ELECTROCHEMICAL STUDY ON CORROSION BEHAVIORS OF MILD STEEL IN A SIMULATED TIDAL ZONE

  • MU Xin ,
  • WEI Ji ,
  • DONG Jun-Hua ,
  • KE Wei
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Science,Shenyang 110016\par

Received date: 2011-10-25

  Revised date: 2011-12-27

  Online published: 2012-04-11

Abstract

The environment of the tidal zone is very complex. And the dry-wet alternation and interaction of sea erosion leads to serious corrosion of metal materials, making it difficult to adopt protective measures. Therefore, it is of great significance to study the corrosion and protection of metal materials in the tidal zone. Corrosion weight loss results showed that the corrosion behaviors of metal in different regions of tidal zone were altered, but the corrosion mechanism of metal materials in the tidal zone is not obvious. In order to study the corrosion mechanism of tidal corrosion, without considering the seawater splashing effect, a corrosion experimental trough was designed to simulation the tidal zone and immersion zone, and the corrosion behaviors of Q235B mild steel (designated) in it were monitored in situ by the potentiostat and electrochemical workstation. The results showed that the corrosion behaviors of Q235B steel at diverse positions are not the same. The corrosion rate of Q235B steel in the mid tide zone and low tide zone is higher than the highest tide zone and immersion zone. In a tidal range fluctuation cycle, the open-circuit potential variation law of the Q235B steel is related with the dry/wet state of the metal surface and the cathode/anode reactions. In the long term tidal corrosion process, the open-circuit potential variation of Q235B steel is related with the thickness of the rust layer.

Cite this article

MU Xin , WEI Ji , DONG Jun-Hua , KE Wei . ELECTROCHEMICAL STUDY ON CORROSION BEHAVIORS OF MILD STEEL IN A SIMULATED TIDAL ZONE[J]. Acta Metall Sin, 2012 , 48(4) : 420 -426 . DOI: 10.3724/SP.J.1037.2011.00666

References

[1] Xia L T, Huang G Q.  China Foundry Machine Technol,2002; (6): 1

    (夏兰廷, 黄桂桥. 中国铸造装备与技术, 2002; (6): 1)

[2] Jeffrey R, Melchers R E.  Corrosion, 2009; 65: 695

[3] Jeffrey R, Melchers R E.  Corrosion, 2007; 63: 872

[4] Al-Fozan S A, Malik A U.  Desalination, 2008; 228: 61

[5] LaQue F L.  Proc ASTM Corrosion Testing, PA: ASTM International, 1951: 495

[6] Larrabee C A.  Corrosion, 1958; 14: 501t

[7] Southwell C R, Bultman J D, Hummer C W.  Seawater Corrosion Handbook,NJ: Noyes Data Corp., 1979: 1

[8] Takamara A, Arakawa K, Fujiwara F, Hirose H. Trans. Iron Steel Inst Jpn, 1971; 11: 299

[9] Farro N W, Veleva L, Aguilar P.  215th ECS Meeting, 2009: 1

[10] Huang G Q.  Corros Prot, 2000; 21(1): 8

     (黄桂桥. 腐蚀与防护, 2000; 21(1): 8)

[11] Lou Y N, Song S Z, Jin W X, Yin L H.  J Chem Ind Eng,2008; 59: 2864

     (雒娅楠, 宋诗哲, 金威贤, 尹立辉. 化工学报, 2008; 59: 2864)

[12] Lou Y N.  PhD Thesis, Tian Jing University, 2007

     (雒娅楠. 天津大学博士论文, 2007)

[13] Gao Z P, Yang F Y, Zhang J L, Hou B R.  Chin Pat, 2252989, 1997

     (高振泮, 杨芳英, 张经磊, 侯宝荣. 中国专利, 2252989, 1997)

[14] Hou B R.  Marine Corrosion and Protection. Beijing: Science Press,1997: 59

     (侯宝荣. 海洋腐蚀与防护. 北京: 科学出版社, 1997: 59)

[15] Wang S T, Gao K W.  Int J Mineral Metall Mater, 2009; 16: 58

[16] Matsushima R, translated by Jing Y K.  Low-alloy Corrosion Resistant Steel Development and Research. Beijing: Metallurgical Industry Press, 2004: 230

     (松岛岩著, 靳裕康译, 低合金耐蚀钢开发、发展及研究. 北京:冶金工业出版社, 2004: 230)

[17] Moller H, Boshoff E T, Froneman H.  J S Afr Inst Min Metall,2006; 106: 585

[18] Yamashita M, Miyuki H, Matsuda Y, Nagano H, Misawa T. Corros Sci, 1994; 36: 283

[19] Hou B R, Zhang J L.  Br Corros J, 2001; 36: 310

[20] Hao L, Zhang S X, Dong J H, Ke W.  Corros Sci,2012; 54: 241

[21] Chen X H, Dong J H, Han E H, Ke W.  Mater Prot,2007; 40(10): 19

     (陈新华, 董俊华, 韩恩厚, 柯伟. 材料保护, 2007; 40(10): 19)

[22] Fu X X.  PhD Thesis, Institute of Metal Research Chinese Academy of Sciences, Shenyang, 2011

     (傅欣欣, 中国科学院金属研究所博士论文, 沈阳, 2011)
Outlines

/

〈 〉