NUMERICAL SIMULATION OF KEYHOLE’S DYNAMIC VARIATION IN CONTROLLED PULSE PAW PROCESS

  • XUN Jun-Hua ,
  • WU Zhuan-Song ,
  • QIN Guo-Liang
Expand
  • Key Lab for Liquid–Solid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061

Received date: 2011-02-14

  Revised date: 2011-04-12

  Online published: 2011-08-11

Supported by

Supported by National Natural Science Foundation of China (No.50936003) and Specialized Research Fund for the Doctoral Program of Higher Education (No.20090131110023)

Abstract

During the controlled pulse key–holing plasma arc welding (PAW), keyhole shape and size change with the welding current dynamically, and undergo variation of the "establishing–expanding–contracting–closing"process. Numerical analysis on such dynamic variation process of keyhole shape and size can provide insight into the process mechanism and basic data for optimizing the process parameters. In this study, a three–dimensional transient model is developed to conduct numerical simulation of welding temperature field, weld pool geometry, and keyhole shape and size in controlled pulse PAW. The keyhole shape and size are computed by analyzing the force–action on the weld pool surface, and two situations are considered to deal with partial keyhole and open keyhole. The dynamic variation features of three–dimensional keyhole shapes in weld pool in a pulse cycle are numerically calculated. Experiments are conducted to validate the numerical simulation result of key–holing duration.

Cite this article

XUN Jun-Hua , WU Zhuan-Song , QIN Guo-Liang . NUMERICAL SIMULATION OF KEYHOLE’S DYNAMIC VARIATION IN CONTROLLED PULSE PAW PROCESS[J]. Acta Metall Sin, 2011 , 47(8) : 1061 -1066 . DOI: 10.3724/SP.J.1037.2011.00072

References

[1] Wu C S, Jia C B, Chen M A. Weld J, 2010; 89: 225s

[2] Jia C B, Wu C S, Gao J Q. Acta Metall Sin, 2010; 46: 991

(贾传宝, 武传松, 高进强. 金属学报, 2010; 46: 991)

[3] Saedi H R, Unkel W. Weld J, 1988; 67: 247s

[4] Vishnu P R, Easterling K E. Mater Sci Technol, 1991; 7: 649

[5] Wu C S, Zheng W, Wu L. Acta Metall Sin, 1998; 34: 416

(武传松, 郑 炜, 吴 林. 金属学报, 1998; 34: 416)

[6] Reddy A A, Guta B, Achar D R G. Numer Heat Trans, 2002; 41A: 41

[7] Liu W L, Hu S S, Ma L. Trans China Weld Inst, 2006; 26(6): 33

(刘望兰, 胡绳荪, 马立. 焊接学报, 2006; 26(6): 33)

[8] Keanini R G, Rubinsky B. Int J Heat Mass Transfer, 1993; 36: 3283

[9] Nehad A K. Int Commun Heat Mass, 1995; 22: 779

[10] Wu C S, Wang H G, Zhang Y M. Weld J, 2006; 85: 284s

[11] Wu C S, Hu Q X, Gao J Q. Comp Mater Sci, 2009; 46:167

[12] Huo Y S, Wu C S. China Weld, 2009; 18(3): 12

[13] Fan H G, Kovacevic R. J Phys, 1999; 32D: 2902

[14] Wu C S. Welding Thermal Processes and Weld Pool Behaviors. Boca Raton: CRC Press/Taylor & Francis Group, 2010: 49

[15] Wu C S, Chen J, Zhang Y M. Comp Mater Sci, 2007; 39: 635

[16] Sahoo P, Debroy T, Mcnallan M J. Metall Mater Trans, 1988; 19B: 483
Outlines

/

〈 〉