论文

Ti-BASED AMORPHOUS COMPOSITES WITH QUANTITATIVELY CONTROLLED IN--SITU FORMATION OF DENDRITES

  • TANG Meng-Jiang ,
  • ZHU Zheng-Wang ,
  • FU Hua-Meng ,
  • YU Ai-Min ,
  • LI Hong ,
  • ZHANG Hong-Wei ,
  • MA Guo-Feng ,
  • ZHANG Hai-Feng ,
  • HU Zhuang-Qi
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2012-04-13

  Revised date: 2012-04-24

  Online published: 2012-07-11

Abstract

A series of  (Ti32.8Zr30.2Ni5.3Cu9Be22.7)100-x (Ti61.5Zr36.4Cu2.1)x (x=10-95) bulk amorphous composites with quantitatively controlled in-situ formation of bcc-dendrites were prepared. The microstructures were analyzed by SEM, XRD and TEM. Thermal behaviors were examined using DSC. The results show that the size and volume fraction of dendrites depend on x in the composites. With increasing x, the volume fraction of dendrites rises monotonically from 20% to 90%. The microstructural transition between the matrix and the dendrites is smooth and successive with no phases observed at the interface. Compression tests show the size and volume fraction of dendrites largely influence the mechanical properties of composites. When the volume fraction is larger than the critical value (approximately 30% in the present work), the plasticity of composites cannot be improved. When the volume fraction is over the critical value, the higher the volume fraction of dendrites, the larger the plastic strain, the stronger the work hardening capacity. It implies that the properties of composite can be mediated by the tunable volume fraction of dendrites. These findings are significant to develop the controllable microstructure and performance materials. When x=90, the plastic strain and the compressive strength of the composites reach 14.4% and 1917 MPa, respectively.

Cite this article

TANG Meng-Jiang , ZHU Zheng-Wang , FU Hua-Meng , YU Ai-Min , LI Hong , ZHANG Hong-Wei , MA Guo-Feng , ZHANG Hai-Feng , HU Zhuang-Qi . Ti-BASED AMORPHOUS COMPOSITES WITH QUANTITATIVELY CONTROLLED IN--SITU FORMATION OF DENDRITES[J]. Acta Metall Sin, 2012 , 48(7) : 861 -866 . DOI: 10.3724/SP.J.1037.2012.00198

References

[1] Wang WH, Dong C, Shek C H. Mater Sci Eng, 2004; R44: 45

[2] Yavari A R, Lewandowski J J, Eckert J. MRS Bull, 2007; 32: 635

[3] Schuh C A, Hufnagel T C, Ramamurty U. Acta Mater, 2007; 55: 4067

[4] Johnson W L. MRS Bull, 1999; 24: 42

[5] Conner R D, Dandliker R B, Johnson W L. Acta Mater, 1998; 46: 6089

[6] Hays C C, Kim C P, Johnson W L. Phys Rev Lett, 2000; 84: 2901

[7] Eckert J, Kuhn U, Mattern N, He G, Gebert A. Intermetallics, 2002; 10: 1183

[8] Fan C, Ott R T, Hufnagel T C. Appl Phys Lett, 2002; 81: 1020

[9] Qiu K Q, Wang A M, Zhang H F, Ding B Z, Hu Z Q. Intermetallics, 2002; 10: 1283

[10] Fu H M, Wang H, Zhang H F, Hu Z Q. Scr Mater, 2006; 54: 1961

[11] Zhang H F, Wang A M, Li H, Sun W S, Ding B Z, Hu Z Q, Cai H N, Wang L, Li W. J Mater Res, 2006; 21: 1351

[12] Zhu Z W, Zhang H F, Wang H, Ding B, Hu Z Q, Huang H. J Mater Res, 2009; 24: 3109

[13] Zhu Z W, Zhang H F, Hu Z Q, Zhang W, Inoue A. Scr Mater, 2010; 62: 278

[14] Deng S T, Diao H, Chen Y L, Yan C, Zhang H F, Wang A M, Hu Z Q. Scr Mater, 2011; 64: 85

[15] Hofmann D C, Suh J Y, Wiest A, Duan G, Lind M L, Demetriou M D, Johnson W L. Nature, 2008; 451: 1085

[16] Hofmann D C, Suh J Y, Wiest A, Lind M L, Demetriou M D, Johnson W L. PNAS, 2008; 105: 20136

[17] Wu Y, Xiao Y, Chen G L, Liu C T, Lu Z P. Adv Mater, 2010; 22: 2770

[18] Qiao J W, Wang S, Zhang Y, Liaw P K, Chen G L. Appl Phys Lett, 2009; 94: 151905

[19] Mu J, Zhu Z W, Zhang H F, Hu Z Q, Wang Y D, Ren Y. Acta Mater, 2010; 58: 6267

[20] Tang M Q, Zhang H F, Zhu Z W, Fu H M, Wang A M, Li H, Hu Z Q. J Mater Sci Technol, 2010; 26: 481

[21] Qiao J W, Sun A C, Huang E W, Zhang Y, Liaw P K, Chuang C P. Acta Mater, 2011; 59: 4126
Outlines

/

〈 〉