Abstract

Utilizing the high–temperature chemical reaction between Ti and AlN, TiN reinforced Ti3Al composite coating was in situ synthesized on TC4 alloy substrate by laser cladding technique. The phase constitution and microstructure of treated samples were examined by XRD and SEM. The results reveal that the coating is mainly composed of TiN and Ti3Al phase. When the molar ratio between Ti and AlN is 4∶2, the content of TiN reduces as the laser power density increases; whereas when the molar ratio between Ti and AlN is 4∶1, the content of TiN increases with increasing the laser power density. SEM observation shows that the morphology of TiN changes gradually from bar–shaped to granular with the increase of laser power density. When the molar ratio between Ti and AlN is 4∶1 and the laser power density is 15.28 kW·s·cm−2, the macro-morphology of surface coating is better, no pores and cracks appear. The average microhardness of laser cladding coating is 3.4 times larger than that of TC4 alloy substrate.

Cite this article

LIU Hong-Xi , ZHANG Xiao-Wei , JIANG Ye-Hua , YU Zhuan-Qi , ZENG Wei-Hua . LASER IN SITU SYNTHESIZED TiN/Ti3Al COMPOSITE COATINGS[J]. Acta Metall Sin, 2011 , 47(8) : 1086 -1093 . DOI: 10.3724/SP.J.1037.2010.00641

References

[1] Astar E, Kayali E S, Cimenoglu H. Surf Coat Technol, 2008; 202: 4583

[2] Gurrappa I, Gogia A K. Surf Coat Technol, 2001; 139: 216

[3] Liu X B, Shi S H, Guo J, Fu G Y, Wang M D. Appl Surf Sci, 2009; 255: 5662

[4] Ceschini L, Lanzoni E, Martini C, Prandstraller D, Sambogna G. Wear, 2008; 264: 86

[5] Leng C Y, Zhou R, Zhang X, Lu D H, Liu H X. Acta Metall Sin, 2009; 45: 764

(冷崇燕, 周荣, 张旭, 卢德宏, 刘洪喜. 金属学报,2009; 45: 764)

[6] Guo B G, Zhou J S, Zhang S T, Zhou H D, Pu Y P, Chen J M. Mater Sci Eng, 2008; A480: 404

[7] Zhang Y Z, Jin J T, Huang C, Shi L K. Rare Met Mater Eng, 2010; 39: 1403

(张永忠, 金具涛, 黄灿, 石力开. 稀有金属材料与工程,2010; 39: 1403)

[8] Liu H X, Jiang Y H, Zhou R, Zhou R F, Jin Q L, Tang B Y. Acta Metall Sin, 2008; 44: 325

(刘洪喜, 蒋业华, 周 荣, 周荣锋, 金青林, 汤宝寅. 金属学报, 2008; 44: 325)

[9] Suresha S J, Bhide R, Jayaram V, Biswas S K. Mater Sci Eng, 2006; A429: 252

[10] Bhaduri D, Chattopadhyay A K. Surf Coat Technol, 2010; 205: 658

[11] Xia F F, Liu C, Wang F, Wu M H, Wang J D, Fu H L, Wang J X. J Alloys Compd, 2010; 490: 431

[12] Zeng X B, Peng P. Acta Metall Sin, 2009; 45: 1049

(曾宪波, 彭平. 金属学报, 2009; 45: 1049)

[13] Shiue R K, Wu S K, Chen Y T. Intermetallics, 2010; 18: 107

[14] Paransky Y, Berner A, Gotman I. Mater Lett, 1999; 40: 180

[15] Wang Y X, Chen X. Appl Surf Sci, 1999; 148: 235

[16] Kun J, Ma X G, Liu X F. J Alloys Compd, 2009; 488: 84

[17] Coelho J P, Abreu M A, Pires M C. Opt Laser Eng, 2000; 34: 385

[18] Li L J, Mazumder J. Appl Laser, 1986; 7: 1

(李力钧, Mazumder J. 应用激光, 1986; 7: 1)

[19] Zhang F, Yan P X, Chen J T, Miao B B, Li G B, Wang J. J Syn Cryst, 2007; 36: 3

(张飞, 闫鹏勋, 陈江涛, 苗彬彬, 李冠斌, 王君. 人工晶体学报, 2007; 36: 3)

[20] Zuo Y S, Chen W Z, Liang W. Modern Analysis Methods of Materials. Beijing: Press of Beijing University of Technology, 2006: 107, 111

(左演声, 陈文哲, 梁伟. 材料现代分析方法. 北京: 北京工业大学出版社, 2006: 107, 111)

[21] Li G F, Wang S H, Shi Z L. Nonferrous Met, 2008; 60: 53

(李国芳, 王顺花, 石宗利. 有色金属, 2008; 60: 53)

[22] Lv W J, Zhang X N, Zhang D, Wu R J, Bian Y J, Fang P W. Acta Metall Sin, 2000; 36: 105

(吕维杰, 张小农, 张 荻, 吴人杰, 卞玉君, 方平伟. 金属学报,2000; 36: 105)

[23] Yin S, Miu S X, Liao X W, Lai H Y, Wang R. J Univ Sci Technol Beijing, 1993; 15: 99

(殷声, 缪曙霞, 廖湘巍, 赖和怡, 王润. 北京科技大学学报,1993; 15: 99)

[24] Dai Y N. Binary Alloy Phase Diagrams. Beijing: Science Press, 2009: 1

(戴永年. 二元合金相图集. 北京: 科学出版社, 2009: 1)

[25] Gao J, Li C R, Wang N, Du Z M. J Univ Sci Technol Beijing, 2000; 15: 420

[26] Zhou G D, Duan L Y. The Basis of Structural Chemistry, 3rd Ed. Beijing: Peking University Press, 2002: 178

(周公度, 段连运. 结构化学基础. 第三版, 北京: 北京大学出版社, 2002: 178)

[27] Ye D L, Hu J H. Thermodynamic Data Sheet of Practical Inorganic, 2nd Ed. Beijing: Metallurgical Industry Press, 2002: 79, 1055

(叶大伦, 胡建华. 实用无机物热力学数据手册. 第二版, 北京: 冶金工业出版社, 2002: 79, 1055)
Outlines

/