论文

EFFECT OF NITROGEN ON MARTENSITIC TRANSFORMATION AND MECHANICAL PROPERTIES OF TWIP STEEL

  • HUANG Bao-Xu ,
  • YU Zhang-Zheng ,
  • YU Xiao-Dong ,
  • RONG Yong-Hua
Expand
  • 1) School of Materials Science and Engineering, Research Institute of Non--ferrous Metals, Liaocheng University, Liaocheng 252059
    2) State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences, Lanzhou 730000
    3) School of Materials Science and Engineering, Shanghai Jiaotong University, Shanghai 200240

Received date: 2012-02-06

  Revised date: 2012-04-24

  Online published: 2012-07-11

Abstract

Twinning induced plasticity (TWIP) steels show large elongation and high tensile strength,
exhibiting a super balance between strength and plasticity. Until now, the effects of Mn, Si and Al on stacking
fault energy (SFE) and phase transformation of TWIP steel had been investigated, but the effect of N on phase
transformation, especially martensitc transformation in TWIP steel has not been reported. In the present paper, the
mechanical properties of TWIP steel with the addition of N were tested. The phases were analyzed by XRD and
the microstructure was characterized by TEM. The average and local probabilities of stacking faults were also
calculated by using shifts of X-ray peak and electron diffraction spot, respectively. Compared with the
conventional TWIP steel, the results showed that at a lower SFE level, when fcc austensite or hcp martensite
transformed to bcc martensite, the largest interstice decreased from 0.1047 to 0.0725 nm. The lattice distortion
energy of bcc martensite was greatly enlarged by N, which situated in the interstices, leading to the suppression of the bcc martensitic transformation. As a result, the content of hcp martensite increased, causing the increase of
strength and decrease of plasticity. Besides, the results also showed that deformation increased stacking faults and
hcp or bcc martensitic transformation consumed a large number of stacking faults.

Cite this article

HUANG Bao-Xu , YU Zhang-Zheng , YU Xiao-Dong , RONG Yong-Hua . EFFECT OF NITROGEN ON MARTENSITIC TRANSFORMATION AND MECHANICAL PROPERTIES OF TWIP STEEL[J]. Acta Metall Sin, 2012 , 48(7) : 769 -774 . DOI: 10.3724/SP.J.1037.2012.00047

References

[1] Grassel O, Frommeyer G, Derder C, Hofmann H. J Phys IV France, 1997; 5: 383

[2] Frommeyer G, Brux U, Neumann P. ISIJ Int, 2003; 43: 438

[3] Vercammen S, Blanpain B, De Cooman B C, Wollants P. Acta Mater, 2004; 52: 2005

[4] Sato K, Ichinose M, Hirotsu Y, Inoue Y. ISIJ Int, 1989; 29: 868

[5] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1

[6] Grassel O, Kruger L, Frommeyer G, Meyer L W. Int J Plasticity, 2000; 16: 1391

[7] Schramm R E, Reed R P. Metall Trans, 1975; 6A: 1345

[8] Yakubtsov I A, Ariapour A, Perovic D D. Acta Mater, 1999; 47:1271

[9] Wan J F, Huang X, Chen S P, Hsu T Y (Xu Z Y). Mater Trans JIM, 2002; 43: 920

[10] Wan J F, Chen S P, Hsu T Y (Xu Z Y). Acta Metall Sin, 2000; 36: 679

(万见峰, 陈世朴, 徐祖耀. 金属学报, 2000; 36: 679)

[11] Huang B X, Wang X, Wang L, Rong Y. Metall Mater Trans, 2008; 39A: 717

[12] Huang B X. PhD Thesis, Shanghai Jiaotong University, 2007

(黄宝旭. 上海交通大学博士论文, 2007)

[13] Huang X, Wan J F, Chen S P, Hsu T Y (Xu Z Y). J Shanghai Jiaotong Univ, 2002; 36: 21

(黄幸, 万见峰, 陈世朴, 徐祖耀. 上海交通大学学报, 2002; 36: 21)

[14] Fan X. Metal X–ray Analysis. Beijing: China Machine Press, 1996: 36

(范雄. 金属X射线学. 北京: 机械工业出版社, 1996: 36)

[15] Zuo Y S, Chen W Z, Liang W. Modern Methods of Materials Testing. Beijing: Beijing University of Technology Press, 2000: 101

(左演声, 陈文哲, 梁伟. 材料现代分析方法. 北京: 北京工业大学出版社, 2000: 101)

[16] Rong Y H, He G, Guo Z H, Chen S P, Hsu T Y (Xu Z Y). J Mater Sci Technol, 2002; 18: 459

[17] Nishiyama Z, Kakinoki J, Kajiwara S. J Phys Soc Jpn, 1965; 20: 1192

[18] Kajiwara S. J Appl Phys, 1970; 9: 385

[19] Kajiwara S. J Phys Soc Jpn, 1967; 22: 795

[20] Wang X D, Huang B X, Rong Y H, Wang L. J Appl Phys, 2007; 101: 093511

[21] Pan J S, Tong J M, Tian M B. Fundamental of Materials. Beijing: Tsinghua University Press, 2002: 18

(潘金生, 仝健民, 田民波. 材料科学基础. 北京: 清华大学出版社, 2002: 18)

[22] Yang F J. Atomic Physics. Beijing: Higher Education Press, 1985: 509

(杨福家. 原子物理学. 北京: 高等教育出版社, 1985: 509)

[23] Jiang B, Qi X, Yang S, Yang S, ZhouW, Hsu T Y (Xu Z Y). Acta Mater, 1998; 46: 501

[24] Warren B E. X-ray diffraction. Massachusett: Addison– Wesley, 1969: 275

[25] Hsu T Y (Xu Z Y). Acta Metall Sin, 1980; 16: 430

(徐祖耀. 金属学报, 1980; 16: 430)

[26] Hsu T Y (Xu Z Y). Martensitic Transformation and Martensite. Beijing: Science Press, 1999: 83

(徐祖耀. 马氏体相变与马氏体. 北京: 科学出版社, 1999: 83)
Outlines

/

〈 〉