论文

RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS

  • LV Zheng
Expand
  • Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819

Received date: 2011-04-25

  Revised date: 2011-05-03

  Online published: 2011-07-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50971033 and 91026013), National Basic Research Program of China (No.2011CB610405), Fundamental Research Funds for the Central Universities (No.N100402001) and Program for New Century Excellent Talents in University (No.NCET-10-0302)

Abstract

Neutron irradiation can lead to the embrittlement and the shift of ductile-brittle transition temperature (DBTT) of the reactor pressure vessel (RPV) steels, which is the potential threat to the safe operation of reactors. Surveillance program for RPVs, irradiation damage and embrittlement of RPV steels and safe evaluation of RPVs were reviewed in this paper.

Cite this article

LV Zheng . RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS[J]. Acta Metall Sin, 2011 , 47(7) : 777 -783 . DOI: 10.3724/SP.J.1037.2011.00265

References

[1] Odette G R, Lucas G E. JOM, 2001; 53: 18

[2] Little E A. Proc EUROMAT 96, Conf Materials and Nuclear Power, London: Institute of Materials, 1996: 29

[3] Nanstad R K, Sokolov M A, McCabe D E. J ASTM Int, 2008; 5: JAI101346

[4] Steele L E. In: Steele L E, ed., Status of USA Nuclear Reactor Pressure Vessel Surveillance for Radiation Effects, ASTM STP 784, Philadelphia, PA: American Society for Testing and Materials, 1983: 277

[5] Wallin K. Eng Fract Mech, 2002; 69: 451

[6] Little E A. Proc Conf Dimensional Stability and Mechanical Behavior of Irradiated Metals and Alloys, London: BNES, 1984: 141

[7] Guionnet C, Robin Y, Flavier C, Lefort A, Gros D, Perdreau R. In: Kramer D, Brager H R, Perrin J S, eds., Effects of Radiation on Materials: Proceedings of the Tenth International Symposium, ASTM STP 725, Philadelphia, PA: American Society for Testing and Materials, 1981: 20

[8] Monzen R, Iguchi M, Jenkins M L. Philos Mag Lett, 2000; 80: 137

[9] Phythian W J, English C A. J Nucl Mater, 1993; 205: 162

[10] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater, 2003; 320: 177

[11] Faulkner R G, Lu Z, Ellis D, Williams T J. J ASTM Int, 2005; 2: 285

[12] Buswell J T, Little E A, Sinclair R N. Nucl Energy, 1998; 37: 387

[13] Schilling W, Ullmaier H. In: Cahn R W, eds., Materials Science and Technology: Nuclear Materials, Vol.10B, Germany: Wiley–VCH, 1994: 179

[14] Domain C, Becquart C S, Malerba L. J Nucl Mater, 2004; 335: 121

[15] Jenkins M L, Kirk M A. Characterisation of Radiation Damage by Transmission Electron Microscopy. Bristol and Philadelphia: IOP Publishing, 2001: 126

[16] Little E A, Harries D R. Met Sci, 1970; 4: 188

[17] English C A, Ortner S R, Gage G, Server W L, Rosinski S T. In: Rosinski S T, Grossbeck M L, Allen T R, Kumar A S, eds., Effects of Radiation on Materials: 20th International Symposium, ASTM STP 1405, West Conshohocken, PA: American Society for Testing and Materials, 2001: 151

[18] Bischler P J E, Wild R K. In: Gelles D S, Nanstad R K, Kumar A S, Little E A, eds., Effects of Radiation on Materials: 17th International Symposium, ASTM STP 1270, West Conshohocken, PA: American Society for Testing and Materials, 1996: 260

[19] Faulkner R G, Jones R B, Lu Z, Flewitt P E J. Philos Mag, 2005; 85: 2065

[20] Pechenkin V A, Konobeev Y V, Stepanov I A, Nikolaev Y A. In: Grossbeck M L, Allen T R, Lott R G, Kumar A S, eds., Effects of Radiation on Materials: 21st International Symposium, ASTM STP 1447, West Conshohocken, PA: American Society for Testing and Materials, 2004: 138

[21] Lu Z, Faulkner R G, Flewitt P E J. Mater Sci Eng, 2006; A437: 306

[22] Lu Z, Faulkner R G, Sakaguchi N, Kinoshita H, Takahashi H J, Flewitt P E. J Nucl Mater, 2006; 351: 155

[23] Brillaud C, Hedin F, Houssin B. In: Garner F A, Henager C H, Igata N, eds., Influence of Radiation on Material Properties: 13th International Symposium, ASTM STP 956, Philadelphia, PA: American Society for Testing and Materials, 1987: 420

[24] Petrequin P. A Review of Formulas for Predicting Irradiation Embrittlement of Reactors Vessel Materials, AMES Report No.6, 1996: 13

[25] Odette G R, Mader E V, Lucas G E, Phythian W J, English C A. In: Kumar A S, Gelles D S, Nanstad R K, Little E A, eds., Effects of Radiation on Materials: 16th International Symposium, ASTM STP 1175, Philadelphia, PA: American Society for Testing and Materials, 1993: 373

[26] Odette G R, Yamamoto R T, Klingensmith R D. Philos Mag, 2005; 85: 779

[27] Miller M K, Russell K F. J Nucl Mater, 2007; 37: 145

[28] Odette G R, Wirth B D. J Nucl Mater, 1998; 251: 157
Outlines

/

〈 〉