论文

VALENCE ELECTRON STRUCTURE ANALYSIS OF EQUILIBRIUM AND METASTABLE PHASES OF Al3M(M=Ti, Zr, Hf)

  • HUANG Lan
Expand
  • College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124

Received date: 2011-11-30

  Revised date: 2012-03-26

  Online published: 2012-04-11

Supported by

National Basic Research Program of China (No. 2012CB723307)

Abstract

The valence electron structure of Al3M(M=Ti, Zr, Hf) with three crystal structures (L12, D022, D023) and the corresponding strongest bond energy (EA) values have been calculated from the empirical electron theory (EET) of solids and molecules. Based on the calculated EA, the stability of the phases with different structures and the sequence of phase transition have been analyzed semi--quantitatively. The results showed that, the EA of the equilibrium phases, i.e., D022-Al3Ti, D023-Al3Zr and D022-Al3Hf, were 57.7, 71.6 and 75.6 kJ/mol, respectively, which showed the same trend in magnitude with the corresponding melting point. This consistence supports the reliability of EET--based calculation results. Similarly, the EAof Al3Ti, Al3Zr and Al3Hf with three structures have been calculated and the calculated phase transition sequences are the same as the experimental results and those from first--principles calculation. The L12-type metastable phases of three intermetallic compounds exhibit many excellent characteristics, whereas their phase stability is crucial for application. The EA is supposed to be a measure for the stability of metastable phase. The calculated EA of L12 structure implied the phase stability in the order of Al3Ti3Zr3Hf, which was the same as that from the transition temperatures experimentally. The EA calculated by EET, therefore, could be a good measure for the stability of metastable phase.

Cite this article

HUANG Lan . VALENCE ELECTRON STRUCTURE ANALYSIS OF EQUILIBRIUM AND METASTABLE PHASES OF Al3M(M=Ti, Zr, Hf)[J]. Acta Metall Sin, 2012 , 48(4) : 492 -501 . DOI: 10.3724/SP.J.1037.2011.00742

References

[1] Zhang Y G, Han Y F, Chen G L, Guo J T, Wan X J, Feng D. Intermetallic Compounds of Structural Materials. Beijing:International Industry Press, 2001: 833

    (张永刚, 韩雅芳, 陈国良, 郭建亭, 万晓景, 冯涤. 金属间化合物结构材料.北京: 国际工业出版社, 2001: 833)

[2] Hui L H, Geng H R, Wang S R, Xu J.  Mech Eng Mater, 2007; 31: 1

    (惠林海, 耿浩然, 王守仁, 徐杰. 机械工程材料, 2007; 31: 1)

[3] Chen G L.  Mater Rev, 2000; 24: 1

    (陈国良. 材料导报, 2000; 24: 1)

[4] Ding J J, Qin G W, Hao S M, Wang X T, Chen G L. J Phase Equilib, 1996; 17: 117

[5] Murray J, Peruzzi A, Abriata J P.  J Phase Equilib, 1992; 13: 227

[6] Okamoto H.  J Phase Equilib Diffus, 2006; 27: 538

[7] Srinivasan S, Desch P B, Schwarz R B.  Scr Metall Mater, 1991; 25: 2513

[8] Schwarz R B, Desch P B, Srinivasan S, Nash P. Nanostruct Mater, 1992; 1: 37

[9] Srinivasan S, Desch P B, Schwarz R B. In: Turchi P E A, Gonis A eds., Statics and Dynamics of Alloy Phase Transformation.New York: Plenum Press, 1994: 81

[10] Knipling K E, Dunand D C, Seidman D N.  Metall Mater Trans,2007; 38A: 2553

[11] Knipling K E, Dunand D C, Seidman D N.  Z Metallkd, 2006; 97: 246

[12] Perdew J P, Zunger A.  Phys Rev, 1981; 23B: 5048

[13] Wu Z G, Cohen R E.  Phys Rev, 2006; 73B: 235116--1

[14] Yu R H.  Chin Sci Bull, 1978; 23: 217

     (余瑞璜. 科学通报, 1978; 23: 217)

[15] Yu R H.  Chin Sci Bull, 1981; 26: 206

     (余瑞璜. 科学通报, 1981; 26: 206)

[16] Carlsson A E, Meschter P J.  J Mater Res, 1989; 4: 1060

[17] Ghosh G, Asta M.  Acta Mater, 2005; 53: 3225

[18] Kaufman L, Nesor H.  Can Metall Q, 1975; 14: 221

[19] Colinet C, Pasturel A.  Intermetallics, 2002; 10: 751

[20] Alcock C B, Jacob K T, Zador S.  At Energy Rev, 1976; 6: 1

[21] Guo J Q, Ohtera K.  Mater Lett, 1996; 27: 343

[22] Anderson O K.  Phys Rev, 1975; 12B: 3060

[23] Colinet C, Pasturel A.  J Alloys Compd, 2001; 319: 154

[24] Meschel S V, Kleppa O.  J Alloys Compd, 1993; 191: 11

[25] Colinet C, Pasturel A.  Phys Rev, 2001; 64B: 1

[26] Wen J B, Ren M H, Chen S P, Rong Y H.  J Shanghai Jiao Tong Univ,1998; 32: 73

     (文九巴, 任敏华, 陈世朴, 戎咏华. 上海交通大学学报, 1998; 32: 73)

[27] Li P J, Ye Y C, He L J.  Chin Sci Bull, 2008; 53: 1345

     (李培杰, 叶益聪, 何良菊. 科学通报, 2008; 53: 1345)

[28] Gao Y J, Zhong X P, Liu H, Wu W M.  Guangxi Sci, 2003; 10: 32

     (高英俊, 钟夏平, 刘慧, 吴伟明. 广西科学, 2003; 10: 32)

[29] Liu Z L, Li Z L, Liu W D.  Electron Structure of the Interface and Interfacial Properties. Beijing: Science Press, 2002: 7

     (刘志林, 李志林, 刘伟东. 界面电子结构与界面性能. 北京: 科学出版社, 2002: 7)

[30] Zhang R L.  Acta Sci Nat Univ Jilinensis, 1984; 3: 74

     (张瑞林. 吉林大学自然科学学报, 1984; 3: 74)

[31] Zhang R L.  The Empirical Electron Theory of Solids and Molecules.Jilin: Jilin Science and Technology Press, 1993: 268

     (张瑞林. 固体与分子经验电子理论. 吉林: 吉林科技出版社, 1993: 268)

[32] Liu Z L.  Valence Electron Structure and Composition Design of Alloy. Jilin: Jilin Science and Technology Press, 1990: 1

     (刘志林. 合金价电子结构与成分设计. 吉林: 吉林科学技术出版社, 1990: 1)

[33] Peng K, Yi M Z, Ran L P.  Acta Metall Sin, 2006; 42: 1125

     (彭可, 易茂中, 冉丽萍, 金属学报, 2006; 42: 1125)

[34] Nes E.  Acta Metall, 1972; 20: 499

[35] Ryun N.  Acta Metall, 1969: 17: 269

[36] Xu J H, Freeman A J.  Phys Rev, 1990; 41B: 12553

[37] Nicholson D M, Schneibel J H, Shelton W A.  Mater Res Soc,1991; 186: 229

[38] Emmauel C, Sanchez J M.  Phys Rev, 2002; 65B: 094105

[39] Hu G X, Cai X, Rong Y H.  Fundamentals of Materials Science.2nd Ed., Shanghai: Shanghai Jiao Tong University Press, 2003: 359

     (胡赓祥, 蔡, 戎咏华.材料科学基础. 第二版, 上海: 上海交通大学出版社, 2003: 359)

[40] Asboll K, Ryum N.  Inst Met, 1973; 101: 14

[41] Knipling K E, Dunand D C, Seidman D N.  Acta Mater, 2008; 56: 114
 
Outlines

/

〈 〉