论文

EFFECT OF CARBON NANOTUBES ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF W

  • TAN Jun ,
  • ZHOU Zhang-Jian ,
  • LIU Ya-Qi ,
  • QUE Dan-Dan ,
  • ZHONG Ming ,
  • GE Chang-Quan
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-06-28

  Revised date: 2011-10-26

  Online published: 2011-12-11

Supported by

Supported by National Natural Science Foundation of China (No.50634060) and National Magnetic Confinement Fusion Program (No.2010GB109000)

Abstract

W–based composites were fabricated by spark plasma sintering (SPS) usingWpowders and carbon nanotubes (CNTs) as raw materials. The effect of the CNTs on the microstructure and room temperature mechanical properties of W was investigated. The results show that the W2C was formed through the reaction of CNTs and W during the SPS process. The formation of the W2C activated the sintering of W and enhanced the densification of W. On the other hand, the in situ formation of W2C decreased the driving force of sintering and consequently inhibited the grain growth of W at high temperature. The grain size, relative density, bending strength and the Vicker’s hardness of W composites were 4 μm, 99%, 1353.9 MPa and 488.4 HV respectively when the content of CNTs was 0.5%.

Cite this article

TAN Jun , ZHOU Zhang-Jian , LIU Ya-Qi , QUE Dan-Dan , ZHONG Ming , GE Chang-Quan . EFFECT OF CARBON NANOTUBES ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF W[J]. Acta Metall Sin, 2011 , 47(12) : 1555 -1560 . DOI: 10.3724/SP.J.1037.2011.00398

References

[1] Lassner E, Schubert W D. Tungsten–Properties, Chemistry, Technology of the Element, Alloys and Chemical Compounds. New York: Kluwer–Academic/Plenum Publishers,

1998: 7

[2] Smid I, Akiba M, Vieider G, Plochl L. J Nucl Mater, 1998; 258–263: 160

[3] Ryu H J, Hong S H. Mater Sci Eng, 2003; A363: 179

[4] Zhang H, Chen X F, Yang Z M, Ding B J. Mater Lett, 1999; 38: 401

[5] Kim Y, Lee K H, Kim E P, Cheong D I, Hong S H. Int J Refract Met Hard Mater, 2009; 27: 842

[6] Rieth M, Daerner B. J Nucl Mater, 2005; 342: 20

[7] Veleva L, Oksiuta Z, Vogtb U, Baluc N. Fus Eng Des, 2009; 84: 1920

[8] Kurishita H, Amano Y, Kobayashi S, Nakai K, Arakawa H, Hiraoka Y, Tajida T, Takebe K, Matsui H. J Nucl Mater, 2007; 367–370: 1453

[9] Kurishita H, Matsuo S, Arakawa H, Narui M, Yamazaki M, Sakamoto T, Kobayashi S, Nakai K, Takida T, Takebe K, Kawai M, Yoshida N. J Nucl Mater, 2009; 386–388: 579

[10] Zhang T Q, Wang Y J, Zhou Y, Lei T Q Song G M. Int J Refract Met Hard Mater, 2007; 25: 445

[11] Rea K E, Viswanathan V, Kruize A , Hosson J Th M De, O’Dell S, Mckechnie T, Rajagopalan S, Vaidyanathan R, Seal S. Mater Sci Eng, 2008; A477: 350

[12] Kinoshitan S, Saito T, Kobayashi M. J Jpn Soc Powder Powder Metall, 2001; 48(1): 51

[13] Oliveira F A C, Granier B, Badie JM, Fernandes J C, Rosa L G, Shohoji N. Int J Refract Met Hard Mater, 2007; 25: 351

[14] Oliveira F A C, Fernandes J C, Badie JM, Granier B, Rosa L G, Shohoji N. Int J Refract Met Hard Mater, 2007; 25: 101

[15] Zhang J, Li D Y, Zhao L Z. Mac Des Manuf, 2011; 2: 266

(张坚, 李德英, 赵龙志. 机械设计与制造, 2011; 2: 266)

[16] Su W, Li W Z. Foundry Technol, 2008; 29: 29

(孙巍, 李文珍. 铸造技术, 2008; 29: 29)

[17] Li S N, Song S Z, Yu T Q. J Wuhan Univ Technol, 2003; 25: 1

(李四年, 宋守志, 余天庆. 武汉理工大学学报, 2003; 25: 1)

[18] Shen J, Sun J F, Zhang F M. Mater Sci Technol, 2006; 14: 165

(沈军, 孙剑飞, 张法明. 材料科学与工艺, 2006; 14: 165)

[19] Zhang L, Schubert W D, Huang B Y. Cement Carbide, 2003; 20: 193

(张立, Schubert W D, 黄伯云. 硬质合金, 2003; 20: 193)

[20] Shankar N, Yu M F, Vanka S P, Glumac Nick G. Mater Lett, 2006; 60: 771

[21] Zhong Z, Liu B, Sun L, Lin J, Tan K L. Chem Phys Lett, 2002; 362: 135

[22] Kreupl F, Guesberg A P, Duesberg G S, Steinh¨ogl W, Liebau M, Unger E, H¨onlein W. Microelectron Eng, 2002; 64: 399

[23] Pei Y B, Guo S J, Meng F, Yang X. Mater Sci Eng Powder Metall, 2005; 10: 160

(裴燕斌, 果世驹, 孟飞, 杨霞. 粉末冶金材料科学与工程, 2005; 10: 160)

[24] Krause B, Mende M, P¨otschke P, Petzold G. Carbon, 2010; 48: 2746

[25] Xi X L, Guo Y Q, Nie Z R, Yang J C, Zuo T Y. J Beijing Univ Technol, 2004; 30: 59

(席晓丽, 郭艳群, 聂祚仁, 杨建参, 左铁镛. 北京工业大学学报, 2004; 30: 59)

[26] Liang Y J, Che Y C. Handbook of Thermodynamic Data for Inorganic Matter. Shenyang: Northeastern University Press, 1993: 12

(梁英教, 车荫昌. 无机物热力学数据手册. 沈阳: 东北大学出版社, 1993: 12)
Outlines

/

〈 〉