An 18Ni (C–250) maraging steel was successfully processed by equal–channel angular pressing (ECAP) for a single pass at room temperature. After ECAP deformation, the peak aging time was cut obviously and the peak strength of the steel was enhanced about 100 MPa. Microstructural observations showed that the martensite laths of 18Ni maraging steel were elongated to more narrow bands with a width of 100—200 nm after ECAP deformation, and the width of martensite lath was not affected by the subsequent aging treatment. ECAP deformation has significant influence on the size of rod–shaped δ–Ni3Mo precipitates. It was observed that the widths (diameters) of precipitates in specimens under treatments of solution+480℃, 4 h, solution+ECAP+480℃, 4 h and solution+ECAP+460 ℃, 4 h are 4.92, 12.33 and 3.54 nm, respectively. Additionally, a decomposition of the δ–Ni3Mo precipitates was accelerated after the peak aging time, resulting in a decrease in the strength.
YANG Mu-Xin
,
YANG Gang
,
LIU Zheng-Dong
,
YU Chang
,
HU Tiao
,
HUANG Chong-Xiang
. EFFECT OF EQUAL–CHANNEL ANGULAR PRESSING ON THE MICROSTRUCTURES AND TENSILE PROPERTIES OF 18Ni(C–250) MARAGING STEEL[J]. Acta Metall Sin, 2012
, 48(2)
: 164
-169
.
DOI: 10.3724/SP.J.1037.2011.00420
[1] ASM Handbook Committee. ASM Handbook. Volume 1, 10th Ed., Ohio: ASM International, 1990: 739
[2] Li X D. PhD Thesis, Harbin Institute of Technology, 1993
(李晓东. 哈尔滨工业大学博士学位论文, 1993)
[3] Sha W, Guo Z. Maraging Steels: Modelling of Microstructure, Properties and Applications. Oxford: Woodhead Publishing, 2009: 3
[4] Roberson J A, Adair A M. Trans TMS–AIME, 1969; 245: 1937
[5] Baker A J, Swann P R. Trans ASM, 1964; 57: 1008
[6] Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881
[7] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S X. Acta Mater, 2006; 54: 655
[8] Huang C X, Yang G, Wang C, Zhang Z F, Wu S D. Metall Mater Trans, 2011; 42A: 2061
[9] Yang G, Huang C X, Wang C, Zhang L Y, Hu C, Zhang Z F, Wu S D. Mater Sci Eng, 2009; A515: 199
[10] Huang C X, Yang G, Gao Y L, Wu S D, Zhang Z F. Mater Sci Eng, 2008; A485: 643
[11] He Y, Yang K, Kong F Y, Qu W S, Su G Y. Acta Metall Sin, 2002; 38: 278
(何毅, 杨柯, 孔凡亚, 曲文生, 苏国跃. 金属学报, 2002; 38: 278)
[12] Yang G, Yin F. Mater Sci Forum, 2010; 667–669: 879
[13] Mobarake M I, Nili–Ahmadabadia M, Poorganji B, Fatehi A, Shirazi H, Furuhara T, Parsaa H, Nejad S H. Mater Sci Eng, 2008; A491: 172
[14] Yang M X, Yang G, Liu Z D, Wang C, Huang C X. Mater Sci Forum, 2010; 667–669: 421
[15] Iwahashi Y, Wang J, Horita Z, Nemoto M, Langdon T G. Scr Mater, 1996; 35: 143
[16] Marder J M, Marder A R. Trans ASM, 1969; 62: 1
[17] Tsai C K, Chu C, He C Z, Shen H W, Luo L K, Song W S, Yu W L. Acta Metall Sin, 1977; 13: 289
(蔡其巩, 朱静, 何崇智, 申辉旺, 罗力更, 宋为顺, 于维乐. 金属学报, 1977; 13: 289)
[18] Ye H Q, Zou S B. Acta Metall Sin, 1979; 15: 69
(叶恒强, 邹三本. 金属学报, 1979; 15: 69)
[19] Tsai C K, Zhu Q, He C Z. Acta Phys Sin, 1974; 23: 178
(蔡其巩, 朱静, 何崇智. 物理学报, 1974; 23: 178)
[20] Tewari R, Mazumder S, Batra I S, Dey G K, Banerjee S. Acta Mater, 2000; 48: 1187
[21] Yin Z D, Li X D, Li H B, Lai Z H. Acta Metall Sin, 1995; 31: 7
(尹钟大, 李晓东, 李海滨, 来忠红. 金属学报, 1995; 31: 7)
[22] Yong Q L, MaMT. Micro–alloyed Steel—Physics and Mechanics Metallurgy. Beijing: Metallurgy Industry Press, 1989: 315
(雍岐龙, 马鸣图. 微合金钢-物理和力学冶金. 北京: 冶金工业出版社, 1989: 315)
[23] Martin J W, Doherty R D. Translated by Li X L. Stability of Microstructure in Metallic Systems. Beijing: Science Press, 1984: 55
(Martin J W, Doherty R D. 李新立 译. 金属系中显微结构的稳定性. 北京: 科学出版社, 1984: 55)
[24] He Y, Liu K, Yang K. Acta Metall Sin, 2003; 39: 381
(何毅, 刘 凯, 杨柯. 金属学报, 2003; 39: 381)