论文

EFFECT OF APPLIED POTENTIALS ON STRESS CORROSION CRACKING OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION

  • YU Zhang-Peng ,
  • DU Cui-Wei ,
  • LIU Zhi-Yong ,
  • LI Xiao-Gang
Expand
  • 1) Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083
    2) Key Lab of Corrosion, Erosion and Surface Technique of Beijing, Beijing 100083

Received date: 2011-01-19

  Revised date: 2011-07-25

  Online published: 2011-11-11

Supported by

Supported by National Natural Science Foundation of China (No.50901041) and the Fundamental Research Funds for the Central Universities (No.FRF-TP-09-029B)

Abstract

Stress corrosion cracking (SCC) of X80 pipeline steel in a simulated solution of the acidic soil environments in Yingtan China was studied by means of potentiodynamic polarization curves, slow strain rate test (SSRT) and corrosion morphologies characterized by SEM. The results show that X80 pipeline steel has high SCC susceptibility in the simulated solution and the failure mode is transgranular cracking. The SCC mechanism would vary with the applied cathodic potential. When the applied potential is positive to about -930 mV, the SCC behavior is controlled by the combined effect of anodic dissolution (AD) and hydrogen embrittlement (HE), i.e. the SCC mechanism is AD+HE. However, when the applied potentials are lower than -930 mV, such as -1000 and -1200 mV,  the process of hydrogen evolution plays the dominant role in SCC occurrence, meaning that the SCC mechanism is HE under such applied potentials. Moreover, SCC susceptibility increases with decreasing applied cathodic potential. Compared with X70 pipeline steel in acidic soil environments, HE plays a more important role in affecting SCC occurrence.

Cite this article

YU Zhang-Peng , DU Cui-Wei , LIU Zhi-Yong , LI Xiao-Gang . EFFECT OF APPLIED POTENTIALS ON STRESS CORROSION CRACKING OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION[J]. Acta Metall Sin, 2011 , 47(11) : 1434 -1439 . DOI: 10.3724/SP.J.1037.2011.00046

References

[1] Liu Z Y, Li X G, Du C W, Zhai G L, Cheng Y F. Corros Sci, 2008; 50: 2251

[2] Zhai G L, Liu Z Y, Du C W, Li X G, Wang L X. Corros Prot, 2009; 30: 149

(翟国丽, 刘智勇, 杜翠薇, 李晓刚, 王立贤. 腐蚀与防护, 2009; 30: 149)

[3] L¨u X Y, Wang Y, Li J C. Electr Weld Machine, 2009; 39(5): 121

(吕向阳, 王义, 李景昌. 电焊机, 2009; 39(5): 121)

[4] Liang P, Du C W, Li X G, Chen X, Zhang L. Int J Miner, Metall Mater, 2009; 16: 407

[5] Gu B, Luo J L, Mao X. Corrosion, 1999; 55: 96

[6] Gu B, Yu W Z, Luo J L,Mao X. Corrosion, 1999; 55: 312

[7] Wang B Y, Huo L X, Wang D P, Deng C Y. J Tianjin Univ, 2007; 40: 757

(王炳英, 霍立兴, 王东坡, 邓彩艳. 天津大学学报, 2007; 40: 757)

[8] Su D L, Feng Y, Chen J B. Mechanical Properties of Engineering Materials. Beijing: China Machine Press, 2005: 1

(束德林, 凤 仪, 陈九磅. 工程材料力学性能. 北京: 机械工业出版社, 2005: 1)

[9] Chu W Y, Qiao L J, Chen Q Z. Fault Rupture and the Environment. Beijing: Science Press, 2000: 109

(禇武扬, 乔利杰, 陈奇志. 断裂与环境断裂. 北京: 科学出版社, 2000: 109)

[10] Ogundele G I, White W E. Corrosion, 1986; 42: 71

[11] Zhang L F. J Iron Steel Res Int, 2006; 13(3): 01

[12] Garet M, Brass A M, Haut C, Solana F G. Corros Sci, 1998; 40: 1073

[13] Parkins R N. Corros Sci, 1980; 20: 147

[14] Liu Z Y, Li X G, Du C W, Zhai G C, Cheng Y F. Corros Sci, 2008; 50: 2251

[15] Cheng Y F, Niu L. Electrochem Commun, 2007; 9: 558

[16] Chen W, Fang K, Vokes E. Corrosion, 2002; 58: 267

[17] Liu Z Y, Zhai G L, Du C W, Li X G. Acta Metall Sin, 2008; 44: 209

(刘智勇, 翟国丽, 杜翠薇, 李晓刚. 金属学报, 2008; 44: 209)

[18] Liu Z Y, Li X G, Du C W, Lu L, Zhang Y R, Cheng Y F. Corros Sci, 2009; 51: 895
Outlines

/

〈 〉