EFFECT OF LONG-TERM AGING ON DYNAMIC TENSILE DEFORMATION BEHAVIOR OF GH4169 ALLOY

  • LIU Yang ,
  • YU Lei ,
  • HE Sai-Shi ,
  • FENG Fei ,
  • ZHANG Bei-Jiang ,
  • DIAO Guang-Pu
Expand
  • 1) Key Lab for Anisotropy and Texture of Materials, Northeastern University, Shenyang 110819
    2) Department of High-temperature Materials, Central Iron and Steel Research Institute, Beijing 100081

Received date: 2011-07-11

  Revised date: 2011-11-22

  Online published: 2012-01-11

Supported by

Supported by National Basic Research Program of China (No.2010CB631203), National Natural Science Foundation of China (No. 51001021) and Doctoral Fund of Ministry of Education of China (Nos.20100042120008 and 20100042110006)

Abstract

In traditional aeroengine manufacturing industry, the variation and mechanism of the mechanical property of superalloy used for rotating parts under the actual dynamic load is not given full considerations during its structure design. The mechanical property and deformation behavior of the alloys under the dynamic load have significant difference compared with that under the static load, and therefore the study on the deformation behavior of the alloy under the dynamic load is important for the safety of rotating parts used under the severe service conditions. The effect of microstructural changes of long-term aging GH4169 alloy on the mechanical properties through tensile testing at strain rates ranging from 101 to 103 s-1 was examined in this paper. The tensile deformation behavior of the alloy and the mechanisms were also discussed. The results showed that the strength of the alloy depends strongly on the aging time, the fracture elongation decreases with the increasing aging time and remains unchanged when aged for 500 h when tensile tested at the strain rates ranging from 101 to 103 s-1. And when the strain rate is high up to 103 s-1, the elongation depends strongly on the aging time and the degradation of ductility by the long-term aging happens ahead of time, but the aging time has no obvious effect on the strength of the alloy. Through tensile testing at the strain rate of 103 s-1, it is too late to release the blocked dislocation motion in the way of dislocation decomposition or climb in the alloy. And there is no peaking size effect of the strengthening phase in the alloy with the aging time ranging from 0 to 1000 h and there is no obvious effect of the aging time on the strength of the alloy. The ability of accommodation of plastic deformation by grain boundaries reduces under the dynamic loads due to the existence of precipitate free zones around δ phase at the grain boundary in the alloy by long-term aging, and thus the ductility of the alloy by aging for a shorter time decreases rapidly when tensile tested at the strain rate of 103 s-1.

Cite this article

LIU Yang , YU Lei , HE Sai-Shi , FENG Fei , ZHANG Bei-Jiang , DIAO Guang-Pu . EFFECT OF LONG-TERM AGING ON DYNAMIC TENSILE DEFORMATION BEHAVIOR OF GH4169 ALLOY[J]. Acta Metall Sin, 2012 , 48(1) : 49 -55 . DOI: 10.3724/SP.J.1037.2011.00435

References

[1] Soo S L, Hood R, Aspinwall D K, Voice W E, Sage C. CIRP Ann–Manuf Technol, 2011; 60: 89

[2] Fang N, Wu Q. J Mater Process Technol, 2009; 209: 4385

[3] Sharghi–Moshtagh R, Asgari S. J Mater Process Technol, 2004; 147: 343

[4] Graverend J B, Cormier J, Caron P, Kruch S, Gallerneau F, Mendez J. Mater Sci Eng, 2011; A528: 2620

[5] Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Acta Metall Sin, 2010; 46: 213

(秦学智, 郭建亭, 袁超, 侯介山, 周兰章, 叶恒强. 金属学报, 2010; 46: 213)

[6] Li G H, Wang M J, Kang R K. Mater Sci Technol, 2010; 18: 824

(李国和, 王敏杰, 康仁科. 材料科学与工艺, 2010; 18: 824)

[7] Zan X, He Y H, Wang Y, Xia Y M. Trans Nonferrous Met Soc, 2011; 21: 45

[8] Lee W S, Lin C F. Mater Sci Eng, 1998; A241: 48

[9] Smerd R, Winkler S, Salisbury C, Worswick M, Lloyd D, Finn M. Int J Impact Eng, 2005; 32: 541

[10] Ishikawa K, Watanabe H, Mukai T. Mater Lett, 2005; 59: 1511

[11] Odeshi A G, Al–ameeri S, Bassim M N. J Mater Process Technol, 2005; 162–163: 385

[12] Gong X, Fan J L, Huang B Y, Tian J M. Mater Sci Eng, 2010; A527: 7565

[13] Lu X D, Du J H, Deng Q, Qu J L, Zhuang J Y, Zhong Z Y. Mater Sci Eng, 2007; A452–453: 584

[14] Hajmrle K, Aangers R, Dufour G. Metall Trans, 1982; 13A: 5

[15] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289

(谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)

[16] Wang L. Mechanical Properties of Materials. Shenyang: Northeastern University Press, 2007: 42

(王磊. 材料的力学性能. 沈阳: 东北大学出版社, 2007: 42)

[17] Walgraef D. Mater Sci Eng, 2010; A322: 167

[18] Ning Y Q, Yao Z K, Xie X H, Guo H Z, Tan L J, Tao Y. Acta Metall Sin, 2010; 46: 324

(宁永权, 姚泽坤, 谢兴华, 郭鸿镇, 谭立军, 陶宇. 金属学报, 2010; 46: 324)

[19] Zhang J H, Jin T, Xu Y B, Hu Z Q, Wu X. J Mater Sci Technol, 2002; 18: 159

[20] Deng Z Y, Huang B Y, He Y H, Sun J. Rare Met Mater Eng, 1999; 28: 228

(邓忠勇, 黄伯云, 孙跃辉, 孙坚. 稀有金属材料与工程, 1999; 28: 228)

[21] Meyers M A, translated by Zhang Q M, Liu Y, Huang F L, Lu Z J. Dynamic Behavior of Materials. Beijing: National Defense Industry Press, 2006: 225

(Meyers M A著; 张庆明, 刘彦, 黄风雷, 吕中杰 译. 材料的动力学行为. 北京: 国防工业出版社, 2006: 225)

[22] Xie X S, Dong J X, Zhang M C. Mater Sci Forum, 2007; 539–543: 262

[23] Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H, Masaki S. Metall Mater Trans, 2002; 33A: 3741

[24] Lours P, Coujou A, Coulomb P. Acta Metall Mater, 1991; 39: 1787

[25] Wang K, Li M Q, Luo J, Li C. Mater Sci Eng, 2011; A528: 4723

[26] Wang Y W, Yang L Y, You W, Bai B Z. Mater Sci Forum, 2005; 475–479: 3003
Outlines

/

〈 〉