Stainless Steels. Beijing: Metallurgical Industry Press, 2008: 244

(赵先存, 宋为顺, 杨志勇, 梁剑雄, 李文辉. 高强度超高强度不锈钢. 北京: 冶金工业出版社, 2008: 244)

[2] Floreen S. Met Rev, 1968; 13: 115

[3] Decker R F, Floreen S. Proc Conf on Maraging Steels–Recent Developments and Applications, Warrendale, PA:TMS–AIME, 1988: 1

[4] Garrison W M. JOM, 1990; 42: 20

[5] Zhou Q Q, Zhai Y C. Acta Metall Sin, 2009; 45: 1249

(周倩青, 翟玉春. 金属学报, 2009; 45: 1249)

[6] Qiao G Y, Xiao F R, Tan C X. Spec Steel, 1998; 19: 18

(乔桂英, 肖福仁, 谭朝鑫. 特殊钢, 1998; 19: 18)

[7] Hsiao C N, Chiou C S, Yang J R. Mater Chem Phys, 2002;74: 134

[8] Wang J, Zou H, Li C, Yeng Y H, Qiu S Y, Shen B L. Nucl Eng Des, 2006; 236: 2531

[9] Sen D, Patra A K, Mazumder S, Mittra J, Dey G K, De P K. Mater Sci Eng, 2005; A397: 370

[10] Schaeffler A L. Met Prog, 1949; 56: 680

[11] Delong W T, Ostrom G, Szumachowski E. Weld J, 1956; 35: s521

[12] Olson G B. Science, 1997; 277: 1237

[13] Xu W, Rivera–Diaz–del–Castillo P E J, Yan W, Yang K, San Martin S, Kestens L A I, van der Zwaag S. Acta Mater, 2010; 58: 4067

[14] Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H, Wu J, Xia J H. J Phys, 2007; 40D: 273

[15] Wang Q, Dong C, Qiang J B, Wang Y M. Mater Sci Eng, 2007; A18: 449

[16] Zhang J, Wang Q, Wang Y M, Li C Y, Wen L S, Dong C. J Mater Res, 2010; 25: 328

[17] Ma R T, Hao C P, Wang Q, Ren M F, Wang Y M, Dong C. Acta Metall Sin, 2010; 46: 1034

(马仁涛, 郝传璞, 王清, 任明法, 王英敏, 董闯. 金属学报, 2010; 46: 1034)

[18] Li B Z, Wang Q, Wang Y M, Li C Y, Qiang J B, Ji C J, Dong C. Metall Mater Trans, 2012; 43A: 544

[19] Takeuchi A, Inoue A. Mater Trans JIM, 2005; 46: 2817

[20] Raynor G V, Rivlin V G. Phase Equilibria in Iron Ternary Alloys. London: Inst Metals, 1988: 316

[21] Abdelshehid M, Mahmodieh K, Mori K, Chen L, Stoyanov P, Davlantes D, Foyos J, Ogren J, Clark Jr R, Es–Said O S. Eng Failure Anal, 2007; 14: 626

[22] Dong H, Esfandiari M, Li X Y. Surf Coat Technol, 2008; 202: 2969

[23] Greer A L. Science, 1995; 267: 1947

[24] Shiflet G. Science, 2003; 300: 443

[25] Lo K H, Shek C H, Lai J K L. Mater Sci Eng, 2009; R65: 39

[26] H¨attestrand M, Nilsson J O, Stiller K, Liu P, Andersson M. Acta Mater, 2004; 52: 1023

Outlines

/

〈 〉