论文

PREPARATION OF NANO-SIZED SiC REINFORCED NiTi SHAPE MEMORY COMPOSITES AND THEIR MECHANICAL PROPERTIES AND DAMPING BEHAVIOR

  • JIANG Hong-Jie ,
  • KE Chang-Bei ,
  • CAO Pan-Pan ,
  • MA Xiao ,
  • ZHANG Xin-Beng
Expand
  • School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640

Received date: 2011-05-04

  Revised date: 2011-07-19

  Online published: 2011-09-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50871039 and 50801029) and the Fundamental Research Funds for the Central Universities (No.2011ZM0001)

Abstract

NiTi shape memory alloys have attracted significant attention for applications in various fields in the past decades. Although porous NiTi alloys exhibit lower density compared with the dense ones, they are inevitably lower in strength, storage modulus and damping capacity. Therefore, it is imperative to study and improve the compressive performance and storage modulus in porous NiTi alloys. In this study, the nano-sized SiC particle reinforced NiTi shape memory alloy based composites (SiC/NiTi) have been successfully fabricated by means of a step powder-sintering method, which show unique characteristics of lightweight, high strength and stable superelasticity. The fabricated SiC/NiTi composites possess almost the same equivalent strength compared with dense NiTi alloys. On the other hand, they are in the nature of higher strength, including compressive strength and equivalent compressive strength, than porous NiTi alloys. Furthermore, the strength increases with increasing contents of SiC particles. It has been indicated that the addition of SiC particles has a slight influence on the phase composition of the SiC/NiTi composites, while the martensitic phase transformation temperatures of the composites keep unchanged compared with the NiTi alloy without SiC reinforcement. Meanwhile, the fabricated composites inherit the high damping performance of the NiTi matrix, and thus exhibit a high storage modulus.

Cite this article

JIANG Hong-Jie , KE Chang-Bei , CAO Pan-Pan , MA Xiao , ZHANG Xin-Beng . PREPARATION OF NANO-SIZED SiC REINFORCED NiTi SHAPE MEMORY COMPOSITES AND THEIR MECHANICAL PROPERTIES AND DAMPING BEHAVIOR[J]. Acta Metall Sin, 2011 , 47(9) : 1105 -1111 . DOI: 10.3724/SP.J.1037.2011.00281

References

[1] Miyazaki S, Otsuka K. Trans ISIJ, 1989; 29: 353

[2] Graesser E J, Cozzarelli F A. J EngMech, 1991; 117: 2590

[3] Aiken I D, Nims K D, Whittaker A S, James M K, Eeri M. Earthq Spectra, 1993; 9: 335

[4] Van Humbeeck J. J Alloys Compd, 2003; 355: 58

[5] Li D S, Zhang Y P, Xiong Z P, Zhang X P. Acta Metall Sin, 2008; 44: 995

(李大圣, 张宇鹏, 熊志鹏, 张新平. 金属学报, 2008; 44: 995)

[6] Li B Y, Rong L J. J Mater Res, 1998; 13: 2847

[7] Yuan B, Chung C Y, Zhang X P, Zeng M Q, Zhu M. Smart Mater Struct, 2005; 14: S201

[8] Zhang Y P, Li D S, Zhang X P. Scr Mater, 2007; 57: 1020

[9] Yang Y, Lan J, Li X C. Mater Sci Eng, 2004; A386: 284

[10] Li D S, Zhang X P, Xiong Z P, Mai Y W. J Alloys Compd, 2010; 490: 15

[11] Maruyama B, Hunt W. JOM, 1999; 11: 59

[12] Contreras A, Angeles–Ch´avez C, Flores O, Perez R. Mater Charact, 2007; 58: 685

[13] Zhang Y P, Yuan B, Zeng M Q, Chung C Y, Zhang X P. J Mater Process Technol, 2007; 439: 192

[14] Kuang Y H, Ngai T, H G, Li Y Y. J Alloys Compd, 2009; 209: 4607

[15] Gale W F, Totemeier T C. Smithell Metals Reference Book. Netherlands: Elsevier, 2004: 9

[16] Ke C B, Ma X, Zhang X P. Acta Metall Sin, 2011; 47: 129

(柯常波, 马骁, 张新平. 金属学报, 2011; 47: 129)

[17] Rao G B, Wang J Q, Han E H, Ke W. Acta Metall Sin, 2002; 38: 575

(饶光斌, 王俭秋, 韩恩厚, 柯 伟. 金属学报, 2002; 38: 575)

[18] Zhang X P, Liu H Y, Yuan B, Zhang Y P. Mater Sci Eng, 2008; A481: 170

[19] Li D S. PhD Thesis, South China University of Technology, Guangzhou, 2009

(李大圣. 华南理工大学博士论文, 广州, 2009)

[20] Zhao J S. The Basis of Dislocation Theory. Beijing: National Defense Industry Press, 1989: 148

(赵敬世. 位错理论基础. 北京: 国防工业出版社, 1989: 148)

[21] Lin H C, Wu S K, Yeh M T. Metall Mater Trans, 1993; 24A: 2189

[22] Nishiyama K, Yamanaka M, Omori M, Umekawa S. Mater Sci Lett, 1990; 9: 526

[23] Gao M X, Oliveira F J, Pan Y, Yang L, Baptista J L, Vieira J M. Intermetallics, 2005; 13: 406

[24] Wang H M, Wang C M, Cai L X. Surf Coat Technol, 2003; 168; 202

[25] Cai W, Lu X L, Zhao L C. Mater Sci Eng, 2005; A394: 78
Outlines

/

〈 〉