EFFECTS OF HCO3- AND SO42- ON THE PITTING CORROSION BEHAVIOR OF Cu

  • YU Zhang-Gang ,
  • DONG Jun-Hua ,
  • KE Wei ,
  • CHEN Nan
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-08-24

  Revised date: 2011-12-07

  Online published: 2012-01-11

Supported by

Supported by National Natural Science Foundation of China (No.51071160)

Abstract

As a kind of clean, efficient and relatively safe energy, nuclear energy has been widely used around the world. The high-level radioactive waste generated in the nuclear has also become a major risk, so the disposal safety of high-level radioactive waste will be especially important. The strategy for disposal of high-level radioactive waste in China is to enclose the spent nuclear fuel in sealed metal canisters which are embedded in bentonite clay hundreds meters down in the bed-rock. The choice of container material depends largely on the redox conditions and the aqueous environment of the repository. One of the choices for the fabrication of waste canisters is Cu, because it is thermodynamically stable under the saline, anoxic conditions over the large majority of the container lifetime. For this advantage, some other countries (Canada, Sweden) have selected Cu as the material of nuclear waste container. However, in the early aerobic phase of the geological disposal the corrosion of Cu could take place, and the corrosion behavior of Cu would be influenced by the complex chemical conditions of groundwater markedly. Pitting corrosion of Cu often take place in power plants or air--conditioning condensate water. The corrosion environment usually contains HCO3-, SO42- and Cl- ions. In the early stage of geological disposal, if the aerobic water with HCO3-, SO42-and Cl- immersion repository, the pitting corrosion of Cu may occur. The content of HCO3- and SO42- in the water chemistry environment, as well as the synergy between them, could affect the behavior of pitting seriously. In this work, the cycle polarization behavior and surface morphology of pitting has been investigated in HCO3- and SO42- mixed solution, respectively by electrochemical cyclic polarization test and SEM. The results showed that the pitting corrosion behavior of Cu can be divided into the type of active dissolve and the type of film rupture; SO42- could increase Cu pitting sensitivity in both of the two types pitting corrosion. Due to synergies with the SO42-, HCO3- could increase the pitting susceptibility first and then reduce the law. In passive film rupture pitting system, SO42- could improve the ability of induce pitting; HCO3- could reduce the ability of induce pitting. There is no significant impact on pitting self--healing capacity by the two ions.

Cite this article

YU Zhang-Gang , DONG Jun-Hua , KE Wei , CHEN Nan . EFFECTS OF HCO3- AND SO42- ON THE PITTING CORROSION BEHAVIOR OF Cu[J]. Acta Metall Sin, 2012 , 48(1) : 85 -93 . DOI: 10.3724/SP.J.1037.2011.00537

References

[1] Wang C G, Dong J H, Ke W, Chen N. Acta Metall Sin, 2011; 47: 354

(王长罡, 董俊华, 柯伟, 陈 楠. 金属学报, 2011; 47: 354)

[2] Cheng Y L, Zhang J Q. Acta Metall Sin, 2002; 38: 74

(程英亮, 张鉴清. 金属学报, 2002; 38: 74)

[3] Liu G Q, Zhu Z Y, Ke W. Acta Metall Sin, 2001; 37: 272

(刘国强, 朱自勇, 柯 伟. 金属学报, 2001; 37: 272)

[4] Zhou X Y, Ke W, Zang Q S. Acta Metall Sin, 1990; 26: 110

(周向阳, 柯伟, 臧启山. 金属学报, 1990; 26: 110)

[5] Yan Z, Xian A P. Acta Metall Sin, 2011; 47: 1327

(颜 忠, 冼爱平. 金属学报, 2011; 47: 1327)

[6] Cao G L, Li G M, Chen S, Chang W S, Chen X Q. Acta Metall Sin, 2011; 47: 145

(曹国良, 李国明, 陈 珊, 常万顺, 陈学群. 金属学报, 2011; 47: 145)

[7] Darren A L, Mallikarjuna N N. Corros Sci, 2010; 52: 1927

[8] Fujii T, Kodama T, Baba H. Corros Sci, 1984; 24: 901

[9] Drogowska M, Brossard L, M´enard H. Surf Coat Technol, 1988; 34: 383

[10] Drogowska M, Brossard L, Menard H. J Electrochem Soc, 1992; 139: 39

[11] Duthil J P, Mankowski G, Giusti A. Corros Sci, 1996; 38: 1839

[12] Reda M R, Alhajji J N. Corrosion, 1996; 3: 232

[13] Cantor A F, Park J K, Vaiyavatjamai P. J Am Water Works Association, 2003; 95(5): 112

[14] Pourbaix M. J Electrochem Soc, 1976; 123: C25

[15] Mankowski G, Duthil J P, Giusti A. Corros Sci, 1997; 39: 27

[16] Milosev I, Metikos–Hukovic M, Drogowska M, Menard H, Brassard L. J Electrochem Soc, 1992; 139: 2409

[17] Cong H, Michels H T, Scully J R. J Electrochem Soc, 2009; 156: C16

[18] Cong H, Scully J R. J Electrochem Soc, 2010; 157: C200

[19] Cong H, Scully J R. J Electrochem Soc, 2010; 157: C36

[20] Christy A G, Lowe A, Otieno–Alego V, Stoll M, Webster R D. J Appl Electrochem, 2004; 34: 225

[21] Abd El Meguid E A, Awad N K. Corros Sci, 2009; 51: 1134

[22] Cao C N. Corrosion Electrochemical Theory. 2nd Ed., Beijing: Chemical Industry Press, 2004: 287

(曹楚南. 腐蚀电化学原理. 第二版, 北京: 化学工业出版社, 2004: 287)
Outlines

/