PHOTOELECTROCHEMICAL STUDY ON SEMICONDUCTOR PROPERTIES OF Ni-BASED ALLOYS OXIDE FILMS FORMED IN 288℃ HIGH TEMPERATURE WATER

  • ZHANG Qing-Han ,
  • TAN Yu ,
  • LIANG Ke-Xin
Expand
  • School of Environmental Science and Engineering, North China Electric Power University, Baoding 071003

Received date: 2011-04-26

  Revised date: 2011-07-16

  Online published: 2011-09-11

Supported by

Supported by National Natural Science Foundation of China (No.50971059) and Fundamental Research Funds for the Central Universities (No.10QX42)

Abstract

The oxide films formed on Ni-based alloys in high temperature water with semiconductor properties were investigated by photoelectrochemical responses. Two Ni-based alloys (Incoloy800HT and Inconel600) were corroded at 288℃ for 100 h in water, and four contributions from the photocurrent are obtained by photoelectrochemical responses. Band gap energy of 2.3 eV is attributed to the presence of nickel hydroxide or nickel-ferrite oxide. Band gap energy of 2.9 and 3.5 eV are attributed to Cr2O3 and band gap energy in the range of 4.1-4.3 eV is attributed to the spinel phase FexNi1-xCr2O4. In the photoelectrochemical responses in function of the applied potential tests, the oxide films on Incoloy800HT alloy indicate n type semiconductor in the potential range from -400 mV\linebreak to +400 mV, and the oxide films on Inconel600 alloy indicate n/p type semiconductor. In addition, the dephasing angle of the photoelectrochemical responses has a 180$^{\circ}$ evolution at the potential where the semiconductor of oxide film turns from n to p type.

Cite this article

ZHANG Qing-Han , TAN Yu , LIANG Ke-Xin . PHOTOELECTROCHEMICAL STUDY ON SEMICONDUCTOR PROPERTIES OF Ni-BASED ALLOYS OXIDE FILMS FORMED IN 288℃ HIGH TEMPERATURE WATER[J]. Acta Metall Sin, 2011 , 47(9) : 1147 -1152 . DOI: 10.3724/SP.J.1037.2011.00270

References

[1] Hamadou L, Kadri A, Benbrahim N, Petit J P. J Electrochem Soc, 2007; 154: 291

[2] Rangel C M, Silva T M, da Cunha Belo M. Electrochim Acta, 2005; 50: 5076

[3] Cheng Y F, Luo J L. Electrochim Acta, 1999; 44: 2947

[4] Schmuki P, B¨ohni H. J Electrochem Soc, 1992; 139: 1908

[5] Maurice V, YangWP, Marcus P. J Electrochem Soc, 1998; 145: 909

[6] Asami K, Hashimoto K, Shimodaira S. Corros Sci, 1978; 18: 151

[7] Sennour M, Marchetti L, Perrin S, Molins R, Pijolat M, Raquet O. Mater Sci Forum, 2008; 595: 539

[8] Sudensh T L, Wijesinghe L, Blackwood D J. Corros Sci, 2008; 50: 23

[9] Mac´ak J, Sajdl P, Kuˇcera P, Novotn´y R, Voˇsta J. Electrochim Acta, 2006; 51: 3566

[10] Carette F, Lafont M C, Chataignier G, Guinard L, Pieraggi B. Surf Interface Anal, 2002; 34: 135

[11] Carette F, Lafont M C, Guinard L, Pieraggi B. Mater High Temp, 2003; 20: 581

[12] Machet A, Galtayries A, Zanna S, Klein L, Maurice V, Jolivet P, Foucault M, Combrade P, Scott P, Marcus P. Electrochim Acta, 2004; 49: 3957

[13] Montemor M F, Ferreira M G, Hakiki N E, da Cunha Belo M D. Corros Sci, 2000; 42: 1635

[14] Fujimoto S, Chihara O, Shibata T. Mater Sci Forum, 1998; 289–292: 989

[15] Tsuchiya H, Fujimoto S, Chihara O, Shibata T. Electrochim Acta, 2002; 47: 4357

[16] Henry S, Mougin J,Wouters Y, Petit J P, Galerie A. Mater High Temp, 2000; 17: 231

[17] Calvarin G, Huntz A M, Molins R. Mater High Temp, 2000; 17: 257

[18] Balaji S, Kalai S R, John B L, Angappan S, Subramanian K, Augustin C O. Mater Sci Eng, 2005; B119: 119

[19] Sunseri O, Piazza S, Di Quarto F. J Electrochem Soc, 1990; 137: 2411

[20] Carpenter M K, Corrigan D A. J Electrochem Soc, 1989; 136: 1022

[21] Marchetti L, Perrin S, Raquet O, Pijolat M. Mater Sci Forum, 2008; 595–598: 529

[22] Marchetti L, Perrin S, Wouters Y, Martin F, Pijolat M. Electrochim Acta, 2010; 55: 5384

[23] Yves Marfaing. J Cryst Growth, 1996; 1–4: 205

[24] Sarrazin P, Galerie A, Fouletier J. Mechanisms of High Temperature Corrosion: A Kinetic Approach, Zurich: Trans Tech Publications Ltd., 2008, 488

[25] Macdonald D D. J Electrochem Soc, 1992; 139: 3434
Outlines

/

〈 〉