论文

SIMULATION AND EXPERIMENTAL STUDY OF PREPARATION OF FUNCTIONALLY GRADIENT MATERIALS BY MIG WELDING UNDER MAGNETIC FIELD\par

  • ZHANG Hai-Ou ,
  • YU Tiao ,
  • YU Gui-Lan
Expand
  • 1) State Key Laboratory of Digital Manufacturing and Equipment Technology, School of Mechanical Engineering, Huazhong University of Science and Technology, Wuhan 430074
    2) State Key Laboratory of Plastic Forming Simulation and Die \& Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074

Received date: 2010-11-29

  Revised date: 2011-05-26

  Online published: 2011-09-11

Supported by

Supported by  National Natural Science Foundation of China (No.50875096)

Abstract

A preparation method of functionally gradient materials (FGM) by metal inert-gas (MIG) welding under magnetic field was proposed in this paper. Three dimensional finite element models of magnetic field, welding gun and metal specimen were built. Maxwell vortex field and instantaneous field were applied to simulate the preparation process with permanent magnetic field, alternating magnetic field and without magnetic field, and the simulation model was verified by the experiment. Simulation and experimental results show that in permanent magnetic field, the stirring of molten pool is weak, the FGM can not be prepared; under alternating magnetic field, the axial oscillating magnetic force and lateral extrusion magnetic force mix round the molten pool effectively, FGM can be prepared by MIG. Without magnetic field, the gradient of Al content in formed FGM is not obvious. Experimental results accord with simulation ones commendably.

Cite this article

ZHANG Hai-Ou , YU Tiao , YU Gui-Lan . SIMULATION AND EXPERIMENTAL STUDY OF PREPARATION OF FUNCTIONALLY GRADIENT MATERIALS BY MIG WELDING UNDER MAGNETIC FIELD\par[J]. Acta Metall Sin, 2011 , 47(9) : 1221 -1226 . DOI: 10.3724/SP.J.1037.2010.00640

References

[1] Ruan J Z, Sparks T E, Panackal A, Ard K E, Liou F W, Slattery K, Chou H N, Kinsella M. J Manuf Sci Eng Trans ASME, 2007; 129: 303

[2] Dwivedi R, Kovacevic R. Int J Machine Tool Manuf, 2006; 46: 1811

[3] Lin J, Zhao H Y, Cai Z P, Hang SW, Lu X M, Ni S F. J Tsinghua Univ (Sci Technol), 2007; 47: 161

(林健, 赵海燕, 蔡志鹏, 黄士卫, 陆向明, 倪淑凤.

清华大学学报(自然科学版), 2007; 47: 161)

[4] Miller P C. Tool Prod, 1990; 55: 100

[5] Tang F, Lu A L, Mei J F. J Mater Process Technol, 1998; 74: 255

[6] Lin J, Huang S W, Cai Z P, Zhao H Y, Lu A L. Chin J Mech Eng. 2006; 42: 208

(林健, 黄士卫, 蔡志鹏, 赵海燕, 鹿安理. 机械工程学报, 2006; 42: 208)

[7] Huang X Q, Cai Z P. Chin J Mech Eng, 2011; 47: 88

(黄欣泉, 蔡志鹏. 机械工程学报, 2011; 47: 88)

[8] Jiang H W, Li C F, Zhao Z H, Li Z, Yu H P. Mater Sci Technol, 2004; 12: 327

(江洪伟, 李春峰, 赵志衡, 李忠, 于海平. 材料科学与工艺, 2004; 12: 327)

[9] Licf, Zhao Z H. J Mater Process Technol, 2002; 123: 225

[10] Zhang H O, Wang G L, Wei Z C. Chin Pat, 200810197001.4, 2008

(张海鸥, 王桂兰, 韦忠朝. 中国专利, 200810197001.4, 2008)

[11] David W, James F. ISIJ Int, 1989; 29: 1016

[12] Wang H M, Chen G X, Ren Z M, Lei Z S, Li G R, Xia X J, Dai Q X. Foundry Technol, 2006; 27: 737

(王宏明, 陈国星, 任忠鸣, 雷作胜, 李桂荣, 夏小江, 戴起勋. 铸造技术, 2006; 27: 737)

[13] Liu D J. Shonghai Steel Iron Res, 1996; 4: 47

(刘大均. 上海钢研, 1996; 4: 47)

[14] Wang L, Felicelli S. Trans ASME J Manuf Sci Eng, 2007; 129: 1028
Outlines

/

〈 〉