Abstract

DLC films with dispersed high crystallinity CrN nanoparticles were prepared by high power pulsed magnetron discharge plasma ion implantation & deposition (HPPMS-PIID) combined with DC magnetron sputtering (DCMS). The surface morphology, structure and properties of CrN--DLC films with the different currents of C target were studied. The results show that the C content increases as the raise of the current of the C target and clear characteristics of DLC films are found at a higher C content. CrN doped in DLC exists as nanoparticles with highly 200 preferred orientation, and the smallest size of the CrN grains is 42.39 nm. The C1s peak primarily consists of the three peaks that correspond to C-sp2, C-sp3 and CN-sp3, and the ratio of total sp3 to sp2 is 44.8%. Excellent adhesion between film and substrate with critical load of 66.8 N and high nanohardness up to 24.3 GPa are achieved due to highly energetic ion bombardment and implantation in HPPMS-PIID.

Cite this article

WU Zhong-Zhen , TIAN Xiu-Bei , CHENG Sai-Ta , GONG Chun-Zhi , YANG Shi-Qi . MICROSTRUCTURE AND MECHANICAL PROPERTIES OF DLC FILMS DOPED WITH HIGH CRYSTALLINITY CrN NANOPARTICLES[J]. Acta Metall Sin, 2012 , 48(3) : 283 -288 . DOI: 10.3724/SP.J.1037.2011.00512

References

[1] Liang F, Yan X J. Acta Phys Sin, 1999; 48: 1095

(梁风, 严学俭. 物理学报, 1999; 48: 1095)

[2] Grill A. Diamond Relat Mater, 1999; 8: 428

[3] Chen G H, Yan S G, Zhang F Q. Acta Phys Sin, 1992; 41: 500

(陈光华, 阎少光, 张仿清. 物理学报, 1992; 41: 500)

[4] Schwarz C, Heeg J, Rosenberg M, Wienecke M. Diamond Relat Mater, 2008; 17: 1685

[5] Takeno T, Hoshi Y, Miki H, Takagi T. Diamond Relat Mater, 2008; 17: 1669

[6] Gu K M, Tang J N, Li J Q, Yang Q P. J Shenzhen Univ Sci Eng, 2007; 24: 159

(谷坤明, 汤皎宁, 李均钦, 杨钦鹏. 深圳大学学报理工版, 2007; 24: 159)

[7] Nie C Y, Zhang B Y, Xie H M. Acta Metall Sin, 2007; 43: 1207

(聂朝胤, 张碧云, 谢红梅. 金属学报, 2007; 43: 1207)

[8] Veprek S, Argon A S. Surf Coat Technol, 2001; 146–147: 175

[9] Mourae Silva C W, Branco J R T, Cavaleiro A. Thin Solid Films, 2006; 515: 1063

[10] Baba K, Hatada R, Tanaka Y. Surf Coat Technol, 2007; 19–20: 8362

[11] Tian X B, Wu Z Z, Gong C Z, Yang S Q. Chin Pat, 201010213894.4, 2010

(田修波, 吴忠振, 巩春志, 杨士勤. 中国专利, 201010213894.4, 2010)

[12] Kouznetsov V, Mac´ak K, Schneider J M, Helmersson U, Petrov I. Surf Coat Technol, 1999; 122: 290

[13] Helmersson U, Lattemann M, Bohlmark J, Ehiasarian A P, Gudmundsson J T. Thin Solid Films, 2006; 513: 1

[14] Wu Z Z, Tian X B, Shi J W, Yang S Q, Chu P K. Rev Sci Inst, 2011; 82: 033511

[15] Wu Z Z, Tian X B, Wang Z M, Gong C Z, Yang S Q. Chin J Vac Sci Technol, 2011; 31: 1

(吴忠振, 田修波, 王泽明, 巩春志, 杨士勤. 真空科学与技术学报, 2011; 31: 1)

[16] Li G, Xia L F, Ma X X, Sun Y, Zhan Z J. Acta Metall Sin (Eng Lett), 1999; 12: 551

[17] Ji H B, Xia L F, Ma X X, Sun Y, Sun M R. Acta Metall Sin (Eng Lett), 2000; 13: 967

[18] Wu Z Z. Master Dissertation, Harbin Institute of technology, 2008

(吴忠振. 哈尔滨工业大学硕士学位论文, 2008)

[19] Tian X B, Wu Z Z, Shi J W, Li X P, Gong C Z, Yang S Q. Vacuum, 2010; 47: 44

(田修波, 吴忠振, 石经伟, 李希平, 巩春志, 杨士勤. 真空, 2010; 47: 44)

[20] Anders A. Surf Coat Technol, 1997; 93: 158

[21] Martin P J, Bendavid A, Cairney J M, Hoffman M. Surf Coat Technol, 2005; 200: 2228

[22] Ma D Y, Ma S L, Xu K W. Acta Metall Sin, 2004; 40: 1037

(马大衍, 马胜利, 徐可为. 金属学报, 2004; 40: 1037)

[23] Guo Y, Xu B, Wu G Z, Ma S L, Xu K W. Acta Metall Sin, 2007; 43: 159

(郭岩, 徐 彬, 吴贵智, 马胜利, 徐可为. 金属学报, 2007; 43: 159)

[24] Alami J, Sarakinos K, Uslu F, Wuttig M. J Phys D: Appl Phys, 2009; 42: 015304

[25] Vyas A, Shen Y G, Zhou Z F, Li K Y. Compos Sci Technol, 2008; 68: 2922

[26] Shi Y, Long S, Liang F. Appl Surf Sci, 2008; 254: 5861

[27] Yang Y Y, Peng Z J, Fu Z Q, Wu S D, Chen X C, Wang C B. Acta Metall Sin, 2010; 46: 34

(杨义勇, 彭志坚, 付志强, 邬苏东, 陈新春, 王成彪. 金属学报. 2010; 46: 34)

[28] Yang W J, Choa Y–H, Sekino T, Shim K B, Niihara K, Auh K H. Thin Solid Films, 2003; 434: 49

[29] Jiang B L, Hu P F, Li H T. Trans Mater Heat Treat, 2010; 31: 134

(蒋百灵, 胡鹏飞, 李洪涛. 材料热处理学报. 2010; 31: 134)

[30] Niu S C, Yu Z M, Dai M J, Lin S S, Hou H J, Li H W. China Surf Eng, 2007; 20: 34

(牛仕超, 余志明, 代明江, 林松盛, 候惠君, 李洪武. 中国表面工程. 2007; 20: 34)

[31] Veprek S, Niederhofer A, Moto K, Bolom T, Mannling H–D, Nesladek P, Dollinger G, Bergmaier A. Surf Coat Technol, 2000; 133–134: 152

[32] Robertson J. Mater Sci Eng, 2002; R37: 129
Outlines

/

〈 〉